Moiré M-Nitridanes (M = Al, B, Ga) Analogues of Carbon Diamanes: Ab Initio Investigation of Atomic Structures, Electronic, and Mechanical Properties Moiré M-Nitridanes (M = Al, B, Ga) Analogues of Carbon Diamanes: Ab Initio Investigation of Atomic Structures, Electronic, and Mechanical Properties AITranslate

Emanuel Institute of Biochemical Physics RAS; Ulyanovsk State University; National Research Nuclear University “MEPhI”; National Research Nuclear University “MEPhI”
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

With an emphasis on remarkable properties, twisted vertical heterostructures have received particular attention in experimental and theoretical works. They have promising unknown effects in science and technology. These twisted systems can be considered a platform for the formation of crystalline film structures. In this paper, we consider one of them, diamond-like crystals with Moiré atomic structure formed from twisted two-dimensional hexagonal layers. Analogues of carbon Moiré diamanes are nanometer-thick films obtained by both stacking and twisting near 30° of two functionalized monolayers of nitrides (AlN, BN, GaN), which have already been actually obtained. We study their energetically stable atomic configurations and electronic and elastic properties. The proposed hydrogenated and/or fluorinated (second side, Janus structures) Moiré nitridane nanostructures with a twisted angle of 27.8° possess a wide band gap from 3 to 4 eV. Electronic band structures are characterized by many flattened bands located near the edges of the valence and conduction bands, which tend to be signatures of Moiré superlattices. The Moiré nitridanes can be used as a base for two-dimensional semiconductors with low-dispersive flattened bands and strong localization of the electronic states, which should increase the probability of their resonant IV characteristics and light excitations. Thus, the circumstance is useful for nano- and optoelectronic resonant devices. In addition, it was found that hydrogenated and fluorinated Moiré nitridane and nitride films have some very different elastic responses, which are attractive for mechanoelectric applications.

KeyWords AITranslate

Moiré bilayers twisted layers van der Waals heterostructures nitridanes DFT
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c01015

Chinese Library Classification Number:

Citation Information:

With an emphasis on remarkable properties, twisted vertical heterostructures have received particular attention in experimental and theoretical works. They have promising unknown effects in science and technology. These twisted systems can be considered a platform for the formation of crystalline film structures. In this paper, we consider one of them, diamond-like crystals with Moiré atomic structure formed from twisted two-dimensional hexagonal layers. Analogues of carbon Moiré diamanes are nanometer-thick films obtained by both stacking and twisting near 30° of two functionalized monolayers of nitrides (AlN, BN, GaN), which have already been actually obtained. We study their energetically stable atomic configurations and electronic and elastic properties. The proposed hydrogenated and/or fluorinated (second side, Janus structures) Moiré nitridane nanostructures with a twisted angle of 27.8° possess a wide band gap from 3 to 4 eV. Electronic band structures are characterized by many flattened bands located near the edges of the valence and conduction bands, which tend to be signatures of Moiré superlattices. The Moiré nitridanes can be used as a base for two-dimensional semiconductors with low-dispersive flattened bands and strong localization of the electronic states, which should increase the probability of their resonant IV characteristics and light excitations. Thus, the circumstance is useful for nano- and optoelectronic resonant devices. In addition, it was found that hydrogenated and fluorinated Moiré nitridane and nitride films have some very different elastic responses, which are attractive for mechanoelectric applications.

quote

GB/T 7714-2015 [1] Leonid A. Chernozatonskii, Aleksey I. Kochaev, Konstantin P. Katin, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c01015.
MLA [1] Leonid A. Chernozatonskii, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c01015.
APA [1] Leonid A. Chernozatonskii, Aleksey I. Kochaev, Konstantin P. Katin, & Mikhail M. Maslov. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c01015
IEEE [1] Leonid A. Chernozatonskii, Aleksey I. Kochaev, Konstantin P. Katin, and Mikhail M. Maslov, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c01015. keywords: {Moiré bilayers twisted layers van der Waals heterostructures nitridanes DFT}