Process consistency and control are bottleneck issues to wider insertion of powder-bed fusion additive manufacturing in the industrial shopfloor. Of particular interest is the porosity of the components, which remains the limiting factor to high-cycle fatigue performance. Recent experiments have shown that, with increasing energy density, a surge in porosity is seen in selectively laser melted metals. In this high-energy density regime, porosity must originate from mechanisms that are different from the well-known incomplete melting in the low energy density regime. To shed light on this interesting phenomenon, this paper first discusses the mechanism of bubble formation in the melt pool and possible trapping during the solidification, and then formulates a predictive model for porosity in this regime. To compare with experimental results, we perform computer modeling and simulations which have been fully validated by experiments to determine the parameters in the model. We show that the model predictions are in good qualitative and quantitative agreement with the experimental measurements. Hence, the proposed model can be used as a tool to predict the porosity, and further to control and possibly reduce porosity in laser powder-bed fusion additive manufacturing, paving the way for its wider adoption in manufacturing shopfloors. Graphical abstract Download : Download high-res image (128KB) Download : Download full-size image
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.addma.2018.05.042
Chinese Library Classification Number:
Citation Information:
Process consistency and control are bottleneck issues to wider insertion of powder-bed fusion additive manufacturing in the industrial shopfloor. Of particular interest is the porosity of the components, which remains the limiting factor to high-cycle fatigue performance. Recent experiments have shown that, with increasing energy density, a surge in porosity is seen in selectively laser melted metals. In this high-energy density regime, porosity must originate from mechanisms that are different from the well-known incomplete melting in the low energy density regime. To shed light on this interesting phenomenon, this paper first discusses the mechanism of bubble formation in the melt pool and possible trapping during the solidification, and then formulates a predictive model for porosity in this regime. To compare with experimental results, we perform computer modeling and simulations which have been fully validated by experiments to determine the parameters in the model. We show that the model predictions are in good qualitative and quantitative agreement with the experimental measurements. Hence, the proposed model can be used as a tool to predict the porosity, and further to control and possibly reduce porosity in laser powder-bed fusion additive manufacturing, paving the way for its wider adoption in manufacturing shopfloors. Graphical abstract Download : Download high-res image (128KB) Download : Download full-size image
quote
| GB/T 7714-2015 | [1] G. Vastola, Q.X. Pei, Y.W. Zhang. Additive Manufacturing, 2018(22). DOI:10.1016/j.addma.2018.05.042. |
| MLA | [1] G. Vastola, et al., Additive Manufacturing, no. 22, 2018, https://doi.org/10.1016/j.addma.2018.05.042. |
| APA | [1] G. Vastola, Q.X. Pei, & Y.W. Zhang. (2018). Additive Manufacturing(22). https://doi.org/10.1016/j.addma.2018.05.042 |
| IEEE | [1] G. Vastola, Q.X. Pei, and Y.W. Zhang, Additive Manufacturing, no. 22, 2018, doi: 10.1016/j.addma.2018.05.042. |