High-Photoresponsivity Transistors Based on Small-Molecule Organic Semiconductors High-Photoresponsivity Transistors Based on Small-Molecule Organic Semiconductors AITranslate
Abstract AITranslate
We investigate the viability of 2,8-difluoro-5,11-bis(triethylsilylethynyl)anthradithiophene (diF-TES ADT) as a photosensor and show that there is a direct correlation between the absorption spectrum of the material and the magnitude of the resulting drain current in a field-effect transistor device made from it. We show that the diF-TES ADT device exhibits very high photosensitivity and photoresponsivity for green and blue light. We also propose a hybrid device structure that leverages the high absorptivities of two organic semiconductors to make a sandwich device with high phototransistor metrics across all wavelengths of visible light.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c00970
Chinese Library Classification Number:
Citation Information:
We investigate the viability of 2,8-difluoro-5,11-bis(triethylsilylethynyl)anthradithiophene (diF-TES ADT) as a photosensor and show that there is a direct correlation between the absorption spectrum of the material and the magnitude of the resulting drain current in a field-effect transistor device made from it. We show that the diF-TES ADT device exhibits very high photosensitivity and photoresponsivity for green and blue light. We also propose a hybrid device structure that leverages the high absorptivities of two organic semiconductors to make a sandwich device with high phototransistor metrics across all wavelengths of visible light.
quote
| GB/T 7714-2015 | [1] Zafrullah Jagoo, Zachary A. Lamport, Oana D. Jurchescu, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00970. |
| MLA | [1] Zafrullah Jagoo, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00970. |
| APA | [1] Zafrullah Jagoo, Zachary A. Lamport, Oana D. Jurchescu, & Laurie E. McNeil. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00970 |
| IEEE | [1] Zafrullah Jagoo, Zachary A. Lamport, Oana D. Jurchescu, and Laurie E. McNeil, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00970. keywords: {diFTES ADT photocurrent photosensitivity photoresponsivity photovoltaic effects photoconductive effects} |