The Latest Development of Sn-based Anode Materials in Lithium Ion Batteries AITranslate
Abstract AITranslate
The latest development of such anode materials as metal tin,Sn-based alloy and tin oxide are reviewed. The problems presented in the current study of the above anode materials are also analyzed. Multicomponent composite Sn-based alloy with a multiple buffer structure and nanometer-sized composite tin ox- idewill be the main Sn-based anode materials of lithium ion batteries.
KeyWords AITranslate
1Hong Li,Xuejie Huang,Liquan Chen,et al. A High capacity Nano-Si composite anode material for lithium rechargeable batteries[J]. Electrochemical and Solid-State Letters, 1999,2(11) :547-549.
2Zhang T,Fu L J ,Gao J. Nanosized tin anode prepared by laser-induced vapor deposition for lithium ion battery [J].Journal of Power Sources, 2007,174: 770-773.
3Xiang ming He, Weihua Pu, Li Wang. Synthesis of spherical nano tin encapsulated pyrolytic polyacry composite anode materieal for for Li-ion batteries[J]. Solid State lonics 2007,178 : 833-836.
4Courtney I A,Dahn J R. Electrochemical and in-situ Xray diffraction studies of the reaction of lithium with tin oxide eomposite[J]. J Electrochem Soc, 1997, 144 (6): 2 045.
5Ying Liang,Jing Fan,Xiaohong Xia,et al. Synthesis and characterization of SnO2 nano-single crystals as anode materials for lithium ion batteries[J]. Material Letters, 2007,61:4 370-4 373.
6Jie Song, Min-zhen Cai, Quan-Feng Dong. Structural and electrochemical characterization of SnOx thin films for Li -ion microbattery[J]. Electrochimica Acta 2009,54(10) : 2 748-2 753.
7By Min-Sik Park, Yong-Mook Kang, Gou-Xiu Wang, et al. The Effect of morphological modification on the electrochemical properties of SnO2 nanomaterial [J ]. Advanced Functional Materials, 2008,18 : 455-461.
8杨同欢,周学酬,李求忠,刘永梅.纳米Sn/SnO_2/石墨复合材料作为锂离子电池负极材料的研究[J].化工时刊,2008,22(6):1-3. 被引量:2
9Zhu X J, Geng L M,Zhang F Q,et al. Synthesis and performance of Zn2 SnO4 as anode materials for lithium ion batteries by hydrothermal method[J]. Journal of Power Sources, 2009,189 ( 1 ) : 828-831.
10Shuijin Lei, Kaibin Tang, Chunhua Chen, et al. Preparation of Mn2SnO4 nanoparticles as anode materials for lithium secondary battery [J]. Materials Research Bulletin, 2009,44(2) :393-397.
1魏巍,王久林,杨军,努丽燕娜.锂离子电池锡基负极材料的研究进展[J].化工进展,2010,29(1):80-87. 被引量:7
2陈素怡,余林,孙明,程高,郑海龙.锂离子电池硅基薄膜负极材料的研究进展[J].电源技术,2016,40(11):2260-2262. 被引量:4
3武明昊,陈剑,王崇,衣宝廉.锂离子电池负极材料的研究进展[J].电池,2011,41(4):222-225. 被引量:34
4赖新方,简弃非,赵灵智.锂离子二次电池用锡基负极材料[J].广东技术师范学院学报,2008,29(12):18-21.
5田琴,胡社军,李伟善,赵灵智.锂离子电池锡基负极材料研究现状[J].电池工业,2007,12(6):429-432. 被引量:4
6贾丰春.锂离子电池负极材料研究进展[J].辽宁化工,2011,40(11):1211-1213. 被引量:3
7万婷,穆道斌,薛欢,陈实.锂离子电池锡基负极材料的研究进展[J].材料导报,2010,24(9):117-120. 被引量:8
8倪聪,莫祥银,俞琛捷,丁毅,康彩荣.纳米磷酸铁锂的研究进展[J].化工新型材料,2010,38(5):1-4. 被引量:13
9佟健,夏华,刘明义.锂离子二次电池负极材料的发展[J].材料导报,2001,15(8):48-50.
10周训富,赵付双.钠离子电池锡基负极材料的研究进展[J].电池,2016,46(3):172-175. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TM912.9[电气工程—电力电子与电力传动]
Citation Information:
The latest development of such anode materials as metal tin,Sn-based alloy and tin oxide are reviewed. The problems presented in the current study of the above anode materials are also analyzed. Multicomponent composite Sn-based alloy with a multiple buffer structure and nanometer-sized composite tin ox- idewill be the main Sn-based anode materials of lithium ion batteries.
quote
| GB/T 7714-2015 | [1] YUAN Wan-song, TIAN Yan-wen, LIU Guo-qiang. The Latest Development of Sn-based Anode Materials in Lithium Ion Batteries[J]. Rare Metals and Cemented Carbides, 2009(4): 53-57. |
| MLA | [1] YUAN Wan-song, et al., "The Latest Development of Sn-based Anode Materials in Lithium Ion Batteries." Rare Metals and Cemented Carbides, no. 4, 2009, pp. 53-57. |
| APA | [1] YUAN Wan-song, TIAN Yan-wen, & LIU Guo-qiang. (2009). The Latest Development of Sn-based Anode Materials in Lithium Ion Batteries. Rare Metals and Cemented Carbides(4), 53-57. |
| IEEE | [1] YUAN Wan-song, TIAN Yan-wen, and LIU Guo-qiang, "The Latest Development of Sn-based Anode Materials in Lithium Ion Batteries," Rare Metals and Cemented Carbides, no. 4, pp. 53-57, 2009. keywords: {lithium ion battery;anode material;Sn-based material;nano-material} |