daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Bioactive Lactose-Modified Chitosan Acts as a Temporary Extracellular Matrix for the Formation of Chondro-Aggregates AITranslate

University of Trieste; University of Trieste; University of Trieste; University of Trieste; University of Trieste; University of Trieste; University of Trieste; University of Trieste
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Spheroids based on chondrocytes are gaining interest in the treatment of injured cartilage tissue due to their regenerative potential. In this study, chondrocyte-based aggregates were formed by culturing cells on a polymeric coating of a lactose-modified chitosan (CTL) and their evolution was followed for 14 days of culture. Morphological analyses through scanning electron microscopy indicated that these cell aggregates formed by a process of cell aggregation rather than proliferation, resulting in structures with an irregular morphology that were up to 1 mm in size. Chondrocytes interact very closely with CTL. In the early days of cellular aggregation, CTL is distributed among the cells, while in later stages, it is localized in the inner part of the aggregates, forming an amorphous matrix. The initial outer position of the polymer is replaced over time by an increased matrix deposition whose main component is type II collagen. Transmission electron microscopy pointed out that the chondrocytes internalized the polymer during the first days of culture. The presence of CTL does not affect the ability of cells to migrate from chondro-aggregates when transferred to uncoated wells, mimicking the ability of cells to colonize a cartilage defect. Overall, these results suggest that CTL plays a role as a temporary matrix for chondrocytes aggregation during chondro-aggregates formation. This opens up innovative therapeutic approaches for cartilage regeneration without the need to use a scaffold to deliver cells to the damaged site.

KeyWords AITranslate

chondrocytes spheroids lactosemodified chitosan cartilage regeneration bioactive polysaccharide
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01613

Chinese Library Classification Number:

Citation Information:

Spheroids based on chondrocytes are gaining interest in the treatment of injured cartilage tissue due to their regenerative potential. In this study, chondrocyte-based aggregates were formed by culturing cells on a polymeric coating of a lactose-modified chitosan (CTL) and their evolution was followed for 14 days of culture. Morphological analyses through scanning electron microscopy indicated that these cell aggregates formed by a process of cell aggregation rather than proliferation, resulting in structures with an irregular morphology that were up to 1 mm in size. Chondrocytes interact very closely with CTL. In the early days of cellular aggregation, CTL is distributed among the cells, while in later stages, it is localized in the inner part of the aggregates, forming an amorphous matrix. The initial outer position of the polymer is replaced over time by an increased matrix deposition whose main component is type II collagen. Transmission electron microscopy pointed out that the chondrocytes internalized the polymer during the first days of culture. The presence of CTL does not affect the ability of cells to migrate from chondro-aggregates when transferred to uncoated wells, mimicking the ability of cells to colonize a cartilage defect. Overall, these results suggest that CTL plays a role as a temporary matrix for chondrocytes aggregation during chondro-aggregates formation. This opens up innovative therapeutic approaches for cartilage regeneration without the need to use a scaffold to deliver cells to the damaged site.

quote

GB/T 7714-2015 [1] Chiara Pizzolitto, Francesca Scognamiglio, Giovanna Baldini, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01613.
MLA [1] Chiara Pizzolitto, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01613.
APA [1] Chiara Pizzolitto, Francesca Scognamiglio, Giovanna Baldini, Roberta Bortul, Gianluca Turco, Ivan Donati, Vanessa Nicolin, & Eleonora Marsich. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01613
IEEE [1] Chiara Pizzolitto, Francesca Scognamiglio, Giovanna Baldini, Roberta Bortul, Gianluca Turco, Ivan Donati, Vanessa Nicolin, and Eleonora Marsich, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01613. keywords: {chondrocytes;spheroids;lactosemodified chitosan;cartilage regeneration;bioactive polysaccharide}