Sol-Gel Synthesis of YAG:Ho3+,Yb3+ Nanocrystal AITranslate

School of Light Industry, Hebei University of Technology;School of Light Industry, Hebei University of Technology;School of Light Industry, Hebei University of Technology;School of Light Industry, Hebei University of Technology;School of Light Industry, Hebei University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

YAG:Ho^3+,1%Yb^3+nanocrystal was synthesized by a sol-gel process from the mixed solution containing aluminum nitrate and rare earth oxide. The technological conditions to synthesize its xerogel were determined by orthogonal tests. DTA-TG,XRD and TEM techniques were used to study the synthe- sis process of the xerogel and characterize the crystal structure and morphology of the prepared YAG.1 Ho3+ , 1%Yb3+. The results show that monophase YAG crystallite can be formed without any intermediate phase after calciningthe xerogel at 1 200℃ Absorption spectrum and upconversion emission spectrum of YAG. 1 % Ho3+, 1% Yh3+ nanocrystal were investigated. Yb3+ ions have the function of transferring energy in the luminescence process. Contributed to the Ho^3+ transition, strong red and green upconversion fluorescence can be observed centered at 650 nm and 540 nm,respectively.

KeyWords AITranslate

sol-gel YAG:Ho^3+ Yb^3+ nanocrystal upconversion luminescence

1李江,吴玉松,潘裕柏,刘文斌,安丽琼,王士维,郭景坤.固相反应法制备高浓度掺杂Nd:YAG激光透明陶瓷及其性能[J].硅酸盐学报,2007,35(12):1600-1604. 被引量:13

2杨建虎,戴世勋,姜中宏.稀土离子的上转换发光及研究进展[J].物理学进展,2003,23(3):284-298. 被引量:70

3戴世勋,厉旭杰,聂秋华,徐铁峰,沈祥,王训四.Yb^(3+)敏化的Er^(3+)/Ho^(3+)共掺碲酸盐玻璃的上转换发光研究[J].物理学报,2007,56(9):5518-5525. 被引量:12

1徐嘉林,金维召,刘旺,彭海益,刘贺,李春,林海,刘景和,曾繁明.Ho,Yb:Tb_3Ga_5O_(12)纳米粉体制备及发光性能研究[J].中国光学,2015,8(4):608-614. 被引量:6

1刘旺,董玮利,王殿巍,李春,林海,曾繁明.共沉淀法合成Ho:BaY_2F_8粉体的研究[J].长春理工大学学报:自然科学版,2015,38(5):76-79. 被引量:3

2刘金金,徐明祥.氧化硅薄膜中掺杂Tb^(3+)离子的发光敏化[J].发光学报,2016,37(12):1464-1470. 被引量:1

3刘艳花,拜文霞,耿中荣,冯利邦.Sr_3Al_2O_6∶Tb^(3+),Yb^(3+)荧光粉的近红外量子剪裁效应[J].发光学报,2017,38(4):423-429. 被引量:4

4沈正皓,吴以恒,张丽萍,刘洪伟,李春.溶胶凝胶法制备TGG纳米粉体与结构研究[J].长春理工大学学报:自然科学版,2017,40(3):112-116.

5刘晓辉,马世童,郑克志,秦伟平.基于合作能量传递的Sm^(2+)离子上转换发光[J].发光学报,2017,38(11):1413-1419. 被引量:3

6赖凤琴,李嘉鹏,吴有福生,胡美兰,肖青辉,姚庆林,夏李斌,叶信宇,游维雄.烧结温度和掺杂浓度对Y_4Zr_3O_(12)∶Eu^(3+)荧光粉发光性质的影响[J].发光学报,2017,38(11):1436-1442. 被引量:4

1邱深玉,余唯,王宵静.熔盐法制备条件对NaYF_4∶Eu^(3+)晶体的影响及发光性能研究[J].人工晶体学报,2016,45(3):639-644.

2吴凌晖,吴嘉达,伍长征,李富铭.金属表面激光烧蚀的发射光谱分析[J].应用激光,1994,14(4):149-152. 被引量:1

3郭永廉,初真林,任兵,谷松海.光学薄膜发射光谱分析中的标样应用[J].光学机械,1989(3):35-40.

4满宝元,王象泰,胡燮荣,许炳章.激光烧蚀金属表面产生的发射光谱分析[J].光学学报,1997,17(2):161-165. 被引量:10

5王文春,吴彦,李学初.氮气中电晕放电高能电子密度沿反应器分布的光谱研究[J].大连理工大学学报,1998,38(2):162-165. 被引量:1

6申丽华,于春侠,闫蓓,张成孝.低电压下氮气放电的发射光谱分析[J].光谱学与光谱分析,2015,35(3):791-795. 被引量:5

7姚红兵,孟春梅,张永康,佟艳群,管海兵.多脉冲高能量强激光诱导产生Al等离子体发射光谱分析[J].强激光与粒子束,2011,23(8):2111-2115. 被引量:3

8王文春,吴彦,李学初.(SO_2,N_2)气体中脉冲放电SO发射光谱测量实验研究[J].分子科学学报,1999,15(1):3-7. 被引量:2

9邸建华.Ge激活SrCl2单晶的发射光谱[J].发光快报,1993(6):45-48.

10光谱分析与光谱测量[J].中国光学,1995,0(1):14-16.

Basic Information:

DOI:

Chinese Library Classification Number:O482.31[理学—固体物理]

Citation Information:

YAG:Ho^3+,1%Yb^3+nanocrystal was synthesized by a sol-gel process from the mixed solution containing aluminum nitrate and rare earth oxide. The technological conditions to synthesize its xerogel were determined by orthogonal tests. DTA-TG,XRD and TEM techniques were used to study the synthe- sis process of the xerogel and characterize the crystal structure and morphology of the prepared YAG.1 Ho3+ , 1%Yb3+. The results show that monophase YAG crystallite can be formed without any intermediate phase after calciningthe xerogel at 1 200℃ Absorption spectrum and upconversion emission spectrum of YAG. 1 % Ho3+, 1% Yh3+ nanocrystal were investigated. Yb3+ ions have the function of transferring energy in the luminescence process. Contributed to the Ho^3+ transition, strong red and green upconversion fluorescence can be observed centered at 650 nm and 540 nm,respectively.

quote

GB/T 7714-2015 [1] LI Feng-feng, ZHANG Ming-xi, SHEN Yi, et al. Sol-Gel Synthesis of YAG:Ho3+,Yb3+ Nanocrystal[J]. Rare Metals and Cemented Carbides, 2009(4): 1-6.
MLA [1] LI Feng-feng, et al., "Sol-Gel Synthesis of YAG:Ho3+,Yb3+ Nanocrystal." Rare Metals and Cemented Carbides, no. 4, 2009, pp. 1-6.
APA [1] LI Feng-feng, ZHANG Ming-xi, SHEN Yi, WANG Shao-yan, & Charles Christopher Sorrell. (2009). Sol-Gel Synthesis of YAG:Ho3+,Yb3+ Nanocrystal. Rare Metals and Cemented Carbides(4), 1-6.
IEEE [1] LI Feng-feng, ZHANG Ming-xi, SHEN Yi, WANG Shao-yan, and Charles Christopher Sorrell, "Sol-Gel Synthesis of YAG:Ho3+,Yb3+ Nanocrystal," Rare Metals and Cemented Carbides, no. 4, pp. 1-6, 2009. keywords: {sol-gel;YAG:Ho^3+,Yb^3+;nanocrystal;upconversion luminescence}