High-Performance Pure Red Quasi-Two-Dimensional Perovskite Light-Emitting Diodes with Bifunctional Potassium Trifluoroacetate Additive AITranslate

Xinyu University; Huazhong University of Science and Technology; Huazhong University of Science and Technology; Huazhong University of Science and Technology; Huazhong University of Science and Technology; Huazhong University of Science and Technology; Nanchang University; Huazhong University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Solution-processed pure iodide-based quasi-two-dimensional (quasi-2D) perovskites exhibit tremendous potential for pure red light-emitting diodes, required for a wide color gamut display. However, the nonradiative recombination derived from the numerous defects and broad phase distribution restricts the performance of quasi-2D perovskite light-emitting diodes (PeLEDs). Herein, we demonstrate high-performance pure red quasi-2D PeLEDs by introducing a bifunctional potassium trifluoroacetate (KTFA) additive that simultaneously passivates the defects and regulates phase distribution. The KTFA-modified PeLEDs achieve a peak external quantum efficiency of 18.70%, a maximum luminance of 2377.1 cd m–2, and an electroluminescence (EL) emission peak at 650 nm with a CIE coordinate of (0.705,0.295) approaching the pure red emission of Rec.2020 standard. Moreover, our devices demonstrate a stable EL spectrum and a half-lifetime (T50) of 476 min at an initial luminance of 100 cd m–2. Our work provides a viable strategy to boost the performance of quasi-2D PeLEDs.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c00557

Chinese Library Classification Number:

Citation Information:

Solution-processed pure iodide-based quasi-two-dimensional (quasi-2D) perovskites exhibit tremendous potential for pure red light-emitting diodes, required for a wide color gamut display. However, the nonradiative recombination derived from the numerous defects and broad phase distribution restricts the performance of quasi-2D perovskite light-emitting diodes (PeLEDs). Herein, we demonstrate high-performance pure red quasi-2D PeLEDs by introducing a bifunctional potassium trifluoroacetate (KTFA) additive that simultaneously passivates the defects and regulates phase distribution. The KTFA-modified PeLEDs achieve a peak external quantum efficiency of 18.70%, a maximum luminance of 2377.1 cd m–2, and an electroluminescence (EL) emission peak at 650 nm with a CIE coordinate of (0.705,0.295) approaching the pure red emission of Rec.2020 standard. Moreover, our devices demonstrate a stable EL spectrum and a half-lifetime (T50) of 476 min at an initial luminance of 100 cd m–2. Our work provides a viable strategy to boost the performance of quasi-2D PeLEDs.

quote

GB/T 7714-2015 [1] Yunhui Kuang, Lvpeng Yang, Junming Ma, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00557.
MLA [1] Yunhui Kuang, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00557.
APA [1] Yunhui Kuang, Lvpeng Yang, Junming Ma, Tong Bie, Di Zhang, Yazhuo Xue, Naigen Zhou, & Ming Shao. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00557
IEEE [1] Yunhui Kuang, Lvpeng Yang, Junming Ma, Tong Bie, Di Zhang, Yazhuo Xue, Naigen Zhou, and Ming Shao, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00557.