Chemical Doping of Well-Dispersed P3HT Thin-Film Nanowire Networks AITranslate

The University of Southern Mississippi; The University of Southern Mississippi; The University of Southern Mississippi; The University of Southern Mississippi; The University of Southern Mississippi; The University of Southern Mississippi
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We demonstrate the preparation of uniformly distributed poly(3-hexylthiophene) (P3HT) nanowire (NW) networks on a variety of substrates. We studied changes in the optical, electronic, and morphological properties upon sequential doping by 2,3,5,6-tetrafluoro-7,7,8,8-tetracyanoquinodimethane (F4TCNQ) by UV–vis spectroscopy, atomic force microscopy (AFM), Kelvin probe force microscopy (KPFM), and electrical conductivity measurements. At a moderate dopant concentration of 250 μg/mL, the P3HT NW networks retain their morphological features with a clear evolution of an absorption band corresponding to doping products. Higher dopant concentrations (∼1 mg/mL) lead to the accumulation of dopant molecules on the surface of the film, forming “dot-like” features. KPFM measurements show a clear difference in the contact potential difference (CPD) of the P3HT NWs with varying doping concentration regimes. Moreover, an increase in the electrical conductivity by 4 orders of magnitude from 10–5 to 10–1 S/cm is observed after moderate doping, demonstrating that significant doping effects can be achieved for a mostly crystalline phase of P3HT such as its nanowire form.

KeyWords AITranslate

conjugated polymers chemical doping nanowire network Kelvin probe force microscopy conductivity
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00653

Chinese Library Classification Number:

Citation Information:

We demonstrate the preparation of uniformly distributed poly(3-hexylthiophene) (P3HT) nanowire (NW) networks on a variety of substrates. We studied changes in the optical, electronic, and morphological properties upon sequential doping by 2,3,5,6-tetrafluoro-7,7,8,8-tetracyanoquinodimethane (F4TCNQ) by UV–vis spectroscopy, atomic force microscopy (AFM), Kelvin probe force microscopy (KPFM), and electrical conductivity measurements. At a moderate dopant concentration of 250 μg/mL, the P3HT NW networks retain their morphological features with a clear evolution of an absorption band corresponding to doping products. Higher dopant concentrations (∼1 mg/mL) lead to the accumulation of dopant molecules on the surface of the film, forming “dot-like” features. KPFM measurements show a clear difference in the contact potential difference (CPD) of the P3HT NWs with varying doping concentration regimes. Moreover, an increase in the electrical conductivity by 4 orders of magnitude from 10–5 to 10–1 S/cm is observed after moderate doping, demonstrating that significant doping effects can be achieved for a mostly crystalline phase of P3HT such as its nanowire form.

quote

GB/T 7714-2015 [1] Kan Tang, Lifeng Huang, Jasmine Lim, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00653.
MLA [1] Kan Tang, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00653.
APA [1] Kan Tang, Lifeng Huang, Jasmine Lim, Trishal Zaveri, Jason D. Azoulay, & Song Guo. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00653
IEEE [1] Kan Tang, Lifeng Huang, Jasmine Lim, Trishal Zaveri, Jason D. Azoulay, and Song Guo, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00653. keywords: {conjugated polymers;chemical doping;nanowire network;Kelvin probe force microscopy;conductivity}