Development of Non-magnetic Cemented Carbide AITranslate
Abstract AITranslate
In this paper,the development of non-magnetic cemented carbide is reviewed. Detailed description is made of the principle, process and key techniques for the preparation of non-magnetic cemented carbide. The paper summarizes the difficulties and problems in the preparation of non-magnetic cemented carbide. Its future development is also explored.
KeyWords AITranslate
1黄宗浩.无磁合金及YN14无磁硬质合金的研制[J].硬质合金,2002,19(1):26-28. 被引量:5
2Pirso J,et al.Friction and wear behaviour of cemented carbides[J].Wear,2004,257 (3-4):257.
3Lisovsky A F.Some speculation on an increase of WC-Co cemented carbide service life under dynamic loads[J].International Journal of Refractory Metals and Hard Materials,2003,21 (1-2):63.
4Engqvist H,et al.Determination of the average grain size of cemented carbides[J].Interntional Journal of Refractory Metals and Hard Materials,2003,21 (1-2):31.
5Engqvist H,et al.A model for the hardness of cemented carbides[J].Wear,2002,252 (5-6):384.
6Andren Hans-Olof.Microstructure of cemented carbides[J].Materials and Design,2001,22(6):491.
7杨宣增,卢伟民,张立.WC-Ni系大直径无磁硬质合金模具的研制[J].稀有金属与硬质合金,2000,28(1):1-5. 被引量:4
8周文运.无磁硬质合金制备工艺[J].磁性材料及器件,1996,27(1):41-45. 被引量:3
9Roebuck B,et al.Infiltration as a method for producing WC hardmetals with Co and Ni alloy binder-phase[J].International Journal of Refractorg Metals and Hard Materials,1984,(3):35.
10Weibrook C M,et al.Thermal residual stress distribution in WC-Ni composites[J].Material Science & Engineering A:Structural Materials,1996,209(1-2):318.
1徐翔宇,郑勇,吴昊,丁青军,王丽珠,欧阳杰.无磁金属陶瓷的研究进展[J].材料导报,2020,34(9):64-68. 被引量:2
2李金普,施瑜蕾,柳学全,姜丽娟,李彪.低压烧结温度对WC-6Ni无磁硬质合金性能的影响[J].粉末冶金工业,2021,31(1):46-50. 被引量:4
1赵明娟,薛林威,赵火平,赵龙志,余梦,李劲.FeCoCrNiAl/Al_(2)O_(3)金属陶瓷坯体凝胶注模研究[J].华东交通大学学报,2021,38(3):82-88. 被引量:1
2罗成,梁小东,唐冬梅,杨文强,王金林,曹志华.WC碳量对WC-6%Ni硬质合金组织与性能影响[J].硬质合金,2022,39(3):195-201. 被引量:2
3杨宇,袁建坤,陈鹏起,郎宏彬,霍俊豪,程继贵.微晶蜡基粘结剂应用于YG10硬质合金注射成形的研究[J].粉末冶金工业,2022,32(6):10-15. 被引量:1
4郑东海,唐愈.高熵合金CoCrFeNiTiAl粘结WC硬质合金的制备与研究[J].粉末冶金工业,2022,32(6):16-20.
5李晓峰,赵宇霞,郭子傲,刘斌,白培康,刘彬.基于增材制造的硬质合金粉末研究现状[J].粉末冶金工业,2023,33(1):1-9.
6张振,苏武丽,孙兰.超声冷冻干燥混粉工艺对WC-6Co-GO/Al_(2)O_(3)硬质合金组织及性能的影响[J].粉末冶金材料科学与工程,2023,28(4):338-346.
1王志峰,赵维民,许甫宁,王志国,贾俊青.多孔金属材料的制备方法及研究进展[J].中国铸造装备与技术,2011,46(1):1-7. 被引量:7
2李雷鸣,徐锦锋.大体积非晶合金的制备技术[J].铸造技术,2007,28(10):1332-1337. 被引量:5
3陆伟,严彪,殷俊林,尤富强,张文彪.大块非晶合金的制备、性能与应用研究进展[J].上海钢研,2004(3):47-54. 被引量:2
4方名尧.无磁硬质合金模具的开发与生产[J].江西冶金,1993,13(2):43-45. 被引量:5
5周文运.无磁硬质合金制备工艺[J].磁性材料及器件,1996,27(1):41-45. 被引量:3
6罗在清.WC15Ni磁合金的质量控制[J].硬质合金,2005,22(2):93-95. 被引量:3
7王维军,马中伟,王伟.无磁钢制模具的热处理[J].机械工人:热加工,2003,27(8):52-54. 被引量:1
8刘文彬,王铁军,陈飞雄,陈福鸽,谢琰军.WC-15Ni高性能无磁硬质合金的制备与性能研究[J].稀有金属与硬质合金,2016,44(5):74-78. 被引量:4
9黄宗浩.无磁合金及YN14无磁硬质合金的研制[J].硬质合金,2002,19(1):26-28. 被引量:5
10孙景,刘俊朋,郭小南,梁福起,赵光远,范明德.含VC的WC-10%Ni硬质合金无磁机理研究[J].硬质合金,2003,20(2):72-75. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
In this paper,the development of non-magnetic cemented carbide is reviewed. Detailed description is made of the principle, process and key techniques for the preparation of non-magnetic cemented carbide. The paper summarizes the difficulties and problems in the preparation of non-magnetic cemented carbide. Its future development is also explored.
quote
| GB/T 7714-2015 | [1] GAO Hai-yan. Development of Non-magnetic Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2006(3): 51-54. |
| MLA | [1] GAO Hai-yan. "Development of Non-magnetic Cemented Carbide." Rare Metals and Cemented Carbides, no. 3, 2006, pp. 51-54. |
| APA | [1] GAO Hai-yan. (2006). Development of Non-magnetic Cemented Carbide. Rare Metals and Cemented Carbides(3), 51-54. |
| IEEE | [1] GAO Hai-yan, "Development of Non-magnetic Cemented Carbide," Rare Metals and Cemented Carbides, no. 3, pp. 51-54, 2006. keywords: {non-magnetic cemented carbide;preparation principle;preparation process;latest development} |