A Sulfonated All-Aromatic Polyamide for Heavy Metal Capture: A Model Study with Pb(II) AITranslate

The University of North Carolina at Chapel Hill; The University of North Carolina at Chapel Hill; The University of North Carolina at Chapel Hill; The University of North Carolina at Chapel Hill
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Polyelectrolytes are widely used in heavy metal removal, finding applications as coagulants and flocculants. We compare the heavy metal removal capability of a water-soluble sulfonated semirigid polyamide, poly(2,2′-disulfonyl-4,4′-benzidine isophthalamide) (PBDI), with that of a well-known random-coil polymer, poly(sodium 4-styrenesulfonate) (PSS). Using lead (Pb(II)) as a model contaminant, both polymers precipitate out from solution at ∼500 mg/L Pb(II) in water. The ability to remove Pb(II) from water was quantified using adsorption isotherms and fitted with Langmuir and Freundlich adsorption models. The sorption of Pb(II) by PSS fit the Langmuir model with a high degree of correlation (0.976 R2), but the sorption of Pb(II) by PBDI could not be accurately predicted using the Langmuir or Freundlich model. The sorption of Pb(II) by PBDI and PSS was compared by normalizing sorption by the number of sulfonate groups of each polymer and the ion exchange capacity (IEC), found by titration. We find that PBDI removes a greater amount of Pb(II) per gram of sorbent compared to PSS, 410 mg/g vs 260 mg/g, respectively, which cannot be accounted for by differences in IEC or number of sulfonate groups. Our findings confirm that the positioning of the sulfonate groups and the rigidity of the polymer backbone play an important role in how Pb(II) coordinates to the polymer prior to precipitating out from solution.

KeyWords AITranslate

sulfonated allaromatic polymer precipitation adsorption ion exchange Pb(II) removal
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01796

Chinese Library Classification Number:

Citation Information:

Polyelectrolytes are widely used in heavy metal removal, finding applications as coagulants and flocculants. We compare the heavy metal removal capability of a water-soluble sulfonated semirigid polyamide, poly(2,2′-disulfonyl-4,4′-benzidine isophthalamide) (PBDI), with that of a well-known random-coil polymer, poly(sodium 4-styrenesulfonate) (PSS). Using lead (Pb(II)) as a model contaminant, both polymers precipitate out from solution at ∼500 mg/L Pb(II) in water. The ability to remove Pb(II) from water was quantified using adsorption isotherms and fitted with Langmuir and Freundlich adsorption models. The sorption of Pb(II) by PSS fit the Langmuir model with a high degree of correlation (0.976 R2), but the sorption of Pb(II) by PBDI could not be accurately predicted using the Langmuir or Freundlich model. The sorption of Pb(II) by PBDI and PSS was compared by normalizing sorption by the number of sulfonate groups of each polymer and the ion exchange capacity (IEC), found by titration. We find that PBDI removes a greater amount of Pb(II) per gram of sorbent compared to PSS, 410 mg/g vs 260 mg/g, respectively, which cannot be accounted for by differences in IEC or number of sulfonate groups. Our findings confirm that the positioning of the sulfonate groups and the rigidity of the polymer backbone play an important role in how Pb(II) coordinates to the polymer prior to precipitating out from solution.

quote

GB/T 7714-2015 [1] Anna C. Fraser, Jacob Yankey, Orlando Coronell, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01796.
MLA [1] Anna C. Fraser, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01796.
APA [1] Anna C. Fraser, Jacob Yankey, Orlando Coronell, & Theo J. Dingemans. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01796
IEEE [1] Anna C. Fraser, Jacob Yankey, Orlando Coronell, and Theo J. Dingemans, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01796. keywords: {sulfonated allaromatic polymer;precipitation;adsorption;ion exchange;Pb(II) removal}