The Latest Development of Pretreatment of Refractory Gold Ores AITranslate

School of Chemistry, Central South University;School of Chemistry, Central South University;School of Chemistry, Central South University;School of Chemistry, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The gold resources in China and present status of pretreatment process of various refractory gold ores are reviewed. Analysis is made of the characteristics of the pretreatment technologies such as roasting oxidization,pressure oxidization, bio-oxidization, chemical oxidization and microwave heating. It is pointed out that the microwave pretreatment, characterized by uniform heating and low energy Consumption, is a very promising pretreatment method for refractory gold ores.

KeyWords AITranslate

refractory gold ores pretreatment process microwave latest development

1李智伟.难浸金矿处理工艺新进展[J].有色金属设计,1998,25(3):10-15. 被引量:12

2张秀华.难选冶金矿石预处理工艺现状[J].湿法冶金,1998(3):13-18. 被引量:25

3李俊萌.难处理金矿石预处理工艺及其选择[J].有色金属:选矿部分,2002(5):16-23. 被引量:17

4王力军,刘春谦.难处理金矿石预处理技术综述[J].黄金,2000,21(1):38-45. 被引量:87

5Breed A W, Hansford G S. Studies on the mechanism and kinetics of bioleaching [J]. Minerals Engineering, 1999, 12(4) : 383-392.

6陈红波,封国宁,李铁球.含碳金矿的次氯酸盐预处理氰化浸出研究[J].铀矿冶,1993,12(4):252-255. 被引量:4

7黎铉海,粟海锋,黄祖强,邱冠周,王淀佐.次氯酸钠一步法浸金的原理与试验研究[J].化工矿物与加工,2001,30(1):15-18. 被引量:10

8Linge H G. Eletrolytic process for refractory arsenopyritic gold ores[J]. Minerals engineering, 1995,18 ( 11 ) : 1 327-1 332.

9Linge H G, Welham N J. Gold recovery from a refractory arsenopyrite (FeAsS) concentrate byin-situ slurry oxidation[J]. Minerals Engineering, 1997,10 ( 6 ) : 557 - 567.

10Arslan Fatma. Electro-oxidation of pyrite in sodium chloride solutions[J]. Hydrometallurgy, 1997,46:157- 170.

1拜鹏程,何烨,陈芳芳,李科科.磨矿细度和二浸二洗对氰化浸出率影响的试验研究[J].黄金科学技术,2012,20(5):71-73. 被引量:7

2邓善芝,曾小波,熊文良.某金银铜矿综合利用新工艺研究[J].中国矿业,2014,23(12):103-107. 被引量:3

3唐立靖,唐云,许正波.难选金矿微波预处理边磨边浸非氰化试验研究[J].黄金科学技术,2015,23(1):85-89. 被引量:7

4陈伟,丁德馨,胡南,李峰.微波焙烧预处理难浸含金硫精矿[J].中国有色金属学报,2015,25(7):2000-2005. 被引量:13

5李鹏程,代淑娟,李晓安,郭小飞,王倩倩.金的氰化物在白云母表面的吸附研究[J].辽宁科技大学学报,2021,44(5):379-385.

6张勋,王国强,陈周,王云伟,罗思岗.硫精矿焙砂提金及铜锌综合回收试验研究[J].矿冶,2022,31(1):77-84.

7赵旭,杨晓峰.高硫富砷难处理金矿焙烧预处理工艺研究进展[J].化工矿物与加工,2023,52(6):38-44.

8李鹏程,代淑娟.硫代硫酸金与高岭石的搅拌吸附试验研究[J].化工矿物与加工,2019,48(3):31-34.

9杨凤云.难处理金矿石预处理工艺[J].科技传播,2013,5(6):107-108. 被引量:7

1何烨,拜鹏程,黄冠银,张先军,陈芳芳,孙美芬.酸浸提高金氰化浸出率的试验研究[J].黄金科学技术,2012,20(6):58-61. 被引量:6

2杨建,王建平.氰化系统阶段提高金精矿磨矿细度的生产实践[J].黄金科学技术,2013,21(4):91-94. 被引量:1

3徐忠敏,沈述保,李学强,叶树峰.氰化磨矿浸出工艺优化试验研究[J].黄金科学技术,2013,21(5):140-144. 被引量:3

4徐名特,孟德铭,代淑娟.难选金预处理工艺研究现状[J].有色矿冶,2014,30(2):18-21. 被引量:5

5陈水波,谢洪珍,赖伟强,郭金溢,阴菡.新疆某金矿重选—氰化联合工艺应用研究[J].黄金科学技术,2014,22(6):87-90. 被引量:6

6邢晴晴,杨长平,任琪.青海某金矿选矿厂扩能改造实践[J].黄金科学技术,2015,23(4):52-56. 被引量:6

7唐立靖,唐云,李娇娇,杨典奇.微细浸染型金矿硫脲—硫氰酸铵浸出研究[J].黄金科学技术,2015,23(4):97-101. 被引量:1

8杨雨山,喻清,胡南,丁德馨.微波加热预处理堆浸铀矿石[J].稀有金属,2016,40(3):280-286. 被引量:9

9马方通,高利坤,董方,陈龙.难处理金矿预处理及强化氰化技术研究现状及进展[J].黄金,2016,0(4):51-55. 被引量:19

10杨雨山,喻清,胡南,丁德馨.微波预处理对堆浸铀尾渣中铀浸出行为的影响及机理[J].中国有色金属学报,2016,26(6):1356-1363. 被引量:7

1雷占昌,虞洁,马红蕊.难处理金矿预处理技术现状及进展[J].现代矿业,2014,30(5):23-24. 被引量:3

2王坚,冯之艾.难处理金矿石的焙烧氧化[J].世界采矿快报,1995,11(7):11-14. 被引量:1

3杨凤云.难处理金矿石预处理工艺[J].科技传播,2013,5(6):107-108. 被引量:7

4关自斌.Progera金矿[J].国外黄金参考,1995(2):18-25.

5肉孜汗.高硫、高砷难选金精矿的处理[J].新疆有色金属,2011,34(3):49-49.

6李俊萌.难处理金矿石预处理工艺及其选择[J].有色金属:选矿部分,2002(5):16-23. 被引量:17

7崔毅琦,王凯,孟奇,童雄.含砷难处理金矿提金工艺的研究现状[J].矿冶,2015,24(1):31-34. 被引量:20

8吴浩,黄万抚,邱峰,胡雪飞.硫氰酸盐浸金研究进展[J].贵金属,2016,37(3):72-78. 被引量:5

9Twin Creeks金矿用加压氧化工艺处理难浸碳质矿的进展[J].国外黄金参考,1997(3):34-36.

10初明,陈振强.含砷难处理金矿研究进展[J].科技资讯,2014,12(20):85-85.

Basic Information:

DOI:

Chinese Library Classification Number:TD921[矿业工程—选矿]

Citation Information:

The gold resources in China and present status of pretreatment process of various refractory gold ores are reviewed. Analysis is made of the characteristics of the pretreatment technologies such as roasting oxidization,pressure oxidization, bio-oxidization, chemical oxidization and microwave heating. It is pointed out that the microwave pretreatment, characterized by uniform heating and low energy Consumption, is a very promising pretreatment method for refractory gold ores.

quote

GB/T 7714-2015 [1] ZHANG Wen-xuan, ZHONG Hong, FU Jian-gang, et al. The Latest Development of Pretreatment of Refractory Gold Ores[J]. Rare Metals and Cemented Carbides, 2008(3): 62-66.
MLA [1] ZHANG Wen-xuan, et al., "The Latest Development of Pretreatment of Refractory Gold Ores." Rare Metals and Cemented Carbides, no. 3, 2008, pp. 62-66.
APA [1] ZHANG Wen-xuan, ZHONG Hong, FU Jian-gang, & WEN Zhen-qian. (2008). The Latest Development of Pretreatment of Refractory Gold Ores. Rare Metals and Cemented Carbides(3), 62-66.
IEEE [1] ZHANG Wen-xuan, ZHONG Hong, FU Jian-gang, and WEN Zhen-qian, "The Latest Development of Pretreatment of Refractory Gold Ores," Rare Metals and Cemented Carbides, no. 3, pp. 62-66, 2008. keywords: {refractory gold ores pretreatment process;microwave latest development}