The Latest Development of Ultrafine/Nano W-Cu Composite Powder Preparation AITranslate
Abstract AITranslate
The latest development of ultrafine/nano W-Cu composite powders is reviewed recently in China and abroad. Several preparation methods of ultrafine/nano W-Cu composite powders are introduced and analyzed on their technical characteristics, including mechanical alloying, mechanical-thermochemieal meth od,spray drying and sol-gel.
KeyWords AITranslate
1朱永兵,沈以赴.钨铜纳米复合粉末的制备技术研究[J].金属功能材料,2006,13(5):31-35. 被引量:9
2范景莲,刘军,严德剑,黄伯云.细晶钨铜复合材料制备工艺的研究[J].粉末冶金技术,2004,22(2):83-86. 被引量:46
3杨明川,宋贞桢,卢柯.W-20%Cu纳米复合粉的制备[J].金属学报,2004,40(6):639-642. 被引量:27
4Srikanth R,David L B. Synthesis and evaluation of ad- vanced nanocrystalline tungsten-based materials[J]. P/ M Science & Technology Briefs, 1999,1 (1) : 9-14.
5Cheng J G, Lei C P, Xiong E, et al. Preparation and characterization of W-Cu nanopowders by a homogene- ous precipitation process [J]. Journal of Alloys and Compounds, 2006,421 : 146-150.
6Li Y P,Qu X H,Zheng Z S,et al. Properties of W-Cu composite powder produced by a thermo- mechanical method[J]. International Journal of Refractory Metals &Hard Materials,2003,21 :259-264.
7Benjamin J S. Dispersion strengthened superalloys by mechanical alloying [J]. Metallurgical Transactions, 1970,1(10) :2 943-2 951.
8Gilman P S,Benjamin J S. Mechanical alloying[J]. Annual Review of Materials Science, 1983,13 : 279-300.
9Aboud T, Weiss B Z, Chaim R. Mechanical alloying of the immiscible system W-Cu[J]. Nanostructurecl Materials, 1994,6 (4) : 405-408.
10范景莲,刘涛,朱松,田家敏.W-Cu复合材料制备新技术与发展前景[J].硬质合金,2011,28(1):56-65. 被引量:21
1王德志,尹邦柱,孙翱魁,李然,段柏华.甘氨酸硝酸盐法制备超细Mo-Cu粉末及烧结[J].有色金属科学与工程,2016,7(2):19-24. 被引量:1
1王德志,张宇晴,段柏华.微波快速熔渗制备钼铜复合材料[J].有色金属科学与工程,2018,9(3):11-16. 被引量:8
1高翔,李先容,朱彩强,贾玉斌,郑刚.热机械合金化法制备纳米晶W-Cu复合粉末[J].粉末冶金材料科学与工程,2015,20(3):444-448. 被引量:7
2曹顺华,林信平,李炯义.纳米晶W-Cu复合粉末烧结行为[J].中国有色金属学报,2005,15(2):248-253. 被引量:10
3范景莲,朱松,刘涛.纳米W-Cu复合粉末制备技术的研究现状[J].硬质合金,2008,25(4):252-256. 被引量:6
4李新春,成会朝,范景莲.纳米镍粉制备技术研究进展[J].粉末冶金技术,2009,27(2):142-147. 被引量:7
5张立,陈述,刘刚,杨贵彬,黄泽兰,黄伯云,张传福.高性能超细、纳米硬质合金及其制备过程中的关键技术问题[J].材料导报,2005,19(11):4-7. 被引量:21
6雷纯鹏,赵勇军,刘刚,唐建成.3种特殊微结构WC-Co硬质合金的研究进展[J].粉末冶金工业,2014,24(5):48-53. 被引量:6
7Moon.,IH.散装W—Cu复合粉末的完全致密化[J].钨钼材料,1999(1):43-50.
8林信平,曹顺华,李炯义.Cu含量对纳米晶W-Cu复合粉末烧结行为的影响[J].电工材料,2004(3):10-14. 被引量:4
9程继贵,弓艳飞,夏永红,宋鹏,蒋阳,吴玉程.机械热化学法制备纳米W-Cu复合粉末及其烧结性能研究[J].材料热处理学报,2007,28(4):11-15. 被引量:4
10周健,周强,袁德林,杨树忠.超细/纳米W-La_2O_3复合粉末的制备及烧结致密化行为研究[J].中国钨业,2015,30(6):42-48. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF123.72[冶金工程—粉末冶金]
Citation Information:
The latest development of ultrafine/nano W-Cu composite powders is reviewed recently in China and abroad. Several preparation methods of ultrafine/nano W-Cu composite powders are introduced and analyzed on their technical characteristics, including mechanical alloying, mechanical-thermochemieal meth od,spray drying and sol-gel.
quote
| GB/T 7714-2015 | [1] HUANG Li-mei, LUO Lai-ma, WU Yu-cheng, et al. The Latest Development of Ultrafine/Nano W-Cu Composite Powder Preparation[J]. Rare Metals and Cemented Carbides, 2012(4): 30-34. |
| MLA | [1] HUANG Li-mei, et al., "The Latest Development of Ultrafine/Nano W-Cu Composite Powder Preparation." Rare Metals and Cemented Carbides, no. 4, 2012, pp. 30-34. |
| APA | [1] HUANG Li-mei, LUO Lai-ma, WU Yu-cheng, & LUO Guang-nan. (2012). The Latest Development of Ultrafine/Nano W-Cu Composite Powder Preparation. Rare Metals and Cemented Carbides(4), 30-34. |
| IEEE | [1] HUANG Li-mei, LUO Lai-ma, WU Yu-cheng, and LUO Guang-nan, "The Latest Development of Ultrafine/Nano W-Cu Composite Powder Preparation," Rare Metals and Cemented Carbides, no. 4, pp. 30-34, 2012. keywords: {W-Cu composite powder;ultrafine/nano crystal grain;preparation method;mechanical alloying;spray drying;sol-gel} |