daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Shape Memory Polymer Constructed by π–π Stacking with Ultrafast Photoresponse and Self-Healing Performance AITranslate

Shaanxi University of Science and Technology; Northwestern Polytechnical University; Northwestern Polytechnical University; Northwestern Polytechnical University; Northwestern Polytechnical University;Xi’an Modern Chemsitry Research Institute; Shaanxi University of Science and Technology; Northwestern Polytechnical University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Recently, polymer materials with light-responsive shape memory and self-healing ability have been extensively studied. Various strategies have been reported to prepare remotely controllable light-responsive shape memory materials by employing carbon-based nanophotothermal agents (e.g., carbon nanotubes (CNTs)) in a shape memory polymer network. However, enhancing the dispersion state and capacity of CNTs remains a challenge for improving the response capability and rate of light-responsive shape memory materials. In this work, poly(vinyl alcohol) (PVA) modified with a pyrene groups was introduced as the polymer network, and CNTs were introduced as the nanophotothermal agent to prepare a light-responsive shape memory material with fast photothermal responsiveness. Because of the stacking interaction between pyrene and CNTs, a large fraction of CNTs are dispersed in an orderly way in the polymer matrix. Moreover, stacking and hydrogen bond interactions build up stable cross-links and endow the material with shape memory and self-healing ability. Therefore, this work provides an innovative strategy for preparing a shape memory material with an ultrafast photoresponse and self-healing performance.

KeyWords AITranslate

shape memory photoresponse pyrene π−π stacking nearinfrared
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c02192

Chinese Library Classification Number:

Citation Information:

Recently, polymer materials with light-responsive shape memory and self-healing ability have been extensively studied. Various strategies have been reported to prepare remotely controllable light-responsive shape memory materials by employing carbon-based nanophotothermal agents (e.g., carbon nanotubes (CNTs)) in a shape memory polymer network. However, enhancing the dispersion state and capacity of CNTs remains a challenge for improving the response capability and rate of light-responsive shape memory materials. In this work, poly(vinyl alcohol) (PVA) modified with a pyrene groups was introduced as the polymer network, and CNTs were introduced as the nanophotothermal agent to prepare a light-responsive shape memory material with fast photothermal responsiveness. Because of the stacking interaction between pyrene and CNTs, a large fraction of CNTs are dispersed in an orderly way in the polymer matrix. Moreover, stacking and hydrogen bond interactions build up stable cross-links and endow the material with shape memory and self-healing ability. Therefore, this work provides an innovative strategy for preparing a shape memory material with an ultrafast photoresponse and self-healing performance.

quote

GB/T 7714-2015 [1] Jiaye Dai, Zichao Wang, Zhenzhen Wu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c02192.
MLA [1] Jiaye Dai, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c02192.
APA [1] Jiaye Dai, Zichao Wang, Zhenzhen Wu, Ziyi Fang, Siyuan Heliu, Wei tao Yang, Yang Bai, & Xuan Zhang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c02192
IEEE [1] Jiaye Dai, Zichao Wang, Zhenzhen Wu, Ziyi Fang, Siyuan Heliu, Wei tao Yang, Yang Bai, and Xuan Zhang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c02192. keywords: {shape memory;photoresponse;pyrene;π−π stacking;nearinfrared}