Effects of Cold Rotary Forging on Microstructure and Mechanical Properties of Nb521 Alloy Bars AITranslate
Abstract AITranslate
The effects of cold rotary forging on the microstructure and tensile mechanical properties of Nb521 alloy bars for high temperature fasteners were investigated using metallographic microscope,electron backscatter diffractometer and tensile mechanical property test.The results show that with the increase of processing rate of cold rotary forging,the grains of the bar are elongated in the axial direction to form fibrous microstructure,the tensile mechanical properties show an obvious tendency of work hardening,and the strength gradually increases.When the bars with different processing rates are annealed in vacuum at 1 350℃for 1 h,all the microstructures are incompletely recrystallized.The recrystallization ratio of the bar with 60% processing rate is medium,but its average grain size is the smallest and its comprehensive mechanical properties are the best.The grain sizes of the core and the edge of the bar with 60% processing rate are quite different,and the strength of the core is higher than that of the edge in the hard state,but lower than that of the edge in the annealed state.
KeyWords AITranslate
1周小军,赵刚,田进鹏.一种面向航天器发动机的新型铌钨合金制备及其抗氧化涂层设计[J].空间科学学报,2016,36(1):99-105. 被引量:14
2张春基,吕宏军,贾中华,陈道勇,胡国林.铌钨合金材料在液体火箭发动机上的应用[J].宇航材料工艺,2007,37(6):57-60. 被引量:26
3张春基,胡国林.Nb521铌钨合金组织性能及其应用研究[J].宇航材料工艺,2012,42(1):105-107. 被引量:15
4夏明星,郑欣,李中奎,张军良.大规格铌钨合金棒材锻造工艺研究[J].热加工工艺,2011,40(17):112-113. 被引量:8
5王峰,郑欣,张小明,王东辉,夏明星,张于胜,李中奎.变形度对退火态Nb-W-Mo-Zr棒材金相组织和力学性能的影响[J].硬质合金,2010,27(2):102-106. 被引量:2
1周昆凤,周志明,涂坚,汪学静,罗荣,方飞松.汽车空心EPS转向轴旋锻工艺及显微组织研究[J].重庆理工大学学报:自然科学,2022,36(2):89-92.
2胡庆宽,谢茂阳,付建建,许永春,何坤.Nb521铌钨合金材料紧固件制造工艺[J].金属加工:冷加工,2023(2):36-39.
3朱宝辉,吴向东,万敏,赵刚,曹艳飞,罗文,李树荣,何季麟.航天用高温铌合金研究进展[J].中国有色金属学报,2023,33(1):1-26. 被引量:1
1卢翔,陈雯,姜楚灵.不同气氛下白云鄂博铌铁矿固相转化热力学研究[J].中国有色金属学报,2023,33(3):922-930. 被引量:1
1闫姝,潘一鸣,王庆刚,王璐,霍文龙,刘静静,张在娟,杨金龙.凹凸棒微珠对废水中孔雀石绿的吸附性能研究[J].功能材料,2018,49(3):3092-3096.
2周志明,罗天星,周昆凤,涂坚,黄伟九,汪红川,罗荣,方飞松,曹敏敏.基于Forge的空心齿轮轴毛坯旋锻工艺优化[J].锻压技术,2018,43(4):27-32. 被引量:4
3王承阳,董帝,滕宇阔,康聚磊,林婷.退火工艺对MHC钼合金板材组织和力学性能的影响[J].金属热处理,2018,43(7):180-183. 被引量:7
4李敏.钼粉分级配比对钼丝性能影响[J].中国钼业,2018,42(4):57-60. 被引量:1
5张勇,岳丽娟,焦晓亮.C17510加工率与时效工艺研究[J].世界有色金属,2018,0(9):291-292.
6杨锡阶,王时越,缪云伟.公路工程用三维复合排水网拉伸力学性能试验研究及思考[J].公路交通科技:应用技术版,2018,14(5):153-155. 被引量:2
7朱军,任文亮.Cu-10Cr-0.1Zr原位复合材料的制备工艺和性能研究[J].热加工工艺,2017,46(22):126-129.
8刘炳南,胡耀君,夏广祥.BT3—1合金棒材挤压工艺研究[J].稀有金属材料与工程,1983,0(4):31-34.
9舒洋,张喜燕,余江平,谭力,尹瑞森,刘庆.镁合金疲劳后的拉伸力学行为(英文)[J].中国有色金属学报:英文版,2018,28(5):896-901. 被引量:3
10刘炳成.降低熔盐结晶率[J].当代化工研究,2018(8):106-107.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.416[金属学及工艺—金属材料]
Citation Information:
The effects of cold rotary forging on the microstructure and tensile mechanical properties of Nb521 alloy bars for high temperature fasteners were investigated using metallographic microscope,electron backscatter diffractometer and tensile mechanical property test.The results show that with the increase of processing rate of cold rotary forging,the grains of the bar are elongated in the axial direction to form fibrous microstructure,the tensile mechanical properties show an obvious tendency of work hardening,and the strength gradually increases.When the bars with different processing rates are annealed in vacuum at 1 350℃for 1 h,all the microstructures are incompletely recrystallized.The recrystallization ratio of the bar with 60% processing rate is medium,but its average grain size is the smallest and its comprehensive mechanical properties are the best.The grain sizes of the core and the edge of the bar with 60% processing rate are quite different,and the strength of the core is higher than that of the edge in the hard state,but lower than that of the edge in the annealed state.
quote
| GB/T 7714-2015 | [1] XIN Meng-ming, LV Yi-ge, LI Shou-ping, et al. Effects of Cold Rotary Forging on Microstructure and Mechanical Properties of Nb521 Alloy Bars[J]. Rare Metals and Cemented Carbides, 2018(4): 37-42. |
| MLA | [1] XIN Meng-ming, et al., "Effects of Cold Rotary Forging on Microstructure and Mechanical Properties of Nb521 Alloy Bars." Rare Metals and Cemented Carbides, no. 4, 2018, pp. 37-42. |
| APA | [1] XIN Meng-ming, LV Yi-ge, LI Shou-ping, ZHANG Xiao, WANG Hui, HAN Wei-songa, HU Xiao-chen, & Shen Li-hua. (2018). Effects of Cold Rotary Forging on Microstructure and Mechanical Properties of Nb521 Alloy Bars. Rare Metals and Cemented Carbides(4), 37-42. |
| IEEE | [1] XIN Meng-ming, LV Yi-ge, LI Shou-ping, ZHANG Xiao, WANG Hui, HAN Wei-songa, HU Xiao-chen, and Shen Li-hua, "Effects of Cold Rotary Forging on Microstructure and Mechanical Properties of Nb521 Alloy Bars," Rare Metals and Cemented Carbides, no. 4, pp. 37-42, 2018. keywords: {Nb521 alloy;cold rotary forging;processing rate;microstructure;tensile mechanical property} |