Preparation and Electrochemical Properties of ZnCoO4@CoWO4 Nanocomposites AITranslate

School of Materials Science and Engineering,Liaoning University of Technology;School of Materials Science and Engineering,Liaoning University of Technology;School of Materials Science and Engineering,Liaoning University of Technology;School of Materials Science and Engineering,Liaoning University of Technology;School of Materials Science and Engineering,Liaoning University of Technology;School of Materials Science and Engineering,Liaoning University of Technology;School of Materials Science and Engineering,Liaoning University of Technology;School of Materials Science and Engineering,Liaoning University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

ZnCo2O4 nanoneedle arrays were grown on nickel foam by hydrothermal synthesis method,and then CoWO4 nanosheets were deposited on the surface to prepare a core-shell ZnCo2O4@CoWO4 composite electrode material.The microstructure,phase structure,and electrochemical properties of the electrode material were characterized by SEM,XRD,and electrochemical workstation.The results show that the ZnCo2O4@CoWO4 electrode material exhibits a rod-like microstructure,with CoWO4 nanosheets tightly wrapping the surface of ZnCo2O4 nanoneedles.Meanwhile,the electrochemical properties of ZnCo2O4@CoWO4 electrode material are significantly improved on the basis of the monomer.Additionally,ZnCo2O4@CoWO4 composite electrode material has a high specific capacity and an enhanced charge-discharge cycle perfor-mance,effectively addressing the problems of poor conductivity and cycle stability caused by the volume expansion of momoner ZnCo2O4 material.

KeyWords AITranslate

electrode material ZnCoO4 CoWO4 nanocomposite hydrothermal synthesis method electro-chemical property

1王思原.基于超级电容的汽车应急启动电源设计[J].时代汽车,2021(12):113-114. 被引量:1

2高玉双,张静,刘鹏.超级电容器的技术特点与市场应用研究[J].科技风,2020,0(2):62-62. 被引量:4

3杨文耀,黄昊,朱欣月,李杰,向静.基于毛竹笋壳生物质碳材料的制备及其超级电容器性能[J].电子元件与材料,2020,39(7):66-71. 被引量:12

Basic Information:

DOI:

Chinese Library Classification Number:TB34[一般工业技术—材料科学与工程]

Citation Information:

ZnCo2O4 nanoneedle arrays were grown on nickel foam by hydrothermal synthesis method,and then CoWO4 nanosheets were deposited on the surface to prepare a core-shell ZnCo2O4@CoWO4 composite electrode material.The microstructure,phase structure,and electrochemical properties of the electrode material were characterized by SEM,XRD,and electrochemical workstation.The results show that the ZnCo2O4@CoWO4 electrode material exhibits a rod-like microstructure,with CoWO4 nanosheets tightly wrapping the surface of ZnCo2O4 nanoneedles.Meanwhile,the electrochemical properties of ZnCo2O4@CoWO4 electrode material are significantly improved on the basis of the monomer.Additionally,ZnCo2O4@CoWO4 composite electrode material has a high specific capacity and an enhanced charge-discharge cycle perfor-mance,effectively addressing the problems of poor conductivity and cycle stability caused by the volume expansion of momoner ZnCo2O4 material.

quote

GB/T 7714-2015 [1] XU Song-lin, LI Jia, ZHOU Zhong-hong, et al. Preparation and Electrochemical Properties of ZnCoO4@CoWO4 Nanocomposites[J]. Rare Metals and Cemented Carbides, 2024(2): 23-31.
MLA [1] XU Song-lin, et al., "Preparation and Electrochemical Properties of ZnCoO4@CoWO4 Nanocomposites." Rare Metals and Cemented Carbides, no. 2, 2024, pp. 23-31.
APA [1] XU Song-lin, LI Jia, ZHOU Zhong-hong, CUI Shi-tao, MA Xiao-xue, TIAN Yue, XIANG Jun, & ZHAO Rong-da. (2024). Preparation and Electrochemical Properties of ZnCoO4@CoWO4 Nanocomposites. Rare Metals and Cemented Carbides(2), 23-31.
IEEE [1] XU Song-lin, LI Jia, ZHOU Zhong-hong, CUI Shi-tao, MA Xiao-xue, TIAN Yue, XIANG Jun, and ZHAO Rong-da, "Preparation and Electrochemical Properties of ZnCoO4@CoWO4 Nanocomposites," Rare Metals and Cemented Carbides, no. 2, pp. 23-31, 2024. keywords: {electrode material;ZnCoO;CoWO;nanocomposite;hydrothermal synthesis method;electro-chemical property}