Experimental Study on Recovery of Vanadium from Titanium Dioxide Wastewater by Solvent Extraction AITranslate
Abstract AITranslate
Vanadium was separated and recovered from titanium dioxide wastewater by solvent extraction using P507 as the extractor.The effects of extractor type and concentration,O/A phase ratio,solution pH,extraction temperature and time on the extraction rate of vanadium in titanium dioxide wastewater were investigated.The results show that the extraction rate of vanadium is more than 98% under the following conditions:organic phase of 15%P507+5%2-octyl alcohol+80% sulfonated kerosene,solution pH value of 2.0,O/A phase ratio of 1.25∶1,extraction temperature and time of 50℃ and 6min.The V2O5 product with a purity greater than 99% is obtained by sulfuric acid reverse extraction of the saturated organic phase,NaClO3 oxidation,ammonium salt precipitation and roasting at 540℃.
KeyWords AITranslate
1崔佳娜,任慧莉.我国钛白粉生产工艺技术的发展及比较[J].稀有金属与硬质合金,2013,41(4):14-17. 被引量:13
2杨涛,王志坚,肖劲,刘吉波,余荣旻,邓志军.赤泥和钛白废液中提钪的浸出工艺研究[J].矿冶,2015,24(5):37-40. 被引量:11
3李具康,代佼.硫酸法钛白粉“三废”治理与利用的研究进展[J].环境科学导刊,2014,33(4):63-66. 被引量:8
4宋宇,李婷,邓燕,邱佳.硫酸法钛白浓废酸的综合治理[J].大众科技,2011,13(9):100-102. 被引量:10
5许红,殷咏梅,李鑫.硫酸法钛白废酸利用及发展简况[J].无机盐工业,2007,39(6):10-11. 被引量:7
6范兵,李志广,李昭,刘士琪,任保增.硫酸法钛白废酸的处理[J].河南化工,2013,30(6):12-15. 被引量:16
7李亮.国内外钛白废酸综合治理及回收利用研究现状[J].湿法冶金,2010,29(3):150-154. 被引量:23
1李望,杨小慧,朱晓波.钛白废液浸出赤泥回收钪和钒的实验研究[J].稀有金属与硬质合金,2021,49(3):1-4. 被引量:3
2李望,马晨,朱晓波.创新开放型化学综合实验的设计与实施[J].教育教学论坛,2021(40):69-72. 被引量:1
3高广言,高利坤,饶兵,王飞旺,沈海榕.硫酸法钛白废酸资源化利用现状及展望[J].钢铁钒钛,2021,42(5):99-108. 被引量:5
4陶荣荣,牛泽鹏,朱晓波,李望,张治国.利用钛白废液制备草酸亚铁实验研究[J].稀有金属与硬质合金,2022,50(1):6-9.
1陈胜文,李洪,刘利,谢茂文,蔡平雄.磷酸铁的制备工艺及应用展望[J].化纤与纺织技术,2021,50(11):37-39. 被引量:3
2申庆飞,许刚,张海涛.硫酸法钛白粉生产能耗分析与降耗对策研究[J].造纸装备及材料,2022,51(1):103-105.
3劳肇菊,黄晓倩,杨萍,张雪,蔡平雄.钛白废酸中钛资源的萃取及磷酸钛的制备研究[J].造纸装备及材料,2022,51(2):51-53.
4杨小慧,李望,朱晓波.D751螯合树脂吸附酸性溶液中钒(Ⅳ)离子的机制[J].中国有色金属学报,2022,32(12):3862-3870.
5徐菲,李如意,邹茜,袁园.自主设计实验在分析化学实验教学中的调查与研究[J].广东化工,2023,50(1):220-222.
6冯雪茹,吕国志,张廷安,赵秋月.P204萃取硫酸体系中V(IV)的性能研究[J].钢铁钒钛,2022,43(6):1-6.
7郝立苗,黄妃慧,程国园,王勇伟,邢延岭,关洋,陈一韬.我国铝矾土尾矿资源化利用研究进展[J].现代矿业,2023,39(4):114-118.
8董朝望,郭学益,夏阳,刘沛东,乔晋玺,李中臣,刘汉宁.低温碱浸高钛渣脱硅去除钛合金中的Ti_(5)Si_(3)相[J].中国有色金属学报:英文版,2023,33(5):1572-1582.
9叶鑫,赵爱春,刘宸嘉,卓泽森,杨小容,秦妍梅,曾淼.赤泥中有价金属的回收工艺研究进展[J].湿法冶金,2023,42(3):229-235.
1曾理,孙振,关文娟,张贵清.P204/4PC新协萃体系萃取分离镍与锰镁钙[J].东北大学学报:自然科学版,2018,39(10):1428-1432. 被引量:4
2张魁芳,刘志强,刘溢,曹洪杨.P204从硫酸体系萃取镓性能研究[J].有色金属:冶炼部分,2020,0(3):50-54. 被引量:4
3曾军,陈进中,叶有明,蔡井泉.从含锰钴镍浸出液中萃取回收锰[J].有色金属:冶炼部分,2020,0(4):12-16. 被引量:3
4明键伟,卢苏君,宛顺磊,张峰瑞,郭勇,卢晓锋,李亦婧.红土镍矿浸出液中钴、锰、铁的协同萃取[J].有色金属工程,2020,10(2):41-45. 被引量:1
5苏磊,张海军,汪瑾,于雪峰,董昌吉,孙泽,宋兴福,于建国.反应萃取法制备熔盐级硝酸钾工艺探讨[J].无机盐工业,2020,52(5):35-39. 被引量:1
6王冬,李硕,杨硕,纪雷鸣.工业脱硝技术应用现状及展望[J].化工科技,2020,28(2):77-82. 被引量:4
Basic Information:
DOI:
Chinese Library Classification Number:TF804.2[冶金工程—有色金属冶金]
Citation Information:
Vanadium was separated and recovered from titanium dioxide wastewater by solvent extraction using P507 as the extractor.The effects of extractor type and concentration,O/A phase ratio,solution pH,extraction temperature and time on the extraction rate of vanadium in titanium dioxide wastewater were investigated.The results show that the extraction rate of vanadium is more than 98% under the following conditions:organic phase of 15%P507+5%2-octyl alcohol+80% sulfonated kerosene,solution pH value of 2.0,O/A phase ratio of 1.25∶1,extraction temperature and time of 50℃ and 6min.The V2O5 product with a purity greater than 99% is obtained by sulfuric acid reverse extraction of the saturated organic phase,NaClO3 oxidation,ammonium salt precipitation and roasting at 540℃.
quote
| GB/T 7714-2015 | [1] ZHU Xiao-bo, NIU Ze-peng, LI Wang, et al. Experimental Study on Recovery of Vanadium from Titanium Dioxide Wastewater by Solvent Extraction[J]. Rare Metals and Cemented Carbides, 2020(1): 9-12. |
| MLA | [1] ZHU Xiao-bo, et al., "Experimental Study on Recovery of Vanadium from Titanium Dioxide Wastewater by Solvent Extraction." Rare Metals and Cemented Carbides, no. 1, 2020, pp. 9-12. |
| APA | [1] ZHU Xiao-bo, NIU Ze-peng, LI Wang, BAI Yun-tao, WANG Tao, & REN Bo. (2020). Experimental Study on Recovery of Vanadium from Titanium Dioxide Wastewater by Solvent Extraction. Rare Metals and Cemented Carbides(1), 9-12. |
| IEEE | [1] ZHU Xiao-bo, NIU Ze-peng, LI Wang, BAI Yun-tao, WANG Tao, and REN Bo, "Experimental Study on Recovery of Vanadium from Titanium Dioxide Wastewater by Solvent Extraction," Rare Metals and Cemented Carbides, no. 1, pp. 9-12, 2020. keywords: {vanadium recovery;solvent extraction;titanium dioxide wastewater;P507;V2O5} |