Abstract AITranslate

This paper introduce a process of preparating nanostructured WCCo composite powders-thermochemical synthesis. The process involves preparation of starting solutions, spray drying to form chemically homogeneous precursor powders and fluid bed thermochemical conversion of the precursor powders into the nanostructured WCCo composite powders. The structures,properties and applications of prepared nanostructured WCCo composite powders are descrebed.

KeyWords AITranslate

nanostructure WCCo cemented carbide thermochemical synthesis spray conversion process properties applications

1Kolaska H.-[J].国外难熔金属与硬质合金材料,1994,10(2):1-1.

1冉广,张中武,周敬恩.纳米钨合金块体材料的制备[J].中国稀土学报,2003,21(z1):52-55. 被引量:2

2范景莲,黄伯云,汪登龙,曲选辉.纳米晶难熔高比重钨合金的研究现状及应用前景[J].粉末冶金材料科学与工程,2001,6(3):205-209.

3马运柱,黄伯云,范景莲,熊翔,汪登龙.纳米级(晶)钨基合金复合粉末的制备[J].粉末冶金材料科学与工程,2004,9(3):204-211. 被引量:3

4叶途明,易健宏,彭元东,胡礼福,吕豫湘.纳米晶高密度钨合金的研究进展[J].稀有金属,2004,28(4):726-730. 被引量:11

5杨汉民,周建,胡中彪,余立新,张烈华.亚微细硬质合金三牙轮钻齿的使用与失效分析[J].武汉理工大学学报,2004,26(12):16-19.

6范景莲,汪登龙,黄伯云,赵慕岳,马运柱.难熔钨基合金的研究开发及其产业化方向[J].有色冶炼,2002,31(6):12-15. 被引量:4

7王振廷,陈华辉.纳米WC-Co硬质合金的研制及发展[J].云南冶金,2005,34(1):37-40. 被引量:10

8张兰亭.纳米硬质合金研究进展[J].四川有色金属,2005(1):29-34. 被引量:7

9陈玮.纳米WC-Co硬质合金研究现状[J].现代制造工程,2006(1):136-138. 被引量:2

10朱流,郦剑,凌国平.超细WC-Co硬质合金及其磨损性能研究[J].材料热处理学报,2006,27(3):112-115. 被引量:17

1刘婷,王巍,施静敏.Pt/WC催化剂甲醇脱氢反应机理的研究[J].当代化工,2020(9):1941-1944.

2李信,曲庆文,崔林.工艺参数对激光增材熔覆成形Co基WC复合涂层的影响[J].热加工工艺,2020,0(2):89-93. 被引量:5

3苏亚凤,陈文革,张孝林,丁秉钧.W-Cu材料的显微结构对电弧阴极斑点的影响[J].稀有金属,2005,29(4):458-460.

4吴晓东,柴永新,傅小明,傅明喜,戴起勋.蓝钨制取超细钨粉的研究[J].稀有金属,2005,29(4):570-573. 被引量:12

5朱流,郦剑.WC-10%Co激光熔覆涂层的制备及耐磨性能[J].机械工程材料,2008,32(8):26-29. 被引量:3

6YE Xiong-lin MA Shi-ning LI Chang-qing.Fabrication and analysis of nano-structured thermal spraying feeds[J].中国有色金属学会会刊:英文版,2004(z1):83-87.

7易忠来,邵刚勤,段兴龙,王冲,史晓亮,谢济仁.直接还原碳化法制备纳米复合WC-Co粉末[J].功能材料,2004(z1):2202-2203. 被引量:3

8冉广,张中武,周敬恩.纳米钨合金块体材料的制备[J].中国稀土学报,2003,21(z1):52-55. 被引量:2

9叶途明,易健宏,李丽娅,彭元东,吕豫湘,胡礼福.高密度钨合金研究的新进展[J].粉末冶金材料科学与工程,2003,8(2):134-140. 被引量:7

10林信平,曹顺华,李炯义.现代烧结技术在制备超细和纳米硬质合金中的应用[J].粉末冶金材料科学与工程,2004,9(2):126-133. 被引量:7

1罗玉长,张凡文,陈蕾,张丽玲.富Al_2O_3区域CaO行为的研究[J].有色金属:冶炼部分,1993(3):41-44. 被引量:2

2张海宝,袁方利,白柳杨,胡鹏,李晋林.球形钨粉制备与应用研究进展[J].中国钨业,2011,26(1):27-29. 被引量:7

3王晓霞,叶红齐,苏周,王锦良.超细铜粉的制备与应用[J].材料导报,2004,18(F10):140-142. 被引量:16

4赵同春,麻洪秋,金成海,张军,黄赞军.金属注射成形用水雾化不锈钢粉末的制备与应用[J].粉末冶金工业,2013,23(3):26-31. 被引量:15

5戴学刚.碳化硅粉末的制备与应用进展[J].化工冶金,1996,17(2):181-185. 被引量:4

6罗玉长,张凡文,陈蕾,张丽玲.富Al_2O_3区域CaO行为的研究[J].轻金属,1993(4):13-16.

7魏建红,官建国,袁润章.金属纳米粒子的制备与应用[J].武汉工业大学学报,2001,23(3):1-4. 被引量:22

8邱文冬,牟济宁,陈金荣,王燕群.宝钢300t钢包用国产浇注料的性能与应用[J].耐火材料,2001,35(6):331-333. 被引量:1

9冯威,李玉龙,朱晓东.钨铜复合材料的制备与应用[J].成都大学学报:自然科学版,2011,30(4):364-367. 被引量:7

10王剑,刘瑛瑛,李来时,翟玉春.超细脱硅剂的制备与应用[J].轻金属,2010(8):17-20.

Basic Information:

DOI:

Chinese Library Classification Number:TF123.74[冶金工程—粉末冶金]

Citation Information:

This paper introduce a process of preparating nanostructured WCCo composite powders-thermochemical synthesis. The process involves preparation of starting solutions, spray drying to form chemically homogeneous precursor powders and fluid bed thermochemical conversion of the precursor powders into the nanostructured WCCo composite powders. The structures,properties and applications of prepared nanostructured WCCo composite powders are descrebed.

quote

GB/T 7714-2015 [1] GAO Rong-gen. Preparation and Applications of NanostructuredWCCo composite Powders[J]. Rare Metals and Cemented Carbides, 1999(2): 49-54.
MLA [1] GAO Rong-gen. "Preparation and Applications of NanostructuredWCCo composite Powders." Rare Metals and Cemented Carbides, no. 2, 1999, pp. 49-54.
APA [1] GAO Rong-gen. (1999). Preparation and Applications of NanostructuredWCCo composite Powders. Rare Metals and Cemented Carbides(2), 49-54.
IEEE [1] GAO Rong-gen, "Preparation and Applications of NanostructuredWCCo composite Powders," Rare Metals and Cemented Carbides, no. 2, pp. 49-54, 1999. keywords: {nanostructure;WCCo cemented carbide;thermochemical synthesis;spray conversion process;properties;applications}