Silicon surfaces with termination of hydrogen (H–Si), quartz, native silicon (native-Si), and chemically deposited (Au–Si)cd and sputtered gold (Au–Si)s were fabricated with roughness less than 6 Å to study the solid–liquid interface of the ionic liquid (IL) methyltrioctylammonium bis(trifluoromethylsulfonyl)imide, [N1888][TFSI], by neutron reflectometry (NR). The modifications made to the silicon surface were to obtain a native positive or negative charge similar to a charged surface in electrochemical systems. The differences in scattering length density (SLD) based on mass density and composition of IL were examined. Perpendicular to the substrate surface, a distinct transition between the first ion layer and the bulk liquid is resolved out of the reflectivity data for the gold surfaces and in particular the chemically deposited Au–Si. Other interfaces are best described by a diffuse transition between regions of different SLDs. The diffuse transitions between SLDs observed here suggest that the interfacial structure of IL, while ordered, is best described by a continuous variation in composition as opposed to distinct layers of ions.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.1c01351
Chinese Library Classification Number:
Citation Information:
Silicon surfaces with termination of hydrogen (H–Si), quartz, native silicon (native-Si), and chemically deposited (Au–Si)cd and sputtered gold (Au–Si)s were fabricated with roughness less than 6 Å to study the solid–liquid interface of the ionic liquid (IL) methyltrioctylammonium bis(trifluoromethylsulfonyl)imide, [N1888][TFSI], by neutron reflectometry (NR). The modifications made to the silicon surface were to obtain a native positive or negative charge similar to a charged surface in electrochemical systems. The differences in scattering length density (SLD) based on mass density and composition of IL were examined. Perpendicular to the substrate surface, a distinct transition between the first ion layer and the bulk liquid is resolved out of the reflectivity data for the gold surfaces and in particular the chemically deposited Au–Si. Other interfaces are best described by a diffuse transition between regions of different SLDs. The diffuse transitions between SLDs observed here suggest that the interfacial structure of IL, while ordered, is best described by a continuous variation in composition as opposed to distinct layers of ions.
quote
| GB/T 7714-2015 | [1] Jeffrey M. Klein, Hanyu Wang, Robert L. Sacci, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01351. |
| MLA | [1] Jeffrey M. Klein, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01351. |
| APA | [1] Jeffrey M. Klein, Hanyu Wang, Robert L. Sacci, James F. Browning, & Burcu Gurkan. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01351 |
| IEEE | [1] Jeffrey M. Klein, Hanyu Wang, Robert L. Sacci, James F. Browning, and Burcu Gurkan, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01351. keywords: {double layer interfacial structure quaternary ammonium scattering length density in situ cell} |