Development of Zirconium Metal Preparation Method AITranslate

Shandong Silk and Textile Vocational College;School of Chemistry Engineering, Shandong University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The paper summarized the conventional processes for producing zirconium metal, including metallothermic reduction, dehydrogenization and electrolytic process,which have the disadvantages of high cost, serious pollution and complicated operation. It is pointed out that direct electro-deoxidation, a new process for preparing single metal and alloy, is characterized by low cost, less energy consumption,less pollution and simple process. It will most probably replace the given conventional processes for zirconium metal production.

KeyWords AITranslate

Zr metal preparation direct electro-deoxidation ZrO2

1熊炳昆,温旺光,杨新民.锆铪合金[M].北京:冶金工业出版社,2002.

2何季麟.钽铌工业的进步与展望[J].稀有金属,2003,27(1):23-27. 被引量:41

3熊炳昆.锆粉的制备与应用[J].稀有金属快报,2005,24(10):45-47. 被引量:11

4《稀有金属手册》编辑委员会.稀有金属手册(下)[M].北京:冶金工业出版社,1992..

5《稀有金属手册》编辑委员会.稀有金属手册(上)[M].北京:冶金工业出版社,1992.

6Mohandas K S,Fray D J. FFC cambridge process and removal of oxygen from metal-oxygen systemsby molten salt electrolysis:an overview [J]. Trans Indian Inst Met,2005,57:579-592.

7Chen G Z, Fray D J, Farthing T W. Direct electrochemical reduction of titanium dioxide to titanium in molten calcium chloride[J]. Nature, 2000,407 : 361-364.

8Fray D J, Farthing T W, Chen G Z. Removal of oxygen from metal oxides and solid solution electrolysis in a fused salt[P]. UK Pat:PCT/GB99/01781,1998-06-05.

9郭春芳,董云会,于先进.熔盐电脱氧法研究进展[J].材料研究与应用,2007,1(3):178-181. 被引量:12

10郭春芳,董云会,于先进,李德刚,张丽鹏.直接电脱氧法制备金属锆[J].中国有色金属学报,2007,17(6):1019-1023. 被引量:17

1张恒,沈化森,车小奎,王力军.氢化-脱氢法制备锆粉工艺研究[J].稀有金属,2011,35(3):417-421. 被引量:15

2郭春芳,董云会.添加石墨粉对直接电脱氧法制备ZrNi合金的影响[J].稀有金属与硬质合金,2012,40(5):33-36. 被引量:2

3迟煜頔,谈萍,荆鹏,康新婷,王建.制备工艺的控制对锆粉性能的影响[J].热加工工艺,2013,42(12):48-50. 被引量:3

4海敏娜,曾永团,王文,李军献,苑晓刚,张永强,刘继雄,熊富仓,王快社.工业级锆及锆合金焊接的最新研究进展[J].焊接技术,2014,43(4):1-4. 被引量:3

5唐进,海敏娜.工业纯锆焊接接头组织性能[J].电焊机,2014,44(5):217-221.

6海敏娜,曾永团,王文,郝亚鑫,李军献,苑晓刚,张永强,刘继雄,王快社.工业纯锆焊接接头腐蚀性能研究[J].热加工工艺,2014,43(11):174-176.

7孙彦华,杨钢,周林,吴云峰.锆粉制备工艺的研究进展[J].云南冶金,2015,44(1):49-52. 被引量:7

8海敏娜,王快社,王文,郝亚鑫,徐瑞琦,李瑶.纯锆R60702板材焊接接头的腐蚀性能研究[J].稀有金属,2015,39(9):787-792. 被引量:2

9姜菡雨,赵凤起,郝海霞,曲文刚,徐司雨,安亭,李猛.锆/聚叠氮缩水甘油醚复合粒子的制备、表征及静电性能[J].兵工学报,2016,37(1):50-55. 被引量:1

10谢珊珊,李慧,张士宪,刘晓,霍东兴.金属锆的制备工艺[J].热加工工艺,2017,46(4):27-29. 被引量:4

1张天广,王家斌,李刚.工业锆合金焊接方法研究现状[J].中外企业家,2020,0(2):154-154.

2周尧.工业级锆及锆合金焊接技术的最新研究进展[J].中外企业家,2019,0(34):87-87. 被引量:1

3贾雷,严红燕,李慧,刘畅,张帅.金属铪的制备和精炼[J].热加工工艺,2020,0(1):10-15. 被引量:1

4王芳,江洪林,尹延西,张顺利,黄永章,王力军.烧结温度对铪块孔隙结构和成分的影响[J].稀有金属,2013,37(1):108-111. 被引量:3

5迟煜頔,谈萍,荆鹏,康新婷,王建.制备工艺的控制对锆粉性能的影响[J].热加工工艺,2013,42(12):48-50. 被引量:3

6唐进,海敏娜.工业纯锆焊接接头组织性能[J].电焊机,2014,44(5):217-221.

7王静哲,张家敏,易健宏,甘国友,刘意春.基于TiH_2粉末制备Ti-13Nb-13Zr合金的微观组织与结构[J].稀有金属材料与工程,2019,48(1):152-158. 被引量:2

8孙彦华,杨钢,周林,吴云峰.锆粉制备工艺的研究进展[J].云南冶金,2015,44(1):49-52. 被引量:7

9李国玲,田丰,李里,田文怀,李星国.氢等离子体电弧熔炼技术在难熔金属提纯中的应用[J].稀有金属材料与工程,2015,44(3):775-780. 被引量:11

10孙彦华,尚青亮,杨钢,方树铭,吴云峰.超细氢化锆粉制备工艺的研究[J].铸造技术,2015,36(3):676-677. 被引量:2

1郭春芳,董云会.添加石墨粉对直接电脱氧法制备金属锆的影响[J].稀有金属与硬质合金,2012,40(2):10-14. 被引量:1

2郭春芳,董云会,于先进,李德刚,张丽鹏.直接电脱氧法制备金属锆[J].中国有色金属学报,2007,17(6):1019-1023. 被引量:17

3郝斌.氢化脱氢法的低氧钛粉末制造技术[J].稀有金属快报,1995(12):18-19.

4冯颖芳,张震.钛粉的生产及应用[J].钛工业进展,2000,17(6):6-9. 被引量:2

5孙彦华,杨钢,周林,吴云峰.锆粉制备工艺的研究进展[J].云南冶金,2015,44(1):49-52. 被引量:7

6佐藤一,李志生.制取金属锆的还原—蒸馏联合法[J].国外稀有金属,1990(4):15-21.

7熊炳昆.锆在有色金属材料中的应用[J].稀有金属快报,2005,24(6):45-47. 被引量:6

8郭春芳,张明.提高直接电脱氧法电流效率的研究进展[J].材料研究与应用,2012,6(1):5-8.

9吴延科,李庆彬,徐志高,王力军,熊炳昆.金属锆的制备方法[J].稀有金属,2009,33(4):462-466. 被引量:15

10郭春芳,董云会,于先进,张丽鹏,李德刚.ZrO_2直接电脱氧反应机理的初步研究[J].山东理工大学学报:自然科学版,2007,21(3):65-67. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TF841.4[冶金工程—有色金属冶金]

Citation Information:

The paper summarized the conventional processes for producing zirconium metal, including metallothermic reduction, dehydrogenization and electrolytic process,which have the disadvantages of high cost, serious pollution and complicated operation. It is pointed out that direct electro-deoxidation, a new process for preparing single metal and alloy, is characterized by low cost, less energy consumption,less pollution and simple process. It will most probably replace the given conventional processes for zirconium metal production.

quote

GB/T 7714-2015 [1] GUO Chun-fang, DONG Yun-hui. Development of Zirconium Metal Preparation Method[J]. Rare Metals and Cemented Carbides, 2008(2): 63-67.
MLA [1] GUO Chun-fang, and DONG Yun-hui. "Development of Zirconium Metal Preparation Method." Rare Metals and Cemented Carbides, no. 2, 2008, pp. 63-67.
APA [1] GUO Chun-fang, & DONG Yun-hui. (2008). Development of Zirconium Metal Preparation Method. Rare Metals and Cemented Carbides(2), 63-67.
IEEE [1] GUO Chun-fang and DONG Yun-hui, "Development of Zirconium Metal Preparation Method," Rare Metals and Cemented Carbides, no. 2, pp. 63-67, 2008. keywords: {Zr metal;preparation;direct electro-deoxidation;ZrO2}