Experimental Study on Decomposition of Tungsten Smelting Slag for Emission Reduction and Resource Recycling AITranslate
Abstract AITranslate
Tungsten smelting slag produced by smelting with NaOH and phosphoric acid of wolframite and scheelite mixed ore was treated with hydrochloric acid as a decomposition reagent,to achieve the goal of impurity removal and tungsten maximum enrichment.The results show that WO3 content in the slag increases from the initial 2.56% to 9.35%,which is nearly 3 times higher under the optimal conditions of liquid-solid(hydrochloric acid solution-tungsten smelting slag) ratio 10∶1,reaction time 3 h,temperature 60 ℃ and hydrochloric acid concentration 2 mol/L.In the acid reaction process,there is no significant tungsten loss,and 91.02% tungsten remains in the slag.The mass of the slag obtained from acid reaction is reduced to one quarter of the original tungsten slag,and it can be mixed with tungsten concentrate for secondary smelting,which effectively realizes emission reduction and resource recycling of tungsten slag and resolves the problem of tungsten smelting slag accumulation.
KeyWords AITranslate
1王明.钨冶炼离子交换工艺技术的研究进展[J].稀有金属与硬质合金,2013,41(6):13-16. 被引量:8
2肖勇军,王昶.我国钨金属资源开发利用发展趋势研究[J].矿冶工程,2007,27(3):107-110. 被引量:6
3李会强,唐忠阳,何利华,陈星宇.离子交换技术在钨冶金中的应用与进展[J].中国钨业,2014,29(5):34-39. 被引量:13
4朱海玲,邓海波,吴承桧,何小民.钨渣的综合回收利用技术研究现状[J].中国钨业,2010,25(4):15-18. 被引量:25
5杨少华,王君,谢宝如,赖晓晖,王浩然.低品位钨渣处理工艺[J].有色金属科学与工程,2015,6(6):29-32. 被引量:10
1廖春发,王良辉,霍瑞浩,谢岁,郭少毓,刘德刚.碱煮黑钨渣还原熔炼回收有价金属的研究[J].稀有金属与硬质合金,2021,49(5):7-12.
2龚丹丹,李祖怡,张勇,万林生,任嗣利.钨渣回收利用技术研究现状[J].稀有金属与硬质合金,2021,49(6):1-8. 被引量:2
3张金祥,罗教生,管建红,洪侃,黄叶钿,普建,李忠岐,陈远林,郭学益.我国钨渣处理现状与研究进展[J].中国钨业,2021,36(6):62-70.
4陈远林,郭学益,王亲猛,田庆华,张金祥,黄少波.黑钨精矿碱浸渣理化与环境特性及有价金属回收工艺[J].中国有色金属学报:英文版,2022,32(5):1638-1649.
1彭伟,黄健,王振杰,刘安荣.钨冶炼渣中有价金属回收利用研究现状[J].化工进展,2022,41(12):6656-6663.
2李祖怡,张勇,郑彬涛,侯志明,龚丹丹.碱分解钨渣硫酸浸出的正交试验研究[J].稀有金属与硬质合金,2023,51(1):1-4.
1许必晏.川法小曲酒中药材入曲对小曲清香白酒酒质影响研究[J].酿酒,2020,47(3):97-98. 被引量:2
2杨建东.石墨烯增韧结构陶瓷材料研究进展[J].化学与粘合,2020,42(3):220-224. 被引量:1
3郑洁,郑纯辉,关晓鸽,康少杰.从赤泥中回收氧化钪的技术研究现状[J].轻金属,2020(3):1-4. 被引量:7
4韩知为.聚焦再生资源回收利用、探索废铜回收再生新出路[J].中国金属通报,2020(7):1-4. 被引量:4
5王涛,宿宇.污泥机械化堆肥工程中的配混料系统[J].西南给排水,2020,42(3):54-60.
6刘玮,葛来福,徐玉涛.城市配网自动化及其配网规划的应用分析[J].电子乐园,2019(32):0205-0205.
7林吓宁.某钢铁厂除尘灰综合利用提取次氧化锌环境影响分析[J].海峡科学,2020,0(4):47-49. 被引量:3
8张盈,潘冬,罗敏,刘晨明,林晓.钼精矿冶炼废水的综合治理技术[J].当代化工研究,2020(11):116-118.
9唐义胜.湖南某尾矿综合回收可行性报告[J].电子乐园,2019,0(32):0493-0494.
10王慧,陈佳颖.初中生物学实验“骨的成分与骨的特性”中脱钙试剂的研究[J].中学生物教学,2020(8):52-54.
Basic Information:
DOI:
Chinese Library Classification Number:TF841.1[冶金工程—有色金属冶金]
Citation Information:
Tungsten smelting slag produced by smelting with NaOH and phosphoric acid of wolframite and scheelite mixed ore was treated with hydrochloric acid as a decomposition reagent,to achieve the goal of impurity removal and tungsten maximum enrichment.The results show that WO3 content in the slag increases from the initial 2.56% to 9.35%,which is nearly 3 times higher under the optimal conditions of liquid-solid(hydrochloric acid solution-tungsten smelting slag) ratio 10∶1,reaction time 3 h,temperature 60 ℃ and hydrochloric acid concentration 2 mol/L.In the acid reaction process,there is no significant tungsten loss,and 91.02% tungsten remains in the slag.The mass of the slag obtained from acid reaction is reduced to one quarter of the original tungsten slag,and it can be mixed with tungsten concentrate for secondary smelting,which effectively realizes emission reduction and resource recycling of tungsten slag and resolves the problem of tungsten smelting slag accumulation.
quote
| GB/T 7714-2015 | [1] FAN Ze-kun, HUANG Chao, XU Guo-zuan, et al. Experimental Study on Decomposition of Tungsten Smelting Slag for Emission Reduction and Resource Recycling[J]. Rare Metals and Cemented Carbides, 2020(2): 1-4. |
| MLA | [1] FAN Ze-kun, et al., "Experimental Study on Decomposition of Tungsten Smelting Slag for Emission Reduction and Resource Recycling." Rare Metals and Cemented Carbides, no. 2, 2020, pp. 1-4. |
| APA | [1] FAN Ze-kun, HUANG Chao, XU Guo-zuan, YANG Zheng-feng, HU Jia-yuan, TANG Xiao-jiang, & LIANG Yong. (2020). Experimental Study on Decomposition of Tungsten Smelting Slag for Emission Reduction and Resource Recycling. Rare Metals and Cemented Carbides(2), 1-4. |
| IEEE | [1] FAN Ze-kun, HUANG Chao, XU Guo-zuan, YANG Zheng-feng, HU Jia-yuan, TANG Xiao-jiang, and LIANG Yong, "Experimental Study on Decomposition of Tungsten Smelting Slag for Emission Reduction and Resource Recycling," Rare Metals and Cemented Carbides, no. 2, pp. 1-4, 2020. keywords: {tungsten smelting slag;acid decomposition;tungsten enrichment;emission reduction;resource recycling;secondary resource} |