Enhanced Mechanical Properties of Poly(butylene adipate-co-terephthalate)/Cellulose Nanocrystal Nanocomposites Obtained by In Situ Polymerization AITranslate

Korea Research Institute of Chemical Technology (KRICT); Korea Research Institute of Chemical Technology (KRICT); Korea Research Institute of Chemical Technology (KRICT); Korea Research Institute of Chemical Technology (KRICT); Korea Research Institute of Chemical Technology (KRICT); Korea Research Institute of Chemical Technology (KRICT);Ecovance Co., Ltd.;Ecovance Co., Ltd.; Korea Research Institute of Chemical Technology (KRICT); Chungnam National University; Kyung Hee University; Sogang University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Biodegradable plastic films, in which poly(butylene adipate-co-terephthalate) (PBAT) is a major component, play a significant role in the expansion of the sustainable plastic packaging market. Unfortunately, biodegradable films tear easily. To garner consumer attention, it is paramount that these materials not only offer sustainability benefits but also provide durability. To enhance the mechanical properties of PBAT, an in situ method that polymerizes monomers upon the addition of aqueous cellulose nanocrystal (CNC) suspensions was developed herein to directly synthesize all-organic nanocomposites. The prepared films (containing only 0.05 wt % of CNC relative to the total amount of monomers) exhibited the highest tensile strength (71 MPa) and elongation at break (1018%) reported thus far for PBAT-based composites. The composite films were processed facilely through a blown extrusion process that is suitable for mass production, and a 22% improvement in tear toughness was achieved in relation to that of neat PBAT. The composite was completely decomposed into CO2 and water under composting conditions, exhibiting excellent biodegradability. This biodegradable PBAT/CNC nanocomposite with simultaneous improvements in tensile and tear resistance properties is expected to positively contribute to the expansion of the biodegradable plastics market.

KeyWords AITranslate

in situ polycondensation poly(butylene adipatecoterephthalate) cellulose nanocrystal allorganic nanocomposite Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01694

Chinese Library Classification Number:

Citation Information:

Biodegradable plastic films, in which poly(butylene adipate-co-terephthalate) (PBAT) is a major component, play a significant role in the expansion of the sustainable plastic packaging market. Unfortunately, biodegradable films tear easily. To garner consumer attention, it is paramount that these materials not only offer sustainability benefits but also provide durability. To enhance the mechanical properties of PBAT, an in situ method that polymerizes monomers upon the addition of aqueous cellulose nanocrystal (CNC) suspensions was developed herein to directly synthesize all-organic nanocomposites. The prepared films (containing only 0.05 wt % of CNC relative to the total amount of monomers) exhibited the highest tensile strength (71 MPa) and elongation at break (1018%) reported thus far for PBAT-based composites. The composite films were processed facilely through a blown extrusion process that is suitable for mass production, and a 22% improvement in tear toughness was achieved in relation to that of neat PBAT. The composite was completely decomposed into CO2 and water under composting conditions, exhibiting excellent biodegradability. This biodegradable PBAT/CNC nanocomposite with simultaneous improvements in tensile and tear resistance properties is expected to positively contribute to the expansion of the biodegradable plastics market.

quote

GB/T 7714-2015 [1] Hyeri Kim, Hyeonyeol Jeon, Minkyung Lee, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01694.
MLA [1] Hyeri Kim, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01694.
APA [1] Hyeri Kim, Hyeonyeol Jeon, Minkyung Lee, SeulA Park, SeonMi Kim, Sung Bae Park, Kyung Youn Kim, Seong Dong Kim, Dongyeop X. Oh, Jun Mo Koo, Sung Yeon Hwang, & Jeyoung Park. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01694
IEEE [1] Hyeri Kim, Hyeonyeol Jeon, Minkyung Lee, SeulA Park, SeonMi Kim, Sung Bae Park, Kyung Youn Kim, Seong Dong Kim, Dongyeop X. Oh, Jun Mo Koo, Sung Yeon Hwang, and Jeyoung Park, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01694. keywords: {in situ polycondensation;poly(butylene adipatecoterephthalate);cellulose nanocrystal;allorganic nanocomposite;Show More}