Study on Preparation of Be-Ti Alloys and their Microstructure and Properties AITranslate

Science and Technology on Surface Physics and Chemistry Laboratory;Science and Technology on Surface Physics and Chemistry Laboratory;Science and Technology on Surface Physics and Chemistry Laboratory;Science and Technology on Surface Physics and Chemistry Laboratory
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Be-16%Ti,Be-24%Ti and Be-30.8%Ti alloys were prepared by arc melting and suction casting.The phase composition,microstructure and microhardness of the alloys were analyzed.The results show that Be-16%Ti and Be-24%Ti alloys are composed of Be phase and Be12Ti phase,and Be-30.8%Ti alloy contains Be12Ti phase in addition to Be phase and Be12Ti phase.With the increase of solidification rate du-ring suction casting,the grain size of Be-30.8%Ti alloy casting gradually decreases.The primary dendrite spacing ofφ8 mm Be-30.8%Ti alloy casting is up to 40μm,while the primary dendrite spacing ofφ4 mm casting is about 10μm.With the increase of Ti content,the hardness of Be-Ti alloys obviously increases,and the microhardness of Be-30.8%Ti alloy can reach 950 HV.

KeyWords AITranslate

Be-Ti alloy arc melting suction casting microstructure hardness

1丛伟.模数法在铸钢件冒口设计中的应用[J].沈阳航空工业学院学报,2002,19(4):17-19. 被引量:7

1张福荣,韩明,王善瑞,鲁昌凯.Ti合金中亚稳过渡相与基体之间的位向关系[J].河北工业大学学报,2022,51(2):40-46.

2郭学益,董朝望,夏阳,刘沛东,刘汉宁,田庆华.氧化物直接还原制备低氧Ti-48Al-2Cr-2Nb合金粉末[J].中国有色金属学报:英文版,2022,32(4):1351-1361. 被引量:2

3岳帅帅,叶子天,郭扬帆,唐云宇,张小丽.定向凝固过程中单晶合金枝晶生长的研究进展[J].材料研究与应用,2022,16(2):328-336. 被引量:1

4王建武,王宁,杨树峰.基于数值模拟的镍基高温合金电渣重熔工艺优化[J].中国冶金,2022,32(3):80-86. 被引量:3

5孙志标,宋帮鹍,耿耀,崇洋.CU5MCuC镍基合金止回阀体铸造工艺的探讨[J].铸造工程,2022,46(3):1-5.

6吴元浩,李玥,金雪花,徐婧婷,郭顺堂.高浓度煮浆对豆腐品质提升的作用及其机制[J].食品科学,2022,43(7):61-66. 被引量:4

7赵刘强,邓安强,杨洋,康晓燕,罗永春.La-Nd-Y-Ni系A_(5)B_(19)型退火合金的相结构及储氢与电化学性能研究[J].中国稀土学报,2022,40(2):250-260. 被引量:3

8艾诚,王国鑫,郭敏,孙志平,张凤英,刘林.沉淀强化钴基单晶高温合金凝固行为的研究进展[J].中国有色金属学报,2022,32(3):645-657. 被引量:1

9孙宝德,王俊,康茂东,汪东红,董安平,王飞,高海燕,王国祥,杜大帆.高温合金超限构件精密铸造技术及发展趋势[J].金属学报,2022,58(4):412-427. 被引量:8

Basic Information:

DOI:

Chinese Library Classification Number:TG146.24[金属学及工艺—金属材料]

Citation Information:

Be-16%Ti,Be-24%Ti and Be-30.8%Ti alloys were prepared by arc melting and suction casting.The phase composition,microstructure and microhardness of the alloys were analyzed.The results show that Be-16%Ti and Be-24%Ti alloys are composed of Be phase and Be12Ti phase,and Be-30.8%Ti alloy contains Be12Ti phase in addition to Be phase and Be12Ti phase.With the increase of solidification rate du-ring suction casting,the grain size of Be-30.8%Ti alloy casting gradually decreases.The primary dendrite spacing ofφ8 mm Be-30.8%Ti alloy casting is up to 40μm,while the primary dendrite spacing ofφ4 mm casting is about 10μm.With the increase of Ti content,the hardness of Be-Ti alloys obviously increases,and the microhardness of Be-30.8%Ti alloy can reach 950 HV.

quote

GB/T 7714-2015 [1] PENG Shi-xian, WANG Jing, ZHAO Fu-ze, et al. Study on Preparation of Be-Ti Alloys and their Microstructure and Properties[J]. Rare Metals and Cemented Carbides, 2022(2): 70-74.
MLA [1] PENG Shi-xian, et al., "Study on Preparation of Be-Ti Alloys and their Microstructure and Properties." Rare Metals and Cemented Carbides, no. 2, 2022, pp. 70-74.
APA [1] PENG Shi-xian, WANG Jing, ZHAO Fu-ze, & ZHANG Xin-jian. (2022). Study on Preparation of Be-Ti Alloys and their Microstructure and Properties. Rare Metals and Cemented Carbides(2), 70-74.
IEEE [1] PENG Shi-xian, WANG Jing, ZHAO Fu-ze, and ZHANG Xin-jian, "Study on Preparation of Be-Ti Alloys and their Microstructure and Properties," Rare Metals and Cemented Carbides, no. 2, pp. 70-74, 2022. keywords: {Be-Ti alloy;arc melting;suction casting;microstructure;hardness}