daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on Comprehensive Recovery of Valuable Elements in the Tail Slag from Titanium Tetrachloride Refining by Vanadium Removal with Copper Powder AITranslate

Sichuan JCC Rare Earth Metals CO.,Ltd.;Sichuan JCC Rare Earth Metals CO.,Ltd.;Sichuan JCC Rare Earth Metals CO.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The tail slag from TiCl4 refining by vanadium removal with copper powder is of complex composition,easy to hydrolyze and generate corrosive gas,which seriously pollutes the environment,and the valuable elements are difficult to recover.A new method for recovering copper and other valuable elements was studied according to the characteristics of the compounds contained in the tail slag of TiCl4 refining by vanadium removal with copper powder.It consists of chlorination in NaCl-KCl molten salt,oxidation leaching of CuCl2 with NaOCl,alkaline dechlorination with NaOH,acid leaching with H2SO4,and preparation of CuSO4 by cooling crystallization.CuSO4·5 H2O product with the quality meeting the national and industrial requirements was obtained by washing,filtering and drying of CuSO4·5 H2O crystal.The recovery rate of copper reaches 94.5%.After chlorination process,titanium and vanadium can be separated and recovered by fractional distillation from the distilled mixture of TiCl4 and VOCl3.The waste NaCl-KCl molten salt and NaOCl,which are by-products in the production of titanium sponge,are used as raw materials to reduce the production cost.The filter residue and washing water produced by this process can be reused in the process and titanium sponge production.Therefore,there is no waste generated in this process.

KeyWords AITranslate

titanium tetrachloride refining slag copper chlorination oxidizing leaching alkaline dechlorination acid leaching cooling crystallization

1李定元.我国四氯化钛的铜丝除钒工艺[J].钛工业进展,1996(5):12-14. 被引量:7

2张力萍,王学文,袁继维,龚仕成.粗TiCl4铜丝塔除钒废水的净化新工艺[J].中国有色金属学报,2008,18(6):1159-1163. 被引量:2

3烟伟,蔡万玲.从混合铜矿混酸浸出液中去除Ca和Fe,结晶、重结晶制备CuSO_4·5H_2O工艺研究[J].湿法冶金,2000,19(1):16-20. 被引量:8

4柳云龙,桂劲松.四氯化钛精制车间氯化物泥浆提钒新工艺[J].钛工业进展,2013,30(3):36-39. 被引量:9

5柳云龙.四氯化钛精制尾渣铝钒渣的无害化处理研究[J].轻金属,2014(9):62-64. 被引量:2

6张健,吴贤.国内外海绵钛生产工艺现状[J].钛工业进展,2006,23(2):7-14. 被引量:34

7何耀.利用废铜渣生产硫酸铜及回收有价金属的研究[J].有色冶炼,1999,28(4):38-39. 被引量:15

8李亚军,孙虎民,许伟春.粗四氯化钛除钒工艺现状及发展趋势[J].现代化工,2007,27(6):24-26. 被引量:18

9王学文,张力萍,肖连生,张贵清,袁继维,龚仕成.粗TiCl4铜丝塔除钒废水沉淀泥浆综合回收工艺[J].中国有色金属学报,2008,18(E01):422-427. 被引量:3

10邓彤,文震,刘东.硫酸介质中氯化物参与下氧化浸出铜渣过程[J].中国有色金属学报,2001,11(2):302-306. 被引量:17

1堵伟桐,姜丛翔,陈卓,居殿春,徐玉松.高氯高铁型四氯化钛除钒尾渣焙烧提钒工艺研究[J].矿冶工程,2022,42(2):106-109. 被引量:1

1孙宁,李俊翰.硅藻土对含钒废液中钒的吸附性能研究[J].钢铁钒钛,2022,43(5):111-116.

1孙艳群,任杰,刘乐,王勇山,赖德荣,蓝启铭,王安渊.粗颗粒焙砂碱洗脱氯试验研究及工业应用[J].中国有色冶金,2020,49(2):10-13.

2无.商业银行环境风险分析与管理[J].审计观察,2018(4):90-93.

3贾昇.BIM技术在装配式建筑中的具体运用[J].建筑技术开发,2020(6):37-39.

4瞿昕薇.等离子体发射光谱仪测定四氯化钛中的FeCl3、SiCl4、VOCl3、AlCl3实验方法报告[J].科技风,2020(25):104-105.

5赵浩然,房孟钊,方准.氨氮废水中回收铜与银的试验研究[J].硫磷设计与粉体工程,2020(4):16-19. 被引量:2

6张先茂,陈宗杰,王泽,王国兴.石脑油加氢装置运行总结[J].石油化工应用,2020,39(10):120-122.

7王晓磊.福建省矿山尾矿调查与综合利用研究[J].现代矿业,2020,36(10):105-107.

8陶学勇,竺超皓.建筑钢结构工程吊装安全技术[J].数码设计,2020,9(15):74-74.

9姜晓滨,孙国鑫,贺高红.高效膜蒸馏结晶过程的研究进展[J].化工学报,2020,71(9):3905-3918. 被引量:4

10臧文优,赵娜,王路平,刘慧.新疆某含可溶铜高硫金铜矿石选矿试验[J].现代矿业,2020,36(10):238-239. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TF09[冶金工程—冶金物理化学]

Citation Information:

The tail slag from TiCl4 refining by vanadium removal with copper powder is of complex composition,easy to hydrolyze and generate corrosive gas,which seriously pollutes the environment,and the valuable elements are difficult to recover.A new method for recovering copper and other valuable elements was studied according to the characteristics of the compounds contained in the tail slag of TiCl4 refining by vanadium removal with copper powder.It consists of chlorination in NaCl-KCl molten salt,oxidation leaching of CuCl2 with NaOCl,alkaline dechlorination with NaOH,acid leaching with H2SO4,and preparation of CuSO4 by cooling crystallization.CuSO4·5 H2O product with the quality meeting the national and industrial requirements was obtained by washing,filtering and drying of CuSO4·5 H2O crystal.The recovery rate of copper reaches 94.5%.After chlorination process,titanium and vanadium can be separated and recovered by fractional distillation from the distilled mixture of TiCl4 and VOCl3.The waste NaCl-KCl molten salt and NaOCl,which are by-products in the production of titanium sponge,are used as raw materials to reduce the production cost.The filter residue and washing water produced by this process can be reused in the process and titanium sponge production.Therefore,there is no waste generated in this process.

quote

GB/T 7714-2015 [1] LIU Yun-long, YUAN Hong-xia, GU Xiao-ming. Study on Comprehensive Recovery of Valuable Elements in the Tail Slag from Titanium Tetrachloride Refining by Vanadium Removal with Copper Powder[J]. Rare Metals and Cemented Carbides, 2020(5): 1-4.
MLA [1] LIU Yun-long, et al., "Study on Comprehensive Recovery of Valuable Elements in the Tail Slag from Titanium Tetrachloride Refining by Vanadium Removal with Copper Powder." Rare Metals and Cemented Carbides, no. 5, 2020, pp. 1-4.
APA [1] LIU Yun-long, YUAN Hong-xia, & GU Xiao-ming. (2020). Study on Comprehensive Recovery of Valuable Elements in the Tail Slag from Titanium Tetrachloride Refining by Vanadium Removal with Copper Powder. Rare Metals and Cemented Carbides(5), 1-4.
IEEE [1] LIU Yun-long, YUAN Hong-xia, and GU Xiao-ming, "Study on Comprehensive Recovery of Valuable Elements in the Tail Slag from Titanium Tetrachloride Refining by Vanadium Removal with Copper Powder," Rare Metals and Cemented Carbides, no. 5, pp. 1-4, 2020. keywords: {titanium tetrachloride;refining slag;copper;chlorination;oxidizing leaching;alkaline dechlorination;acid leaching;cooling crystallization}