Reversible Phase Transitions of all Inorganic Copper-Based Perovskites: Water-Triggered Fluorochromism for Advanced Anticounterfeiting Applications AITranslate

Jiangsu Second Normal University; Jiangsu Second Normal University; Jiangsu Second Normal University; Tianjin University of Technology; Jiangsu Second Normal University; Jiangsu Second Normal University; Jiangsu Second Normal University; Tianjin University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Recently, several lead halide perovskites have been demonstrated as functional materials with hydrochromic, thermochromic, and photochromic properties for anticounterfeiting applications. However, their lead toxicity and relatively poor stability are still drawbacks for large-scale practical applications. In this work, we report the reversible water-triggered fluorochromism of the copper-based perovskites, which utilize the crystalline phase transition between Cs3Cu2I5 and CsCu2I3. The custom-designed images printed using the Cs3Cu2I5 ink are invisible under daylight but emit intense blue fluorescence under UV light. This fluorescence undergoes a blue-to-orange color change upon exposure to water, which can be recovered upon removing water. Furthermore, the fluorochromism of Cs3Cu2I5 is tunable to blue, blue-green, and cyan via anion-exchange reactions in various halide salt solutions. These multicolor- and multistimuli-responsive benefits make Cs3Cu2I5 a promising chromic material for high-level information security applications.

KeyWords AITranslate

allinorganic perovskite copperbased perovskite phase transition chromism anticounterfeiting ball milling
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c00967

Chinese Library Classification Number:

Citation Information:

Recently, several lead halide perovskites have been demonstrated as functional materials with hydrochromic, thermochromic, and photochromic properties for anticounterfeiting applications. However, their lead toxicity and relatively poor stability are still drawbacks for large-scale practical applications. In this work, we report the reversible water-triggered fluorochromism of the copper-based perovskites, which utilize the crystalline phase transition between Cs3Cu2I5 and CsCu2I3. The custom-designed images printed using the Cs3Cu2I5 ink are invisible under daylight but emit intense blue fluorescence under UV light. This fluorescence undergoes a blue-to-orange color change upon exposure to water, which can be recovered upon removing water. Furthermore, the fluorochromism of Cs3Cu2I5 is tunable to blue, blue-green, and cyan via anion-exchange reactions in various halide salt solutions. These multicolor- and multistimuli-responsive benefits make Cs3Cu2I5 a promising chromic material for high-level information security applications.

quote

GB/T 7714-2015 [1] Jilin Feng, Jiaxin Wang, Di Wang, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c00967.
MLA [1] Jilin Feng, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c00967.
APA [1] Jilin Feng, Jiaxin Wang, Di Wang, Meina Han, Guangsheng Qian, Fan Wu, Qian Lin, & Zhanggui Hu. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c00967
IEEE [1] Jilin Feng, Jiaxin Wang, Di Wang, Meina Han, Guangsheng Qian, Fan Wu, Qian Lin, and Zhanggui Hu, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c00967. keywords: {allinorganic perovskite copperbased perovskite phase transition chromism anticounterfeiting ball milling}