daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Preparation and Performance Study of Single-host White-emitting Phosphor GdPO∶Dy AITranslate

School of Chemistry and Materials Science,Guizhou Normal University;School of Chemistry and Materials Science,Guizhou Normal University;School of Chemistry and Materials Science,Guizhou Normal University;School of Chemistry and Materials Science,Guizhou Normal University;School of Chemistry and Materials Science,Guizhou Normal University;School of Chemistry and Materials Science,Guizhou Normal University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Single-host white-emitting Gd3PO7∶Dy^3+ phosphor was synthesized by wet chemical method.The phase structure,morphologies and optical properties of the as-prepared samples were characterized by X-ray powder diffraction(XRD),scanning electron microscope(SEM),Fourier transform infrared spectroscopy(FT-IR),and fluorescence spectroscopy.The XRD results show that the samples are Dy^3+ doped Gd3PO7 crystals with monoclinic structure and slight impurity.The fluorescence spectra show that under the excitation with the characteristic excitation band of Gd^3+ ions at 276 nm,Gd3PO7∶Dy^3+ samples emit the characteristic emission bands of Dy^3+ ions in yellow light region(4F9/2→6H13/2) and blue light region(4F9/2→6H15/2),which indicates that the energy transfer from Gd^3+ to Dy^3+ occurs in the Gd3PO7∶Dy^3+matrix.The luminescence intensity of the samples depends on pH values and Dy^3+ dosage.When the pH value is 6.00 and the Dy^3+ dosage is 0.5%,the sample exhibits a relatively high luminescence intensity.The Dy^3+ dosage directly affects the luminescence color of Gd3PO7∶Dy^3+ samples,and the as-synthesized Gd3PO7∶Dy^3+ sample with 3% Dy^3+ can emit white light with the coordinate of(0.335,0.345),which indicates that Gd3PO7∶Dy^3+ is a potential single-host white-emitting phosphor.

KeyWords AITranslate

Gd3PO7 single-host phosphors Dy^3+doping white-emitting energy transfer

1彭玲玲,韩涛,陈慧,张铁军.Spectroscopic properties of Gd_2O_3:Dy^(3+)nanocrystals[J].稀土学报:英文版,2013,31(3):235-240. 被引量:1

2郑思琪,王娟,燕映霖,张海鹏.pH值对LaVO_4:Eu^(3+)纳米晶的相变及发光性能的影响[J].中国稀土学报,2015,33(3):316-322. 被引量:3

3袁桃利,夏婉婉,于宏柱,张成山,张方程,段佩华,王晓峰,付作岭.白光LED用正交相Gd_2(MoO_4)_3:Dy^(3+)荧光粉的制备与发光性能[J].发光学报,2012,33(9):929-933. 被引量:9

4吴拓,潘桦滟,陈如标,罗东,张宏,沈晔,李旸晖,王乐.Effect of solution pH value changes on fluorescence intensity of magnetic-luminescent Fe3O4@Gd2O3:Eu^3+ nanoparticles[J].稀土学报:英文版,2016,34(1):71-76. 被引量:2

5欧娅,付兵,朱莉萍,陈雪羽,杨锦瑜.共沉淀法制备Eu^(3+)掺杂La_3PO_7荧光材料及其性能[J].中国有色金属学报,2017,27(5):974-980. 被引量:7

6曹耀武,罗黎,郭清海,舒杼.纳米级水氯铁镁石的制备及颗粒团聚控制[J].材料科学与工艺,2018,26(2):27-33. 被引量:6

7吕少哲,张家骅,张继森,鄂书林,赵海峰,骆永石.Eu^(3+)掺杂的含氧磷酸盐发光性质[J].发光学报,2013,34(11):1435-1439. 被引量:4

8乐天,曾庆光,盛业青,张梅,侯亮,陈锋.前驱液pH值对2ZnO·2.2B_2O_3·3H_2O∶Eu^(3+)荧光粉发光性能的影响[J].人工晶体学报,2012,41(3):661-665. 被引量:2

1李博,李亚杰,王哲.光照疗法对改善阿尔茨海默症患者睡眠障碍的系统综述[J].中国护理管理,2020,20(9):1299-1305. 被引量:9

2郭璐庆.游资恶炒抖音概念 风险加剧[J].商业观察,2020(12):80-81.

3袁楷,陈祯,杨婷婷,姜静,周文健.光谱和光强度对柑橘木虱成虫趋光行为的影响[J].云南农业大学学报:自然科学版,2020,35(5):750-755. 被引量:3

4姜秀榕,张钦应,刘铠铭,江程,郑文进.白光LED用红色荧光粉Ca0.7Sr0.18-0.15xMoO4:Eu^3+0.08:Gd^3+x水热合成与发光性能研究[J].功能材料,2020,51(9):9201-9207. 被引量:1

5杨亮,陈宁,宋西平,张蓓.多孔钛的制备及力学性能研究[J].热加工工艺,2020,49(18):60-64. 被引量:2

6赵小杨,温慧霞,李红喜,许成功,杨启山.稀土掺杂锡酸盐体系长余辉发光材料研究进展[J].化学研究与应用,2020,32(10):1737-1746. 被引量:4

7高效稳定并可溶液加工的一维1D-AI0杂化荧光材料[J].中国品牌与防伪,2020(5):80-81.

8王世龙,熊传兵,汤英文,李晓珍,刘倩.共晶芯片数及芯片位置对陶瓷共晶封装LED发光性能的影响[J].发光学报,2020,41(11):1421-1430. 被引量:5

9张飞翔,王建,田星原,孙海杰.不同晶体结构的La0.9Sr0.1Ga0.8Mg0.2O3-δ体系氧空位的形成和迁移研究[J].化学工程与技术,2020,10(4):322-328.

10籍永华,秦丙克,黄润,张金柱.固相反应快速制备CoTe2及其热电性质研究[J].昆明理工大学学报:自然科学版,2020(3):24-28.

Basic Information:

DOI:

Chinese Library Classification Number:O482.31[理学—固体物理]

Citation Information:

Single-host white-emitting Gd3PO7∶Dy^3+ phosphor was synthesized by wet chemical method.The phase structure,morphologies and optical properties of the as-prepared samples were characterized by X-ray powder diffraction(XRD),scanning electron microscope(SEM),Fourier transform infrared spectroscopy(FT-IR),and fluorescence spectroscopy.The XRD results show that the samples are Dy^3+ doped Gd3PO7 crystals with monoclinic structure and slight impurity.The fluorescence spectra show that under the excitation with the characteristic excitation band of Gd^3+ ions at 276 nm,Gd3PO7∶Dy^3+ samples emit the characteristic emission bands of Dy^3+ ions in yellow light region(4F9/2→6H13/2) and blue light region(4F9/2→6H15/2),which indicates that the energy transfer from Gd^3+ to Dy^3+ occurs in the Gd3PO7∶Dy^3+matrix.The luminescence intensity of the samples depends on pH values and Dy^3+ dosage.When the pH value is 6.00 and the Dy^3+ dosage is 0.5%,the sample exhibits a relatively high luminescence intensity.The Dy^3+ dosage directly affects the luminescence color of Gd3PO7∶Dy^3+ samples,and the as-synthesized Gd3PO7∶Dy^3+ sample with 3% Dy^3+ can emit white light with the coordinate of(0.335,0.345),which indicates that Gd3PO7∶Dy^3+ is a potential single-host white-emitting phosphor.

quote

GB/T 7714-2015 [1] ZHANG Ling, RAO Qi-liang, GUO Hai-rui, et al. Preparation and Performance Study of Single-host White-emitting Phosphor GdPO∶Dy[J]. Rare Metals and Cemented Carbides, 2020(5): 41-47.
MLA [1] ZHANG Ling, et al., "Preparation and Performance Study of Single-host White-emitting Phosphor GdPO∶Dy." Rare Metals and Cemented Carbides, no. 5, 2020, pp. 41-47.
APA [1] ZHANG Ling, RAO Qi-liang, GUO Hai-rui, ZHU Hao-tian, ZHU Li-ping, & YANG Jin-yu. (2020). Preparation and Performance Study of Single-host White-emitting Phosphor GdPO∶Dy. Rare Metals and Cemented Carbides(5), 41-47.
IEEE [1] ZHANG Ling, RAO Qi-liang, GUO Hai-rui, ZHU Hao-tian, ZHU Li-ping, and YANG Jin-yu, "Preparation and Performance Study of Single-host White-emitting Phosphor GdPO∶Dy," Rare Metals and Cemented Carbides, no. 5, pp. 41-47, 2020. keywords: {Gd3PO7;single-host phosphors;Dy^3+doping;white-emitting;energy transfer}