Toward 4D Printing of Shape Memory Polymers Based on Polyaryletherketone/NVP/PEGDA through Molecular Engineering and Direct Ink Writing 3D Printing AITranslate

Lanzhou University of Technology; University of Chinese Academy of Sciences; University of Chinese Academy of Sciences; University of Chinese Academy of Sciences; University of Chinese Academy of Sciences; University of Chinese Academy of Sciences; University of Chinese Academy of Sciences; Lanzhou University of Technology; University of Chinese Academy of Sciences; University of Chinese Academy of Sciences
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Polyaryletherketone (PAEK), an engineering plastic with exceptional mechanical properties and a high glass transition temperature, can be tailored with various properties to meet the multiple requirements of aerospace applications. However, it remains a challenge to 3D print PAEK with good properties. Herein, a direct ink writing (DIW) 3D printable PAEK ink has been developed, and the yielded PAEK parts possess high tensile strength and excellent shape memory properties. The incorporation of N-vinyl-2-pyrrolidone (NVP) and polyethylene glycol diacrylate PEGDA into PAEK oligomers (PAEKOs) facilitated their versatility as diluents or reactive functional monomers. This characteristic enabled random cross-linking through photoinitiator exposure for the formation of block copolymers, establishing the essential stationary and reversible phases needed for shape memory capabilities. The photocured PAEK demonstrated excellent comprehension performances, including an outstanding tensile strength (42.6 MPa), thermal stability (Td-246 °C), shape fixation ratio (>93%), and shape recovery ratio (>100%). Furthermore, PAEK with a greater shape memory effect was utilized as an actuator to realize gripping and releasing at high temperatures (140 °C). This study therefore provides an emerging strategy to fabricate shape memory components for challenging environments using DIW technology. This approach also holds promise for implementation in systems beyond PAEK which have typically been difficult to print.

KeyWords AITranslate

shape memory polymer polyaryletherketone photocuring 4D printing solventfree
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01020

Chinese Library Classification Number:

Citation Information:

Polyaryletherketone (PAEK), an engineering plastic with exceptional mechanical properties and a high glass transition temperature, can be tailored with various properties to meet the multiple requirements of aerospace applications. However, it remains a challenge to 3D print PAEK with good properties. Herein, a direct ink writing (DIW) 3D printable PAEK ink has been developed, and the yielded PAEK parts possess high tensile strength and excellent shape memory properties. The incorporation of N-vinyl-2-pyrrolidone (NVP) and polyethylene glycol diacrylate PEGDA into PAEK oligomers (PAEKOs) facilitated their versatility as diluents or reactive functional monomers. This characteristic enabled random cross-linking through photoinitiator exposure for the formation of block copolymers, establishing the essential stationary and reversible phases needed for shape memory capabilities. The photocured PAEK demonstrated excellent comprehension performances, including an outstanding tensile strength (42.6 MPa), thermal stability (Td-246 °C), shape fixation ratio (>93%), and shape recovery ratio (>100%). Furthermore, PAEK with a greater shape memory effect was utilized as an actuator to realize gripping and releasing at high temperatures (140 °C). This study therefore provides an emerging strategy to fabricate shape memory components for challenging environments using DIW technology. This approach also holds promise for implementation in systems beyond PAEK which have typically been difficult to print.

quote

GB/T 7714-2015 [1] Ketian Gao, Junhui Gong, Pengrui Cao, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01020.
MLA [1] Ketian Gao, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01020.
APA [1] Ketian Gao, Junhui Gong, Pengrui Cao, Zhangzhang Tang, Tingmei Wang, Liming Tao, Xinrui Zhang, Jianqiang Zhang, Qihua Wang, & Yaoming Zhang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01020
IEEE [1] Ketian Gao, Junhui Gong, Pengrui Cao, Zhangzhang Tang, Tingmei Wang, Liming Tao, Xinrui Zhang, Jianqiang Zhang, Qihua Wang, and Yaoming Zhang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01020. keywords: {shape memory polymer;polyaryletherketone;photocuring;4D printing;solventfree}