daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Probing Band-Alignment at the Interface of 3D/2D Perovskites for Solar Cell Applications Probing Band-Alignment at the Interface of 3D/2D Perovskites for Solar Cell Applications AITranslate

School of Physical Sciences, Indian Association for the Cultivation of Science;School of Physical Sciences, Indian Association for the Cultivation of Science; University Campus
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this report, the effect of interfacial band-alignment in 3D/2D perovskite heterostructures on the performance of solar cells has been studied. The heterostructures have emerged as a preferred approach to slow down the degradation of 3D perovskites. We have incorporated three different organic spacers, namely butylammonium (BA+), phenethylammonium (PEA+), and ethanolamine (EA+), in forming the 2D perovskite layer over the top of a 3D triple-cation halide perovskite. The power conversion efficiency has been found to depend on the 2D perovskite. The band-energies of the 3D and the 2D perovskites, derived from scanning tunneling spectroscopy and Kelvin probe force microscopy, have showed that the EA+-based capping layer forms a type-II band-alignment at the 3D/2D interface and thereby facilitates charge separation. Our work depicts the necessity of probing the interfacial band-alignment while fabricating solar cells based on 3D/2D perovskites.

KeyWords AITranslate

Perovskite solar cells 3D/2D heterostructures interfacial band alignment energy band diagram scanning tunneling spectroscopy
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00358

Chinese Library Classification Number:

Citation Information:

In this report, the effect of interfacial band-alignment in 3D/2D perovskite heterostructures on the performance of solar cells has been studied. The heterostructures have emerged as a preferred approach to slow down the degradation of 3D perovskites. We have incorporated three different organic spacers, namely butylammonium (BA+), phenethylammonium (PEA+), and ethanolamine (EA+), in forming the 2D perovskite layer over the top of a 3D triple-cation halide perovskite. The power conversion efficiency has been found to depend on the 2D perovskite. The band-energies of the 3D and the 2D perovskites, derived from scanning tunneling spectroscopy and Kelvin probe force microscopy, have showed that the EA+-based capping layer forms a type-II band-alignment at the 3D/2D interface and thereby facilitates charge separation. Our work depicts the necessity of probing the interfacial band-alignment while fabricating solar cells based on 3D/2D perovskites.

quote

GB/T 7714-2015 [1] Raja Chakraborty, Goutam Paul, Amlan J. Pal. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00358.
MLA [1] Raja Chakraborty, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00358.
APA [1] Raja Chakraborty, Goutam Paul, & Amlan J. Pal. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00358
IEEE [1] Raja Chakraborty, Goutam Paul, and Amlan J. Pal, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00358. keywords: {Perovskite solar cells 3D/2D heterostructures interfacial band alignment energy band diagram scanning tunneling spectroscopy}