daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

UV-Resistant Trifluoropropyl-Substituted Open-Cage Silsesquioxane-Pendant Polysiloxanes AITranslate

Kyoto Institute of Technology; Kyoto Institute of Technology; Kyoto Institute of Technology; Kyoto Institute of Technology; Kyoto Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We prepared three types of tris(dimethoxysilyl)-heptatrifluoropropyl-substituted open-cage silsesquioxanes, namely hepta(3,3,3-trifluoropropyl)-substituted open-cage silsesquioxanes (IC-POSSs) attached to three dimethoxysilyl groups by linkers of variable lengths at the opening vertex (TFP-Hdi, TFP-Vdi, and TFP-Adi). The dimethoxysilyl groups allowed subsequent hydrolysis and polycondensation under mild conditions to form flexible siloxane bonds. The structures of the resulting trifluoropropyl-substituted open-cage silsesquioxane-pendant polysiloxanes (P-H, P-V, and P-A) could be tuned by polycondensation temperature and the linker lengths of the tris(dimethoxysilyl)-heptatrifluoropropyl-substituted open-cage silsesquioxanes. The hybrid structure of the trifluoropropyl-substituted open-cage silsesquioxane-pendant polysiloxanes exhibited a low glass transition temperature, good thermal stability, hydrophobicity, optical transparency, and ultraviolet (UV) resistance. In particular, the transmittance of P-H exhibited no significant changes even after 11 days of UV irradiation with an average transmittance of >90% (250–600 nm). On the other hand, the transmittance of sulfur-containing P-V and P-A initially decreased after 2 days of irradiation due to oxidation of sulfur atoms to sulfoxide. Sulfoxide presence was then validated by XPS measurements. However, the transmittance remained largely unchanged during further consistent irradiation, indicating no further changes.

KeyWords AITranslate

Cage silsesquioxanes fluorine alkoxysilanes hydrolysis condensation polysiloxane UV resistance
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01236

Chinese Library Classification Number:

Citation Information:

We prepared three types of tris(dimethoxysilyl)-heptatrifluoropropyl-substituted open-cage silsesquioxanes, namely hepta(3,3,3-trifluoropropyl)-substituted open-cage silsesquioxanes (IC-POSSs) attached to three dimethoxysilyl groups by linkers of variable lengths at the opening vertex (TFP-Hdi, TFP-Vdi, and TFP-Adi). The dimethoxysilyl groups allowed subsequent hydrolysis and polycondensation under mild conditions to form flexible siloxane bonds. The structures of the resulting trifluoropropyl-substituted open-cage silsesquioxane-pendant polysiloxanes (P-H, P-V, and P-A) could be tuned by polycondensation temperature and the linker lengths of the tris(dimethoxysilyl)-heptatrifluoropropyl-substituted open-cage silsesquioxanes. The hybrid structure of the trifluoropropyl-substituted open-cage silsesquioxane-pendant polysiloxanes exhibited a low glass transition temperature, good thermal stability, hydrophobicity, optical transparency, and ultraviolet (UV) resistance. In particular, the transmittance of P-H exhibited no significant changes even after 11 days of UV irradiation with an average transmittance of >90% (250–600 nm). On the other hand, the transmittance of sulfur-containing P-V and P-A initially decreased after 2 days of irradiation due to oxidation of sulfur atoms to sulfoxide. Sulfoxide presence was then validated by XPS measurements. However, the transmittance remained largely unchanged during further consistent irradiation, indicating no further changes.

quote

GB/T 7714-2015 [1] Lina Li, Hiroaki Imoto, Arifumi Okada, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01236.
MLA [1] Lina Li, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01236.
APA [1] Lina Li, Hiroaki Imoto, Arifumi Okada, Kenji Kanaori, & Kensuke Naka. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01236
IEEE [1] Lina Li, Hiroaki Imoto, Arifumi Okada, Kenji Kanaori, and Kensuke Naka, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01236. keywords: {Cage silsesquioxanes;fluorine;alkoxysilanes;hydrolysis;condensation;polysiloxane;UV resistance}