Experimental Study on Na_2MoO_4 Solution Purification by Precipitation-Coprecipitation AITranslate
Abstract AITranslate
In view of the problems existing in the conventional precipitation with MgCl2 for Si and P removal and based on the composition characteristics,Na2MoO4 solution was purified deep by precipitation-coprecipitation.Compared with conventional magnesium or aluminum salt precipitation,precipitation-coprecipitation can bring about better purifying effect and more simple process control,overcoming the shortcomings in the conventional precipitation process,e.g.severe Mo inclusion loss.
KeyWords AITranslate
1赵小翠,马成兵,吴敏,闫志勇.钼资源的回收与应用前景[J].中国钼业,2007,31(3):38-40. 被引量:10
2Templeton,Charles C.Dissolving siliceous material with self-acidifying liquid[P].US Pat:3828854,1974-08-13.
3王少娜,郑诗礼,张懿.铬盐清洁生产工艺中铝硅的脱除[J].中国有色金属学报,2007,17(7):1188-1194. 被引量:16
4Luo T L,Miyazaki,Shibayama A,et al.A novel process for recovery of tungsten and vanadium from a leach solution of tungsten alloy scrap[J].Minerals Engineering,2003,16:665-670.
5Matjie R H,Engelbrecht R.Selective removal of dissolved silicon and aluminium ions from gas liquor by hydrometallurgical methods[J].Hydrometallurgy,2007,85:172-182.
6Dinesh Mohan,Charles U,Pittman Jr.Arsenic removal from waste water using adsorbents a critical review[J]Journal of Hazardous Materials,2007,142:1-53.
7Guan Xiaohong,Dong Haoran,Ma Jun,et al.Removal of arsenic from water effects of competing anions on As(Ⅲ)removal in KMnO4Fe(Ⅱ)process[J].Water Research,2009,43(15):1-9.
8莫鼎成,唐志红,关影莲,夏毅萍.高硅硫酸锌溶液脱硅的方法[J].中国有色金属学报,1994,4(4):38-40. 被引量:1
9Glen F Van Landeghem,Marc E De Broe,Patrick C D'Haese.Al and Si:their speciation,distribution,and toxicity[J].Clinical Biochemistry,1998,31(5):385-397.
10Zhang Jinsuo,Klasky Marc,Bruce C Letellier.The aluminum chemistry and corrosion in alkaline solutions[J].Journal of Nuclear Materials,2009,384:175-189.
1朱珠,沈恒冠,林丽美,陈姝.共沉淀法沉淀废水中微量钴以及测试方法的研究和应用[J].中国化工贸易,2013,5(6):313-313.
2曾辉,彭万通.用中和水解法从粗钴盐溶液中除硅[J].湿法冶金,2016,35(3):235-238. 被引量:2
1叶雪梅,田森,董亚萍,冯海涛,刘鑫,李波,李武,张波.铬酸中和法去除铬酸钠电解液中硅的实验研究[J].盐湖研究,2020,28(2):101-108.
2马超,黄隆.SEDIPACT高密池工艺应用于反渗透浓水除硅[J].辽宁化工,2022,51(11):1573-1576.
1吴免利,伊继光,赵虎,谢添,杨芬,张贵清.碱性离子交换制取钼酸铵溶液研究[J].中国有色冶金,2010,39(6):71-74. 被引量:3
2丁扬力,肖连生,曹佐英,张贵清,曾理.N263从钼酸钠溶液中萃取分离钼钒[J].有色金属科学与工程,2017,8(1):15-20. 被引量:6
3吕莹,孙放.Fe(OH)_3吸附法从高钨钼酸钠溶液中分离钨钼的研究[J].稀有金属与硬质合金,2005,33(3):1-3. 被引量:19
4陈星宇,肖露萍,赵中伟.钨钼冶炼过程中除钒[J].中国有色金属学报,2014,24(7):1883-1887. 被引量:5
5张刚,赵中伟,霍广生,曹才放,李江涛,陈爱良,李洪桂.镍钼矿处理工艺的研究现状[J].稀有金属与硬质合金,2008,36(4):37-41. 被引量:31
6潘志胜,王谦,何生平,李玉刚.连铸保护渣组分对粘度的影响[J].四川冶金,2010,32(5):17-21. 被引量:3
7赵由才,于淑秋,陈家镛.伯胺-磷酸三丁酯协同萃取分离钼酸钠溶液中磷的机理研究[J].有色金属,1992(3):59-62. 被引量:1
8赵剑波,王成彦,尹飞,陈永强,阮书锋.含锌、铜溶液萃取分离及锌的回收研究[J].矿冶,2014,23(5):35-38. 被引量:9
9皮关华,孔凡祥,贾露萍,王长江,杜建新.瑞木红土镍矿高压酸浸的生产实践[J].中国有色冶金,2015,0(6):11-14. 被引量:7
10万林生,龚丹丹,付赞辉,李红超,孙丽.仲钨酸铵结晶母液深度脱除氨氮的研究[J].稀有金属与硬质合金,2011,39(4):4-7. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF803.25[冶金工程—有色金属冶金]
Citation Information:
In view of the problems existing in the conventional precipitation with MgCl2 for Si and P removal and based on the composition characteristics,Na2MoO4 solution was purified deep by precipitation-coprecipitation.Compared with conventional magnesium or aluminum salt precipitation,precipitation-coprecipitation can bring about better purifying effect and more simple process control,overcoming the shortcomings in the conventional precipitation process,e.g.severe Mo inclusion loss.
quote
| GB/T 7714-2015 | [1] XIAO Chao, XIAO Lian-sheng. Experimental Study on Na_2MoO_4 Solution Purification by Precipitation-Coprecipitation[J]. Rare Metals and Cemented Carbides, 2010(4): 10-12. |
| MLA | [1] XIAO Chao, and XIAO Lian-sheng. "Experimental Study on Na_2MoO_4 Solution Purification by Precipitation-Coprecipitation." Rare Metals and Cemented Carbides, no. 4, 2010, pp. 10-12. |
| APA | [1] XIAO Chao, & XIAO Lian-sheng. (2010). Experimental Study on Na_2MoO_4 Solution Purification by Precipitation-Coprecipitation. Rare Metals and Cemented Carbides(4), 10-12. |
| IEEE | [1] XIAO Chao and XIAO Lian-sheng, "Experimental Study on Na_2MoO_4 Solution Purification by Precipitation-Coprecipitation," Rare Metals and Cemented Carbides, no. 4, pp. 10-12, 2010. keywords: {precipitation-coprecipitation;Na2MoO4 solution;purification;silicon removal} |