daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

A hair-trigger self-powered electrochromic window and a rechargeable battery ignoring charging process AITranslate

Soochow University; Soochow University; Soochow University; Soochow University; Soochow University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Self-powered electrochromic windows (ECWs) have become an appealing research hotspot for their multifunctionality and energy efficiency without external voltage supplies. Many previous researches that utilized active metals, solar cells and nanogenerators to realize self-powered ECWs were baroque or inefficient. In this work, we propose a tri-layered electrochromic (EC) window comprising multifunctional hydrogel, EC material and current collector to realize controllable self-coloration and self-bleaching processes of the ECW by introducing a magnesium (Mg) anode and an ammonium persulfate (AP) cathode, which also serve as secondary batteries ignoring charging processes via reverse electrons migration between Mg/EC and AP/EC circuits. This unique architecture yields remarkable electrochemical performances, including rapid self-coloration time (0.5 s) and self-bleaching time (1.9 s), a high optical contrast (∼51%), long cycling durability (99.12% optical contrast remains after ∼1500 cycles when driven by electricity supply), and lighting a 1.8 V red LED up for 2 h. In addition, we also established a 10 × 10 cm2 prototype device as the suitability demonstration for large-area ECWs. This newly proposed configuration offers opportunity for multifunctional self-powered ECWs, and will possibly accelerate the development of environment-friendly and energy-saving appliances. Graphical abstract We propose and realize a tri-layered electrochromic windows comprising multifunctional hydrogel, electrochromic material and current collector with completely controllable self-coloration and self-bleaching processes by introducing a magnesium (Mg) sheet and an ammonium persulfate (AP) foil, in which the self-coloration and self-bleaching processes can also serve as a reusable battery without the charging section. Download : Download high-res image (224KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2022.101543

Chinese Library Classification Number:

Citation Information:

Self-powered electrochromic windows (ECWs) have become an appealing research hotspot for their multifunctionality and energy efficiency without external voltage supplies. Many previous researches that utilized active metals, solar cells and nanogenerators to realize self-powered ECWs were baroque or inefficient. In this work, we propose a tri-layered electrochromic (EC) window comprising multifunctional hydrogel, EC material and current collector to realize controllable self-coloration and self-bleaching processes of the ECW by introducing a magnesium (Mg) anode and an ammonium persulfate (AP) cathode, which also serve as secondary batteries ignoring charging processes via reverse electrons migration between Mg/EC and AP/EC circuits. This unique architecture yields remarkable electrochemical performances, including rapid self-coloration time (0.5 s) and self-bleaching time (1.9 s), a high optical contrast (∼51%), long cycling durability (99.12% optical contrast remains after ∼1500 cycles when driven by electricity supply), and lighting a 1.8 V red LED up for 2 h. In addition, we also established a 10 × 10 cm2 prototype device as the suitability demonstration for large-area ECWs. This newly proposed configuration offers opportunity for multifunctional self-powered ECWs, and will possibly accelerate the development of environment-friendly and energy-saving appliances. Graphical abstract We propose and realize a tri-layered electrochromic windows comprising multifunctional hydrogel, electrochromic material and current collector with completely controllable self-coloration and self-bleaching processes by introducing a magnesium (Mg) sheet and an ammonium persulfate (AP) foil, in which the self-coloration and self-bleaching processes can also serve as a reusable battery without the charging section. Download : Download high-res image (224KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Shiqing Zhao, Xu Gao, Linsen Chen, et al. Applied Materials Today, 2022(28). DOI:10.1016/j.apmt.2022.101543.
MLA [1] Shiqing Zhao, et al., Applied Materials Today, no. 28, 2022, https://doi.org/10.1016/j.apmt.2022.101543.
APA [1] Shiqing Zhao, Xu Gao, Linsen Chen, Wenbin Huang, & Yanhua Liu. (2022). Applied Materials Today(28). https://doi.org/10.1016/j.apmt.2022.101543
IEEE [1] Shiqing Zhao, Xu Gao, Linsen Chen, Wenbin Huang, and Yanhua Liu, Applied Materials Today, no. 28, 2022, doi: 10.1016/j.apmt.2022.101543.