Commercial scale Test of Selective Precipitation for Removal of Mo,As and Sn from Tungstate Solution AITranslate
Abstract AITranslate
with M 115 reagent,good results for removal of the Mo and other impurities from commercial tungstate solution are obtained. The Mo removal rate can reach 97%~99% for commercial (NH 4) 2WO 4 stripped solution containing Mo 0.56~1.75g/L. Besides, As and Sn can also be removed after evaporation crystallization of the purified (NH 4) 2WO 4 solution, the resultant APT can conform to GB 10116-88APT-0 standard at 95.5%~98.7% crystallization rate. Meanwhile it results in a very simple and effective method to recover the NH 4Cl and WO 3 from mother crystal solution and to decrease the “three wastes” discharge
KeyWords AITranslate
1李洪桂 孙培梅 等.-[J].中国钨业,1998,4:17-17.
2李洪桂 刘茂盛 等.-[J].中国科学基金,1997,11(3):210-210.
1曹佐英,张启修.钨钼分离研究进展[J].稀有金属,2004,28(6):1076-1081. 被引量:13
2李荣敏.浅谈硬质合金轧辊在钢铁轧制技术中的应用[J].中国科技博览,2010(34):277-278.
3孙培梅,李洪桂,李运姣,苏鹏抟,赵中伟,霍广生,刘茂盛.APT结晶母液处理新工艺[J].中南工业大学学报,2000,31(1):27-29. 被引量:7
4李运姣,李洪桂,孙培梅,苏鹏抟,赵中伟,霍广生,刘茂盛.选择性沉淀法从钨酸钠溶液中除钼[J].稀有金属,2000,24(5):356-359. 被引量:6
5朱来东,鲁兴武,易超,何国才.废旧催化剂中多金属综合回收工艺研究[J].有色金属:冶炼部分,2014(7):35-37. 被引量:2
6肖连生,张启修,龚柏藩,黄芍英.密实移动床——流化床离子交换除钼技术在工业上的应用[J].中国钨业,2001,16(2):26-29. 被引量:21
7孙培梅,李洪桂,李运姣,苏鹏抟,霍广生,赵中伟,刘茂盛.选择性沉淀法从钨酸盐溶液中除钼的工业试验[J].中国有色金属学报,2001,11(3):499-502. 被引量:22
8张邦胜,肖连生,张启修.沉淀法分离钨钼的研究进展[J].江西有色金属,2001,15(2):26-29. 被引量:7
9赵中伟,何利华.地球化学对钨钼分离的借鉴[J].中国有色金属学报,2014,24(6):1637-1647. 被引量:3
10关文娟,张贵清,肖连生,张启修,李晓宇,张互标.双氧水配合TRPO/TBP萃取分离钨钼的工业试验[J].稀有金属,2015,39(11):1030-1037. 被引量:4
1赵中伟,李江涛,曹才放,霍广生,陈爱良,李洪桂.从钼酸盐溶液中深度除去杂质钨的研究[J].稀有金属与硬质合金,2008,36(1):1-4. 被引量:4
2吕莹,孙放.Fe(OH)_3吸附法从高钨钼酸钠溶液中分离钨钼的研究[J].稀有金属与硬质合金,2005,33(3):1-3. 被引量:19
3文颖频,熊洁羽.钨钼分离的研究与进展[J].湖南冶金,2005,33(6):8-11. 被引量:7
4李洪桂,赵中伟.我国钨冶金技术的进步——纪念中国钨业100年[J].中国钨业,2007,22(6):7-10. 被引量:15
5赵小翠,郑明东,黄宪法,桂林.废催化剂中钼和钨的溶剂萃取分离研究[J].中国钼业,2008,32(2):28-32. 被引量:4
6韩青涛,赵良仁,张春雷,杜志明,杨洁.我国铀矿冶领域应用的离子交换塔[J].湿法冶金,2008,27(3):176-180. 被引量:9
7胡凯光,陈祥标,谭凯旋,杨金辉,汪爱河.流化床离子交换从含铀废水中吸附铀[J].有色金属,2008,60(4):88-90. 被引量:3
8余晓皎,姚秉华,周孝德,范薇,李鹏.N503为载体的支撑液膜体系中Mo(Ⅵ)的传输[J].稀有金属,2008,32(5):654-658. 被引量:2
9刘铁梅.钨酸钠溶液Na_2S除钼工艺的改进[J].稀有金属与硬质合金,2009,37(1):27-31. 被引量:2
10肖清清,杨天林,陈虎兵,麻建军.仲钨酸铵生产工艺中钼的分离[J].无机盐工业,2009,41(10):53-55. 被引量:4
1孙培梅,李洪桂,李运姣,苏鹏抟,霍广生,赵中伟,刘茂盛.选择性沉淀法从钨酸盐溶液中除钼的工业试验[J].中国有色金属学报,2001,11(3):499-502. 被引量:22
2姜萍,徐迎春.钨钼分离方法的研究现状与发展[J].世界有色金属,2000(10):16-17. 被引量:1
3邓舜勤.离子交换法提取钨的新工艺[J].湿法冶金,1996,15(1):34-38. 被引量:7
4李洪桂,孙培梅,李运姣,起中伟,苏鹏抟,刘茂盛.选择性沉淀法从钨酸盐溶液中除钼、砷、锑、锡等杂质的研究[J].中国钨业,1998,13(4):17-19. 被引量:19
5冶金过程强化学科组.“选择性沉淀法从钨酸盐溶液中除钼、砷、锡、锑”专利技术的新进展[J].中国钨业,2000,15(4):29-30. 被引量:7
6李运姣,李洪桂,孙培梅,苏鹏抟,赵中伟,霍广生,刘茂盛.选择性沉淀法从钨酸钠溶液中除钼[J].稀有金属,2000,24(5):356-359. 被引量:6
7谭柯.选择性沉淀法从废催化剂中回收金属钯的研究[J].湖南冶金,2002,30(3):17-20. 被引量:9
8侯静,杨绍利,吴恩辉,李军.含镓生铁电解法回收镓铁试验研究[J].湿法冶金,2013,32(4):256-258. 被引量:2
9张邦胜,肖连生,张启修.沉淀法分离钨钼的研究进展[J].江西有色金属,2001,15(2):26-29. 被引量:7
10霍广生,孙培梅,贾根贵.关于钨钼分离的可能方法[J].稀有金属与硬质合金,1997,25(1):52-56. 被引量:12
Basic Information:
DOI:
Chinese Library Classification Number:TF841.103[冶金工程—有色金属冶金]
Citation Information:
with M 115 reagent,good results for removal of the Mo and other impurities from commercial tungstate solution are obtained. The Mo removal rate can reach 97%~99% for commercial (NH 4) 2WO 4 stripped solution containing Mo 0.56~1.75g/L. Besides, As and Sn can also be removed after evaporation crystallization of the purified (NH 4) 2WO 4 solution, the resultant APT can conform to GB 10116-88APT-0 standard at 95.5%~98.7% crystallization rate. Meanwhile it results in a very simple and effective method to recover the NH 4Cl and WO 3 from mother crystal solution and to decrease the “three wastes” discharge
quote
| GB/T 7714-2015 | [1] LI Yun-jiao, LI Hong-gui, SUN Pei-mei, et al. Commercial scale Test of Selective Precipitation for Removal of Mo,As and Sn from Tungstate Solution[J]. Rare Metals and Cemented Carbides, 1999(3): 1-4. |
| MLA | [1] LI Yun-jiao, et al., "Commercial scale Test of Selective Precipitation for Removal of Mo,As and Sn from Tungstate Solution." Rare Metals and Cemented Carbides, no. 3, 1999, pp. 1-4. |
| APA | [1] LI Yun-jiao, LI Hong-gui, SUN Pei-mei, SU Peng-tuan, ZHAO Zhong-wei, & LIU Mao-sheng. (1999). Commercial scale Test of Selective Precipitation for Removal of Mo,As and Sn from Tungstate Solution. Rare Metals and Cemented Carbides(3), 1-4. |
| IEEE | [1] LI Yun-jiao, LI Hong-gui, SUN Pei-mei, SU Peng-tuan, ZHAO Zhong-wei, and LIU Mao-sheng, "Commercial scale Test of Selective Precipitation for Removal of Mo,As and Sn from Tungstate Solution," Rare Metals and Cemented Carbides, no. 3, pp. 1-4, 1999. keywords: {W metallurgy;W/Mo separation;selective precipitation} |