Biopolypropylene-Based Wood Plastic Composites Reinforced with Mango Peel Flour and Compatibilized with an Environmentally Friendly Copolymer from Itaconic Acid AITranslate
Abstract AITranslate
This work reports on the successful development of biopolypropylene/mango peel flour (bioPP/MPF) composites using extrusion and injection molding processes. The compatibility between bioPP and MPF is improved through the use of PP-g-IA (3 phr) as a compatibilizer (which is prepared by reactive extrusion REX) and dicumyl peroxide (DCP) (1 phr) as a cross-linker. The mechanical, morphological, thermal, thermomechanical, chemical, colorimetric, water absorption, and flowability properties are characterized and analyzed. The results show that MPF (30 wt %) compatibilized with PP-g-IA and DCP increased the stiffness of bioPP in terms of Young’s modulus values. Elongation at break also shows very promising results, with a maximum value of almost 30% for the bioPP/MPF/PP-g-IA/DCP sample. PP-g-IA and DCP seem to exert a synergetic effect. Thermal stability is also improved as a result of these additives, as well as crystallinity, which is increased due to an heterogeneous nucleation phenomenon, enhanced by a higher dispersion of MPF particles in the matrix. Moreover, the excellent mechanical results are verified in FESEM images, where a very narrow gap between the MPF particles and the bioPP matrix is appreciated.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c00373
Chinese Library Classification Number:
Citation Information:
This work reports on the successful development of biopolypropylene/mango peel flour (bioPP/MPF) composites using extrusion and injection molding processes. The compatibility between bioPP and MPF is improved through the use of PP-g-IA (3 phr) as a compatibilizer (which is prepared by reactive extrusion REX) and dicumyl peroxide (DCP) (1 phr) as a cross-linker. The mechanical, morphological, thermal, thermomechanical, chemical, colorimetric, water absorption, and flowability properties are characterized and analyzed. The results show that MPF (30 wt %) compatibilized with PP-g-IA and DCP increased the stiffness of bioPP in terms of Young’s modulus values. Elongation at break also shows very promising results, with a maximum value of almost 30% for the bioPP/MPF/PP-g-IA/DCP sample. PP-g-IA and DCP seem to exert a synergetic effect. Thermal stability is also improved as a result of these additives, as well as crystallinity, which is increased due to an heterogeneous nucleation phenomenon, enhanced by a higher dispersion of MPF particles in the matrix. Moreover, the excellent mechanical results are verified in FESEM images, where a very narrow gap between the MPF particles and the bioPP matrix is appreciated.
quote
| GB/T 7714-2015 | [1] Jaume GomezCaturla, Rafael Balart, Juan IvorraMartinez, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00373. |
| MLA | [1] Jaume GomezCaturla, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00373. |
| APA | [1] Jaume GomezCaturla, Rafael Balart, Juan IvorraMartinez, Daniel GarciaGarcia, Franco Dominici, Debora Puglia, & Luigi Torre. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00373 |
| IEEE | [1] Jaume GomezCaturla, Rafael Balart, Juan IvorraMartinez, Daniel GarciaGarcia, Franco Dominici, Debora Puglia, and Luigi Torre, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00373. keywords: {polymer composites;biopolymers;reinforcements;mango peel flour;compatibilization} |