Cardanol-Derived Epoxy Resins as Biobased Gel Polymer Electrolytes for Potassium-Ion Conduction AITranslate
Abstract AITranslate
In this study, biobased gel polymer electrolyte (GPE) membranes were developed via the esterification reaction of a cardanol-based epoxy resin with glutaric anhydride, succinic anhydride, and hexahydro-4-methylphthalic anhydride. Nonisothermal differential scanning calorimetry was used to assess the optimal curing time and temperature of the formulations, evidencing a process activation energy of ∼65–70 kJ mol–1. A rubbery plateau modulus of 0.65–0.78 MPa and a crosslinking density of 2 × 10–4 mol cm–3 were found through dynamic mechanical analysis. Based on these characteristics, such biobased membranes were tested for applicability as GPEs for potassium-ion batteries (KIBs), showing an excellent electrochemical stability toward potassium metal in the −0.2–5 V voltage range and suitable ionic conductivity (10–3 S cm–1) at room temperature. This study demonstrates the practical viability of these biobased materials as efficient GPEs for the fabrication of KIBs, paving the path to increased sustainability in the field of next-generation battery technologies.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c00335
Chinese Library Classification Number:
Citation Information:
In this study, biobased gel polymer electrolyte (GPE) membranes were developed via the esterification reaction of a cardanol-based epoxy resin with glutaric anhydride, succinic anhydride, and hexahydro-4-methylphthalic anhydride. Nonisothermal differential scanning calorimetry was used to assess the optimal curing time and temperature of the formulations, evidencing a process activation energy of ∼65–70 kJ mol–1. A rubbery plateau modulus of 0.65–0.78 MPa and a crosslinking density of 2 × 10–4 mol cm–3 were found through dynamic mechanical analysis. Based on these characteristics, such biobased membranes were tested for applicability as GPEs for potassium-ion batteries (KIBs), showing an excellent electrochemical stability toward potassium metal in the −0.2–5 V voltage range and suitable ionic conductivity (10–3 S cm–1) at room temperature. This study demonstrates the practical viability of these biobased materials as efficient GPEs for the fabrication of KIBs, paving the path to increased sustainability in the field of next-generation battery technologies.
quote
| GB/T 7714-2015 | [1] Eleonora Manarin, Francesca Corsini, Sabrina Trano, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00335. |
| MLA | [1] Eleonora Manarin, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00335. |
| APA | [1] Eleonora Manarin, Francesca Corsini, Sabrina Trano, Lucia Fagiolari, Julia Amici, Carlotta Francia, Silvia Bodoardo, Stefano Turri, Federico Bella, & Gianmarco Griffini. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00335 |
| IEEE | [1] Eleonora Manarin, Francesca Corsini, Sabrina Trano, Lucia Fagiolari, Julia Amici, Carlotta Francia, Silvia Bodoardo, Stefano Turri, Federico Bella, and Gianmarco Griffini, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00335. keywords: {biobased epoxy resins;cardanolbased polymers;biobased polymer membranes;succinic anhydride;gel polymer electrolytes;Show More} |