daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Fast and Reversible Cross-Linking Reactions of Thermoresponsive Polymers Based on Dynamic Dialkylaminodisulfide Exchange AITranslate

Tokyo Institute of Technology; Tokyo Institute of Technology; Tokyo Institute of Technology; Tokyo Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Thermoresponsive polymers that can cross-link rapidly and reversibly under solvent-free conditions via the dynamic exchange of bis(hindered amino)disulfide (BiTEMPS) units have been prepared. Linear polymers with BiTEMPS units in their side chains were synthesized via free-radical copolymerization of hexyl methacrylate and a BiTEMPS-containing methacrylate monomer. When a polymer containing 5 mol % BiTEMPS was heated to 120 °C in the bulk, a cross-linked polymer was obtained within 10 min via exchange reactions of BiTEMPS units. The thermal cross-linking behavior of the linear polymer was investigated using in situ rheological measurements. Tensile tests indicated that the BiTEMPS-based small molecules generated during the cross-linking reaction acted as a plasticizer and enhanced the toughness of the polymer. A de-cross-linking reaction was also achieved under solvent-free conditions via an exchange reaction between the cross-linked polymer and a low-molecular-weight BiTEMPS derivative, which resulted in structural transformation to the original state. The structural transformation and the physical properties of the original linear polymer and the cross-linked polymers were characterized using gel permeation chromatography, rheology, tensile tests, and swelling experiments.

KeyWords AITranslate

dynamic covalent chemistry polymer reactions disulfide bonds crosslinked polymers decrosslinking
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01205

Chinese Library Classification Number:

Citation Information:

Thermoresponsive polymers that can cross-link rapidly and reversibly under solvent-free conditions via the dynamic exchange of bis(hindered amino)disulfide (BiTEMPS) units have been prepared. Linear polymers with BiTEMPS units in their side chains were synthesized via free-radical copolymerization of hexyl methacrylate and a BiTEMPS-containing methacrylate monomer. When a polymer containing 5 mol % BiTEMPS was heated to 120 °C in the bulk, a cross-linked polymer was obtained within 10 min via exchange reactions of BiTEMPS units. The thermal cross-linking behavior of the linear polymer was investigated using in situ rheological measurements. Tensile tests indicated that the BiTEMPS-based small molecules generated during the cross-linking reaction acted as a plasticizer and enhanced the toughness of the polymer. A de-cross-linking reaction was also achieved under solvent-free conditions via an exchange reaction between the cross-linked polymer and a low-molecular-weight BiTEMPS derivative, which resulted in structural transformation to the original state. The structural transformation and the physical properties of the original linear polymer and the cross-linked polymers were characterized using gel permeation chromatography, rheology, tensile tests, and swelling experiments.

quote

GB/T 7714-2015 [1] Shimon Kataoka, Ayuko Tsuruoka, Daisuke Aoki, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01205.
MLA [1] Shimon Kataoka, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01205.
APA [1] Shimon Kataoka, Ayuko Tsuruoka, Daisuke Aoki, & Hideyuki Otsuka. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01205
IEEE [1] Shimon Kataoka, Ayuko Tsuruoka, Daisuke Aoki, and Hideyuki Otsuka, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01205. keywords: {dynamic covalent chemistry;polymer reactions;disulfide bonds;crosslinked polymers;decrosslinking}