Application of Phosphonazo Developer in the Analysis of Metals and Alloys AITranslate

Zhongnan University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The latest development of application of phosphonazo developer in the analysis of metals and alloys is described. Colouring reaction conditions. something about the inspection limit. interference and measuring scope of the related spectrophotometry are presented in the paper.

KeyWords AITranslate

metal alloy phosphonazo application

1徐军,张恒陆.直读光谱仪在铸铁分析中应用[J].光谱仪器与分析,1995(2):13-18.

2段群章.金属及合金中锆(铪)的光度分析近况[J].上海有色金属,1995,16(1):35-38. 被引量:5

3段群章.钡和锶的光度分析[J].湖南有色金属,1995,11(4):50-52. 被引量:4

4段群章.金属及合金中铋的光度分析近况[J].有色矿冶,1994,10(3):51-56. 被引量:6

5段群章.钾和钠的光度分析近况[J].新疆有色金属,1993,0(4):32-35.

6段群章.金属及合金中铜的光度分析近况[J].湖南有色金属,1994,10(4):241-246.

7段群章.噻唑偶氮显色剂在金属及合金分析中的应用[J].广西冶金,1995(1):41-44.

8段群章.吡啶偶氮显色剂在金属及合金分析中的应用[J].甘肃有色金属,1995(2):1-6.

9段群章.罗丹明B类显色剂在稀有金属分析中应用近况[J].新疆有色金属,1998,21(3):30-35.

10段群章.米氏硫酮类化合物及其在光度分析中的应用[J].有色金属与稀土应用,1995(1):30-36. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TG115.335[金属学及工艺—物理冶金]

Citation Information:

The latest development of application of phosphonazo developer in the analysis of metals and alloys is described. Colouring reaction conditions. something about the inspection limit. interference and measuring scope of the related spectrophotometry are presented in the paper.

quote

GB/T 7714-2015 [1] DUAN Qun-zhang. Application of Phosphonazo Developer in the Analysis of Metals and Alloys[J]. Rare Metals and Cemented Carbides, 1995(3): 34-41.
MLA [1] DUAN Qun-zhang. "Application of Phosphonazo Developer in the Analysis of Metals and Alloys." Rare Metals and Cemented Carbides, no. 3, 1995, pp. 34-41.
APA [1] DUAN Qun-zhang. (1995). Application of Phosphonazo Developer in the Analysis of Metals and Alloys. Rare Metals and Cemented Carbides(3), 34-41.
IEEE [1] DUAN Qun-zhang, "Application of Phosphonazo Developer in the Analysis of Metals and Alloys," Rare Metals and Cemented Carbides, no. 3, pp. 34-41, 1995. keywords: {metal, alloy, phosphonazo, application}