daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Large Gap Topological Insulating Phase and Anisotropic Rashba and Chiral Spin Textures in Monolayer Zintl A2MX2 Large Gap Topological Insulating Phase and Anisotropic Rashba and Chiral Spin Textures in Monolayer Zintl A2MX2 AITranslate

National Sun Yat-sen University; National Sun Yat-sen University; National Sun Yat-sen University; National Sun Yat-sen University; National Sun Yat-sen University; Nanyang Technological University; National Tsing Hua University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A family of two-dimensional (2D) materials, particularly the complex-structured Zintl phase compounds, has attracted tremendous research attention because of tunable material properties and exceptional applications. Utilizing first-principles computations under the hybrid functional approach, we performed a systematic study on A2MX2 (A = Ca, Sr, or Yb; M = Zn or Cd; X = P, As, Sb, or Bi). Among the three surface terminations considered, the metal element XM-termination (T2) was found to be the most stable structural phase with the lowest total ground state energies. Thermodynamic stability was further confirmed through phonon dispersion and formation energy calculations. Surprisingly, the T2 monolayer Sr2CdBi2 was found to host the topological insulating phase with a sizable bandgap of 556 meV, as well as a Z2 topological invariance of 1. The corresponding topologically protected edge states link the conduction and valence bands. Moreover, the topological phase is driven by the spin–orbit coupling, which causes the inverted bands at Γ point close to the Fermi level concerning the Cd-s + Bi2-s and Bi2-px + py orbitals. Moreover, Rashba and chiral spin-splittings were also observed. The computed Rashba strengths along Γ-M (αRΓ-M) are 1.970, 0.676, and 0.669 eV·Å, whereas the computed values along Γ-K (αRΓ-K) are 1.701, 0.731, and 0.646 eV·Å, for Ca2ZnAs2, Sr2CdBi2, and Yb2ZnAs2, respectively. Our study provides fundamental knowledge to further experimental investigations and synthesis, which may lead to electronic applications of A2MX2 compounds in quantum computing or spintronics.

KeyWords AITranslate

quantum spin Hall effect topological insulators electronic structures firstprinciples calculations A2MX2 Zintl compounds
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00984

Chinese Library Classification Number:

Citation Information:

A family of two-dimensional (2D) materials, particularly the complex-structured Zintl phase compounds, has attracted tremendous research attention because of tunable material properties and exceptional applications. Utilizing first-principles computations under the hybrid functional approach, we performed a systematic study on A2MX2 (A = Ca, Sr, or Yb; M = Zn or Cd; X = P, As, Sb, or Bi). Among the three surface terminations considered, the metal element XM-termination (T2) was found to be the most stable structural phase with the lowest total ground state energies. Thermodynamic stability was further confirmed through phonon dispersion and formation energy calculations. Surprisingly, the T2 monolayer Sr2CdBi2 was found to host the topological insulating phase with a sizable bandgap of 556 meV, as well as a Z2 topological invariance of 1. The corresponding topologically protected edge states link the conduction and valence bands. Moreover, the topological phase is driven by the spin–orbit coupling, which causes the inverted bands at Γ point close to the Fermi level concerning the Cd-s + Bi2-s and Bi2-px + py orbitals. Moreover, Rashba and chiral spin-splittings were also observed. The computed Rashba strengths along Γ-M (αRΓ-M) are 1.970, 0.676, and 0.669 eV·Å, whereas the computed values along Γ-K (αRΓ-K) are 1.701, 0.731, and 0.646 eV·Å, for Ca2ZnAs2, Sr2CdBi2, and Yb2ZnAs2, respectively. Our study provides fundamental knowledge to further experimental investigations and synthesis, which may lead to electronic applications of A2MX2 compounds in quantum computing or spintronics.

quote

GB/T 7714-2015 [1] Aniceto B. Maghirang, III, Rovi Angelo B. Villaos, Marku Nyevel R. Perez, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00984.
MLA [1] Aniceto B. Maghirang, III, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00984.
APA [1] Aniceto B. Maghirang, III, Rovi Angelo B. Villaos, Marku Nyevel R. Perez, LiangYing Feng, ZhiQuan Huang, ChiaHsiu Hsu, & FengChuan Chuang. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00984
IEEE [1] Aniceto B. Maghirang, III, Rovi Angelo B. Villaos, Marku Nyevel R. Perez, LiangYing Feng, ZhiQuan Huang, ChiaHsiu Hsu, and FengChuan Chuang, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00984. keywords: {quantum spin Hall effect topological insulators electronic structures firstprinciples calculations A2MX2 Zintl compounds}