Modeling of molar volume for the Ni–Al γ/γ′ binary phases within the framework of CALPHAD method AITranslate

Shanghai Polytechnic University; Shanghai University; Shanghai University; Shanghai University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Assisted by the first-principles calculations, the molar volumes of γ and γ′ phases in the binary Ni–Al system were modeled within the framework of the CALPHAD method. A CALPHAD database integrating thermodynamic and molar volume descriptions was established. The present Ni–Al binary database was validated to make good predictions of molar volumes/lattice parameters and thermal expansivities for both γ and γ′ phases. The predicted γ/γ′ lattice misfits from low to high temperatures turn out to be reasonable.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.calphad.2020.101792

Chinese Library Classification Number:

Citation Information:

Assisted by the first-principles calculations, the molar volumes of γ and γ′ phases in the binary Ni–Al system were modeled within the framework of the CALPHAD method. A CALPHAD database integrating thermodynamic and molar volume descriptions was established. The present Ni–Al binary database was validated to make good predictions of molar volumes/lattice parameters and thermal expansivities for both γ and γ′ phases. The predicted γ/γ′ lattice misfits from low to high temperatures turn out to be reasonable.

quote

GB/T 7714-2015 [1] NaQiong Zhu, Wei Liu, ZhiChao Wang, et al. Calphad, 2020(71). DOI:10.1016/j.calphad.2020.101792.
MLA [1] NaQiong Zhu, et al., Calphad, no. 71, 2020, https://doi.org/10.1016/j.calphad.2020.101792.
APA [1] NaQiong Zhu, Wei Liu, ZhiChao Wang, & XiaoGang Lu. (2020). Calphad(71). https://doi.org/10.1016/j.calphad.2020.101792
IEEE [1] NaQiong Zhu, Wei Liu, ZhiChao Wang, and XiaoGang Lu, Calphad, no. 71, 2020, doi: 10.1016/j.calphad.2020.101792.