Research Progress on Quality Control of Ultrafine WC Powder Prepared with Traditional Methods AITranslate

Zigong Cemented Carbide Co.,Ltd.;Zigong Cemented Carbide Co.,Ltd.;Zigong Cemented Carbide Co.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The research progress on quality control of APT calcination, tungsten oxide reduction and W powder carbonization in the preparation process of high-quality ultrafine WC powder is reviewed.The qua-lity of APT raw material and the control of process parameters in the production process are the key to the preparation of ultrafine WC powder.APT with single property is beneficial to control the quality of calcined products, and optimizing calcination process parameters can avoid entrained hard particles.It is di-fficult to control consistent reaction conditions in the reduction process of tungsten oxide.When the heterogeneous reactions simultaneously occur, the key is to control the formation and reduction of WO2 and the growth of W powder.The uniformity of both composition and grain size of WC particles should be con-sidered in the carbonization process.

KeyWords AITranslate

ultrafine WC powder quality control APT calcination tungsten oxide reduction W powder carbonization

1张卫兵,刘向中,陈振华,陈鼎,彭程.WC-Co硬质合金最新进展[J].稀有金属,2015,39(2):178-186. 被引量:63

2陈杉杉.高性能超细碳化钨粉质量影响因素探讨[J].硬质合金,2019,36(5):337-344. 被引量:7

3高晓菊,满鹏,汪海东,白荣,李国斌,张涛.碳化钨硬质合金制备技术研究进展[J].硅酸盐通报,2013,32(1):71-76. 被引量:9

4陈绍衣.用W_(18)O_(49)制造超细钨粉及超细碳化钨粉[J].中南工业大学学报,1997,28(5):456-460. 被引量:14

5刘光耀.蒸发结晶条件与仲钨酸铵物理性能的关系[J].稀有金属与硬质合金,1991(3):15-17. 被引量:5

6陈世瑞.钨及仲钨酸铵[J].江西冶金,1997,17(5):57-60. 被引量:6

7魏勇,刘心宇,李毅夫,陈丽华.原料APT对还原蓝钨特性的影响[J].中国钨业,1996,0(7):9-14. 被引量:6

8彭卫珍.蓝钨物理性能对钨粉和碳化钨粉性能的影响[J].硬质合金,2004,21(3):142-148. 被引量:7

9傅练英.APT煅烧工艺对WC质量的影响[J].硬质合金,2006,23(1):15-20. 被引量:5

10王玥,陈杉杉,马丽丽,林高安.不同单斜仲钨酸铵在惰性气体中的热分解研究[J].中国钨业,2019,34(1):58-63. 被引量:4

1丁紫阳,白玲,晋玉霞,马宗彬.WC添加量对Ni基等离子熔覆层组织与性能的影响[J].稀有金属与硬质合金,2022,50(1):32-36. 被引量:1

2詹友基,左振,许永超,王英杰,苏乙峻.纳米硬质合金磨削温度及热量分配比例试验研究[J].机床与液压,2023,51(5):117-121.

1崔陈,朱协彬,程敬卿,刘振华,韩顺顺.等离子熔覆Fe基/WC-10Co-4Cr涂层的组织与性能研究[J].表面技术,2023,52(7):167-176. 被引量:1

1程光明.建筑工程中的框架结构施工技术运用[J].门窗,2021(7):65-66. 被引量:1

2王玉洁,路潜,金三丽,庞冬,杨萍,曹怡纬.头颈部癌症患者放射治疗期间口咽部症状管理的研究进展[J].中国护理管理,2021,21(6):936-940. 被引量:3

3潘竞虎.基于混凝土碳化过程的公路隧道衬砌寿命预测[J].山西建筑,2021,47(14):125-127. 被引量:2

4邢宇轩,郭英奎,陈磊,赵壮志,王玉金.气压浸渗法制备ZrC-W-Cu复合材料的显微组织与力学性能[J].材料工程,2021,49(7):124-132. 被引量:3

5孙志娟.建筑工程施工工序的质量控制分析探讨[J].现代物业:中旬刊,2021,20(1):73-73.

6何登武,李冠超,李小燕,王杨,王昱莹,付晓辉.CuInS_(2)光催化材料制备及光催化还原溶液中U(Ⅵ)的性能[J].有色金属工程,2021,11(7):18-24.

7林小璇,易辉平,龙本夫,张淑彬,林高安.直流电弧原子发射光谱法测定超细碳化钨中痕量元素[J].冶金分析,2021,41(5):41-45. 被引量:1

8王晓晨,张英华,宋波.粉末循环使用对3D打印钴铬合金牙冠机械性能及耐腐蚀性的影响研究[J].工具技术,2021,55(6):68-72.

9陈赦,刘红梅,吴婷,汪沨,庄池杰.低温等离子体增强催化氨合成机理的一维流体动力学模型[J].电工技术学报,2021,36(13):2730-2739. 被引量:4

10刘英杰,胡强,赵新明,王志刚,张少明,王永慧,张金辉.增材制造用高流动性铝合金粉末制备技术研究[J].稀有金属材料与工程,2021,50(5):1767-1774. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TF123[冶金工程—粉末冶金]

Citation Information:

The research progress on quality control of APT calcination, tungsten oxide reduction and W powder carbonization in the preparation process of high-quality ultrafine WC powder is reviewed.The qua-lity of APT raw material and the control of process parameters in the production process are the key to the preparation of ultrafine WC powder.APT with single property is beneficial to control the quality of calcined products, and optimizing calcination process parameters can avoid entrained hard particles.It is di-fficult to control consistent reaction conditions in the reduction process of tungsten oxide.When the heterogeneous reactions simultaneously occur, the key is to control the formation and reduction of WO2 and the growth of W powder.The uniformity of both composition and grain size of WC particles should be con-sidered in the carbonization process.

quote

GB/T 7714-2015 [1] XIE Fan, SHI Kai-hua, GU Jin-bao. Research Progress on Quality Control of Ultrafine WC Powder Prepared with Traditional Methods[J]. Rare Metals and Cemented Carbides, 2021(3): 31-36.
MLA [1] XIE Fan, et al., "Research Progress on Quality Control of Ultrafine WC Powder Prepared with Traditional Methods." Rare Metals and Cemented Carbides, no. 3, 2021, pp. 31-36.
APA [1] XIE Fan, SHI Kai-hua, & GU Jin-bao. (2021). Research Progress on Quality Control of Ultrafine WC Powder Prepared with Traditional Methods. Rare Metals and Cemented Carbides(3), 31-36.
IEEE [1] XIE Fan, SHI Kai-hua, and GU Jin-bao, "Research Progress on Quality Control of Ultrafine WC Powder Prepared with Traditional Methods," Rare Metals and Cemented Carbides, no. 3, pp. 31-36, 2021. keywords: {ultrafine WC powder;quality control;APT calcination;tungsten oxide reduction;W powder carbonization}