Wetting Phenomena in Nanofluidics AITranslate

max-planck-institut für metallforschung, 70569 stuttgart;max-planck-institut für metallforschung, 70569 stuttgart
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We focus on the dynamical aspects of wetting phenomena on the nanoscale for which bulk hydrodynamic equations become invalid. At the nanoscale, phenomena that are irrelevant on the micrometer scale and larger, or that can be summarily incorporated in terms of boundary conditions, become important. Among these features are long-ranged molecular interactions such as dispersion forces, thermal fluctuations, hydrodynamic slip, segregation of mixtures and solutions at walls, and electrical double layers.

KeyWords AITranslate

dewetting nanochannels hydrodynamic slip thermal fluctuations
No data

Basic Information:

DOI:https://doi.org/10.1146/annurev.matsci.38.060407.132451

Chinese Library Classification Number:

Citation Information:

We focus on the dynamical aspects of wetting phenomena on the nanoscale for which bulk hydrodynamic equations become invalid. At the nanoscale, phenomena that are irrelevant on the micrometer scale and larger, or that can be summarily incorporated in terms of boundary conditions, become important. Among these features are long-ranged molecular interactions such as dispersion forces, thermal fluctuations, hydrodynamic slip, segregation of mixtures and solutions at walls, and electrical double layers.

quote

GB/T 7714-2015 [1] M. Rauscher, S. Dietrich. Annual Review of Materials Research, 2008(38). DOI:10.1146/annurev.matsci.38.060407.132451.
MLA [1] M. Rauscher, and S. Dietrich. Annual Review of Materials Research, no. 38, 2008, https://doi.org/10.1146/annurev.matsci.38.060407.132451.
APA [1] M. Rauscher, & S. Dietrich. (2008). Annual Review of Materials Research(38). https://doi.org/10.1146/annurev.matsci.38.060407.132451
IEEE [1] M. Rauscher and S. Dietrich, Annual Review of Materials Research, no. 38, 2008, doi: 10.1146/annurev.matsci.38.060407.132451. keywords: {dewetting;nanochannels;hydrodynamic slip;thermal fluctuations}