Quantum Dot–Block Copolymer Hybrids for Low Scattering Luminescent Solar Concentrators AITranslate
Abstract AITranslate
Luminescent solar concentrators (LSCs) use down-converting phosphors embedded in a transparent waveguide to absorb sunlight, trap luminescent photons by total internal reflection, and deliver high irradiance, narrowband output light for driving photovoltaic, photochemical, and other solar energy converters. Quantum-dot-based (QD) LSCs are typically affected by several optical loss mechanisms including the loss of a fraction of guided light during transport to the concentrator edges through scattering from QD aggregates. Although the recent introduction of large effective Stokes shift QD luminophores for LSC applications has helped address several shortcomings associated with previous generations of organic and inorganic dyes, including improved solar spectrum matching, photostability, and photoluminescence quantum yield, achieving low light scattering at technologically relevant QD loadings in commercially deployed polymers such as poly(methyl methacrylate) (PMMA) remains challenging. Herein, we study the concept of applying QDs bearing polymer ligands matching the composition of the LSC matrix to reduce aggregation and the resulting parasitic waveguide losses caused by scattering. We report the synthesis and characterization of a thiol-terminated PMMA-based ligand and its successful ligand exchange reaction with copper indium disulfide/zinc sulfide (CIS/ZnS) QDs. QDs bearing PMMA ligands are then applied as down-converting phosphors embedded in a PMMA waveguide. The resulting QD-based LSCs were found to have lower optical scattering with higher loading as a result of reduced aggregation in the devices.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c01837
Chinese Library Classification Number:
Citation Information:
Luminescent solar concentrators (LSCs) use down-converting phosphors embedded in a transparent waveguide to absorb sunlight, trap luminescent photons by total internal reflection, and deliver high irradiance, narrowband output light for driving photovoltaic, photochemical, and other solar energy converters. Quantum-dot-based (QD) LSCs are typically affected by several optical loss mechanisms including the loss of a fraction of guided light during transport to the concentrator edges through scattering from QD aggregates. Although the recent introduction of large effective Stokes shift QD luminophores for LSC applications has helped address several shortcomings associated with previous generations of organic and inorganic dyes, including improved solar spectrum matching, photostability, and photoluminescence quantum yield, achieving low light scattering at technologically relevant QD loadings in commercially deployed polymers such as poly(methyl methacrylate) (PMMA) remains challenging. Herein, we study the concept of applying QDs bearing polymer ligands matching the composition of the LSC matrix to reduce aggregation and the resulting parasitic waveguide losses caused by scattering. We report the synthesis and characterization of a thiol-terminated PMMA-based ligand and its successful ligand exchange reaction with copper indium disulfide/zinc sulfide (CIS/ZnS) QDs. QDs bearing PMMA ligands are then applied as down-converting phosphors embedded in a PMMA waveguide. The resulting QD-based LSCs were found to have lower optical scattering with higher loading as a result of reduced aggregation in the devices.
quote
| GB/T 7714-2015 | [1] Kayla C. Koch, Daniel Korus, Justin Doyle, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01837. |
| MLA | [1] Kayla C. Koch, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01837. |
| APA | [1] Kayla C. Koch, Daniel Korus, Justin Doyle, Megan Plummer, Meredith Boxx, Hla WinPiazza, Stephen McDowall, David L. Patrick, & David A. Rider. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01837 |
| IEEE | [1] Kayla C. Koch, Daniel Korus, Justin Doyle, Megan Plummer, Meredith Boxx, Hla WinPiazza, Stephen McDowall, David L. Patrick, and David A. Rider, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01837. keywords: {luminescent solar concentrator;quantum dot;nanocrystal;ligands;block copolymer;polymer composites;solar concentration} |