Defect Engineered Dendritic Fibrous Nanosilica as Prospective Alloy Anode for the Fabrication of High-Energy Li-Ion Capacitors with Ultralong Durability AITranslate
Abstract AITranslate
Lithium-ion capacitors (LICs) are the next-generation electrochemical energy storage devices with two different types of energy storage mechanisms, anode and cathode. The LICs are anticipated to bridge the gap between lithium-ion batteries and supercapacitors by providing higher energy and power density than the individual charge storage systems. Our work reports the synthesis of defect-engineered dendritic fibrous nanosilica (SiOx) as an anode and commercial activated carbon (AC) as a cathode for the LICs. The Li/SiOx is prelithiated (LixSi + Li2O) prior to the fabrication of the LIC for a few cycles and is then paired with the mass-balanced AC electrode to get AC/(LixSi + Li2O)-based LIC assembly. Our LIC displays an excellent electrochemical performance with a maximum energy density of 169.7 Wh kg–1 at room temperature with ultralong durability of >48 000 cycles. The possibility of exploring LIC at different climatic conditions is also analyzed at various temperatures from −5 to 50 °C.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.2c01224
Chinese Library Classification Number:
Citation Information:
Lithium-ion capacitors (LICs) are the next-generation electrochemical energy storage devices with two different types of energy storage mechanisms, anode and cathode. The LICs are anticipated to bridge the gap between lithium-ion batteries and supercapacitors by providing higher energy and power density than the individual charge storage systems. Our work reports the synthesis of defect-engineered dendritic fibrous nanosilica (SiOx) as an anode and commercial activated carbon (AC) as a cathode for the LICs. The Li/SiOx is prelithiated (LixSi + Li2O) prior to the fabrication of the LIC for a few cycles and is then paired with the mass-balanced AC electrode to get AC/(LixSi + Li2O)-based LIC assembly. Our LIC displays an excellent electrochemical performance with a maximum energy density of 169.7 Wh kg–1 at room temperature with ultralong durability of >48 000 cycles. The possibility of exploring LIC at different climatic conditions is also analyzed at various temperatures from −5 to 50 °C.
quote
| GB/T 7714-2015 | [1] Manohar Akshay, Rajesh Belgamwar, Selvarasu Praneetha, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c01224. |
| MLA | [1] Manohar Akshay, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c01224. |
| APA | [1] Manohar Akshay, Rajesh Belgamwar, Selvarasu Praneetha, Vivek Polshettiwar, & Vanchiappan Aravindan. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c01224 |
| IEEE | [1] Manohar Akshay, Rajesh Belgamwar, Selvarasu Praneetha, Vivek Polshettiwar, and Vanchiappan Aravindan, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c01224. |