Study on the Extraction and Separation of Scandium by N503-P204 and TBP-P204 Synergistic Extraction Systems AITranslate
Abstract AITranslate
In order to separate Sc and impurity ions from titanium white waste acid,the extraction and separation behaviors of Sc,Ti,Fe and Al from titanium white waste acid by N503-P204 and TBP-P204 synergistic extraction systems were studied.The results show that the Sc extraction rates in the systems of 5%N503+5%P204+90%sulfonated kerosene and 5%TBP+5%P204+90%sulfonated kerosene are 99.74%and 99.73%,respectively by two-stage countercurrent extraction under the conditions of 25℃and O/A=1∶20.In the N503-P204 synergistic extraction system,99.34%Ti is eluted with 1 mol/L phosphoric acid through two-stage countercurrent washing under the conditions of 35℃and O/A=1∶2,while only 66.22%Ti is eluted in TBP-P204 synergistic extraction system under the same conditions.Combined with infrared characterization,it is confirmed that the extraction and separation efficiency of N503-P204 synergistic extraction system on Sc is superior to that of TBP-P204 synergistic extraction system.In N503-P204 synergistic extraction system,when 2 mol/L sodium hydroxide is used for stripping under the conditions of 50℃and O/A=3∶1,Sc stripping rate reaches 99.28%,while Fe,Al and other impurities are left in the organic phase,realizing Sc recovery.
KeyWords AITranslate
Basic Information:
DOI:
Chinese Library Classification Number:TF804.2[冶金工程—有色金属冶金]
Citation Information:
In order to separate Sc and impurity ions from titanium white waste acid,the extraction and separation behaviors of Sc,Ti,Fe and Al from titanium white waste acid by N503-P204 and TBP-P204 synergistic extraction systems were studied.The results show that the Sc extraction rates in the systems of 5%N503+5%P204+90%sulfonated kerosene and 5%TBP+5%P204+90%sulfonated kerosene are 99.74%and 99.73%,respectively by two-stage countercurrent extraction under the conditions of 25℃and O/A=1∶20.In the N503-P204 synergistic extraction system,99.34%Ti is eluted with 1 mol/L phosphoric acid through two-stage countercurrent washing under the conditions of 35℃and O/A=1∶2,while only 66.22%Ti is eluted in TBP-P204 synergistic extraction system under the same conditions.Combined with infrared characterization,it is confirmed that the extraction and separation efficiency of N503-P204 synergistic extraction system on Sc is superior to that of TBP-P204 synergistic extraction system.In N503-P204 synergistic extraction system,when 2 mol/L sodium hydroxide is used for stripping under the conditions of 50℃and O/A=3∶1,Sc stripping rate reaches 99.28%,while Fe,Al and other impurities are left in the organic phase,realizing Sc recovery.
quote
| GB/T 7714-2015 | [1] ZHANG Yu-qian, LI Zhi-hua, ZHAO Zhong-wei. Study on the Extraction and Separation of Scandium by N503-P204 and TBP-P204 Synergistic Extraction Systems[J]. Rare Metals and Cemented Carbides, 2025(1): 1-11. |
| MLA | [1] ZHANG Yu-qian, et al., "Study on the Extraction and Separation of Scandium by N503-P204 and TBP-P204 Synergistic Extraction Systems." Rare Metals and Cemented Carbides, no. 1, 2025, pp. 1-11. |
| APA | [1] ZHANG Yu-qian, LI Zhi-hua, & ZHAO Zhong-wei. (2025). Study on the Extraction and Separation of Scandium by N503-P204 and TBP-P204 Synergistic Extraction Systems. Rare Metals and Cemented Carbides(1), 1-11. |
| IEEE | [1] ZHANG Yu-qian, LI Zhi-hua, and ZHAO Zhong-wei, "Study on the Extraction and Separation of Scandium by N503-P204 and TBP-P204 Synergistic Extraction Systems," Rare Metals and Cemented Carbides, no. 1, pp. 1-11, 2025. keywords: {scandium;synergistic extraction;N503;P204;TBP;titanium white waste acid} |