Experimental Study on Drilling Axial Force during Drilling Machining of Molybdenum Alloys AITranslate

School of Machinery and Materials Engineering, Northern University of Technology;School of Machinery and Materials Engineering, Northern University of Technology;School of Machinery and Materials Engineering, Northern University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The drilling axial force and drilling torque during drilling machining of molybdenum alloys with different drilling parameters were measured by experiments.The effect of feed speed and spindle speed on drilling axial force and drilling torque was analyzed.The results indicate that with constant feed rate and changed spindle speed,the drilling axial force slightly decreases with the increase of spindle speed,and the drilling torque also decreases with the increase of spindle speed.With constant spindle speed and changed feed rate,both drilling axial force and drilling torque increase with feed rate increasing.Feed rate has more significant influence on drilling axial force and drilling torque than spindle speed.

KeyWords AITranslate

Mo alloy drilling machining drilling parameter drilling axial force drilling torque

1刘刚,张国君,江峰,丁向东,孙院军,王林,罗建海,孙军.高性能钼合金的微观组织设计制备与性能优化[J].中国材料进展,2016,35(3):205-211. 被引量:15

2王海云,李文平,彭红,姚春臣,常海,段良辉,阮滢滢.钼合金零件螺纹车削的两种工艺方法[J].国防制造技术,2016(1):7-10. 被引量:2

3张青来,李敏,韩寅奔,韩伟东,冯甜甜.交叉轧制钼带冷深冲性能及微观组织研究[J].稀有金属材料与工程,2012,41(12):2109-2112. 被引量:8

4石俊,刘宁,刘爱军,陈新杰,马力.钼及钼合金研究的进展[J].热处理,2014,29(5):19-23. 被引量:13

5陈闯,魏世忠,张国赏,徐流杰.钼合金的研究现状与应用进展[J].稀有金属与硬质合金,2012,40(5):45-50. 被引量:21

6王玉凤,李付国,赵伟,刘趁意,付静波.基于热加工图的钼金属热变形特征研究[J].稀有金属材料与工程,2009,38(8):1358-1362. 被引量:9

1刘东,周开祥.钼合金钻削工艺参数正交试验研究[J].工具技术,2021,55(3):40-43.

1孙巧如,刘晓东,王天晨,姚文昊,张杰,班晓伟.纤维增强复合材料钻削加工技术研究现状[J].玻璃钢/复合材料,2017(9):101-105. 被引量:3

2周宇航,胡平,常恬,邓洁,胡卜亮,王快社,冯鹏发.钼合金强韧化方式及机理研究进展[J].功能材料,2018,49(1):1026-1032. 被引量:14

3以硅基新材料为代表的战新产业发展迅猛[J].铁合金,2017,48(10):23-23.

4王明海,印文典,王奔,张枢南.钻削参数对CFRP/Ti叠层材料钻削温度的影响[J].机械设计与制造,2017(12):98-101. 被引量:4

5谭栓斌,贾先.超声波混合超细粉末制备TZM钼合金性能的研究[J].电子世界,2018,0(1):137-138. 被引量:1

6毛百忍.建设工程中钻孔灌注桩钻孔过程中塌孔成因分析及处理方案[J].中国高新区,2017,0(16):185-185.

7铝合金轮毂生产工艺[J].铝加工,2017,0(6):64-64.

8谢一兵,王守城,薛超旭.基于FLUENT的辊压机破碎过程动态分析[J].矿山机械,2018,46(1):31-34. 被引量:1

9陈永亮,彭涛,刘德帅,王志江.面向现场加工的全液压驱动主轴水下钻孔特性建模与优化方法[J].中国机械工程,2018,29(4):471-476. 被引量:3

10张明俊.钻孔灌注桩在卵石层中的漏浆处理[J].城市建设理论研究:电子版,2017,0(27):127-127. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TG506.1[金属学及工艺—金属切削加工及机床]

Citation Information:

The drilling axial force and drilling torque during drilling machining of molybdenum alloys with different drilling parameters were measured by experiments.The effect of feed speed and spindle speed on drilling axial force and drilling torque was analyzed.The results indicate that with constant feed rate and changed spindle speed,the drilling axial force slightly decreases with the increase of spindle speed,and the drilling torque also decreases with the increase of spindle speed.With constant spindle speed and changed feed rate,both drilling axial force and drilling torque increase with feed rate increasing.Feed rate has more significant influence on drilling axial force and drilling torque than spindle speed.

quote

GB/T 7714-2015 [1] LIU Dong, WANG Fang, ZHOU Peng. Experimental Study on Drilling Axial Force during Drilling Machining of Molybdenum Alloys[J]. Rare Metals and Cemented Carbides, 2018(1): 33-35.
MLA [1] LIU Dong, et al., "Experimental Study on Drilling Axial Force during Drilling Machining of Molybdenum Alloys." Rare Metals and Cemented Carbides, no. 1, 2018, pp. 33-35.
APA [1] LIU Dong, WANG Fang, & ZHOU Peng. (2018). Experimental Study on Drilling Axial Force during Drilling Machining of Molybdenum Alloys. Rare Metals and Cemented Carbides(1), 33-35.
IEEE [1] LIU Dong, WANG Fang, and ZHOU Peng, "Experimental Study on Drilling Axial Force during Drilling Machining of Molybdenum Alloys," Rare Metals and Cemented Carbides, no. 1, pp. 33-35, 2018. keywords: {Mo alloy;drilling machining;drilling parameter;drilling axial force;drilling torque}