Dissolution Properties of Ammonium Paratungstate and Effects of Tungstophosphate Acid Formation in (NH_4)_2HPO_4-H_2O System AITranslate

School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Dissolution properties of ammonium paratungstate(APT)in (NH4)2HPO4-H2O system were studied with dissolution equilibrium method.The results show that the solubility of APT decreases with the increase of(NH4)2HPO4 concentration at the temperature of70℃,but increases with the increase of(NH4)2HPO4 concentration at the temperature of70℃.The formation of tungstophosphate acid at high temperature is the main reason for a substantial increase of APT solubility and dissolution rate.

KeyWords AITranslate

ammonium paratungstate(APT) diammonium hydrogen phosphate (NH4)2HPO4-H2O system dissolution property tungstophosphate acid dissolution equilibrium method

1US Department of the Interior, US Geological Survey. Mineral commodity summaries 2012 [Z]. Washington, DC:US Department of the Interior, US Geological Sur vey, 2012 : 198.

2李俊萌.中国钨矿资源浅析[J].中国钨业,2009,24(6):9-13. 被引量:60

3薛鉴.钨冶炼工业50年回顾及面向新世纪的思考[J].中国钨业,1999,14(5):130-135. 被引量:5

4李洪茂,时友东,刘忠,王宝金,王泽利,邱希萍.东昆仑山若羌地区白干湖钨锡矿床地质特征及成因[J].地质通报,2006,25(1):277-281. 被引量:33

5黄小娥,史维全.我国钨矿地质勘查新进展[J].中国钨业,2007,22(3):6-9. 被引量:15

6万林生,晏慧娟,肖学有,陈帮明,王辉.我国钨冶炼离子交换工艺的技术发展与工艺评价[J].中国钨业,2003,18(6):31-33. 被引量:20

7万林生,邓登飞,赵立夫,李红超,徐国钻,梁勇.钨绿色冶炼工艺研究方向和技术进展[J].有色金属科学与工程,2013,4(5):15-18. 被引量:18

8万林生,赵立夫,李红超.崇义章源钨业APT绿色冶炼的技术进步和发展[J].中国钨业,2012,27(1):47-49. 被引量:13

9万林生,赵立夫,黄泽辉,等.一种铵盐分解白钨矿的方法:中国,CN102154547B[P].2013-01-16.

10WAN Linsheng, XU Zhifeng, and SHI ZhonglingFaculty of Materials and Chemical Engineering, Southern Institute of Metallurgy, Ganzhou 341000, China.Solubility of ammonium paratungstate in the system NH_3·H_2O·H_2O[J].稀有金属:英文版,2003,22(1):10-13. 被引量:3

1万林生,金先文,赖星任,杨亮,刘鹏,梁勇.(NH_4)_2HPO_4-NH_3·H_2O-H_2O系APT溶解度研究[J].稀有金属与硬质合金,2016,44(5):6-10. 被引量:1

1田德柱,饶泽文,欧阳臻,陈永明,叶龙刚.含铁钨粉酸溶除铁的研究[J].稀有金属与硬质合金,2019,47(6):5-9.

1贺华,黄维农,王学魁,朱亮,孙之南,韩梅.扎布耶盐湖卤水碳酸锂溶解度和过饱和度研究[J].盐业与化工,2011,40(1):15-18.

2彭芸,曾英,周琳,李元波.三元体系NaVO_3-H_2NCONH_2-H_2O 298K相平衡及平衡液相物化性质研究[J].矿物岩石,2005,25(2):118-120. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TQ136.13[化学工程—无机化工]

Citation Information:

Dissolution properties of ammonium paratungstate(APT)in (NH4)2HPO4-H2O system were studied with dissolution equilibrium method.The results show that the solubility of APT decreases with the increase of(NH4)2HPO4 concentration at the temperature of70℃,but increases with the increase of(NH4)2HPO4 concentration at the temperature of70℃.The formation of tungstophosphate acid at high temperature is the main reason for a substantial increase of APT solubility and dissolution rate.

quote

GB/T 7714-2015 [1] WAN Lin-sheng, ZHANG Long-hui, LAI Xing-ren, et al. Dissolution Properties of Ammonium Paratungstate and Effects of Tungstophosphate Acid Formation in (NH_4)_2HPO_4-H_2O System[J]. Rare Metals and Cemented Carbides, 2016(3): 1-4.
MLA [1] WAN Lin-sheng, et al., "Dissolution Properties of Ammonium Paratungstate and Effects of Tungstophosphate Acid Formation in (NH_4)_2HPO_4-H_2O System." Rare Metals and Cemented Carbides, no. 3, 2016, pp. 1-4.
APA [1] WAN Lin-sheng, ZHANG Long-hui, LAI Xing-ren, YANG Liang, LIANG Yong, & LIU Peng. (2016). Dissolution Properties of Ammonium Paratungstate and Effects of Tungstophosphate Acid Formation in (NH_4)_2HPO_4-H_2O System. Rare Metals and Cemented Carbides(3), 1-4.
IEEE [1] WAN Lin-sheng, ZHANG Long-hui, LAI Xing-ren, YANG Liang, LIANG Yong, and LIU Peng, "Dissolution Properties of Ammonium Paratungstate and Effects of Tungstophosphate Acid Formation in (NH_4)_2HPO_4-H_2O System," Rare Metals and Cemented Carbides, no. 3, pp. 1-4, 2016. keywords: {ammonium paratungstate(APT);diammonium hydrogen phosphate;(NH4)2HPO4-H2O system;dissolution property;tungstophosphate acid;dissolution equilibrium method}