daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on shear strength and deformation characteristics of sandy silt improved by cement under hydrothermal action AITranslate

Lanzhou Jiaotong University; Lanzhou Jiaotong University; Lanzhou Jiaotong University; Lanzhou Jiaotong University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

At present, researches on the stability of sandy silt improved by cement (SS-C) are abundant, but there are few researches on the shear strength and deformation characteristics of it under the conditions of low temperature and different moisture content in cold regions. Firstly, sandy silt was selected as the research object, which the liquid limit (wL) is 28.6% and plasticity index (IP) is 8.9, the coefficient of nonuniformity (Cu) is 61.5, and the optimum cement incorporation ratio was determined as 6% according to the maximum direct shear strength at − 7 ℃. Secondly, the SS-C was tested by direct shear at different temperatures (−2 ℃, −5 ℃, −7 ℃, −14 ℃) and moisture contents (13.0%, 15.2%, 18.0%). Subsequently, the effects of temperature and moisture content on shear strength and shear modulus were calculated and analyzed. The results show that when the temperature drops from − 2 ℃ to − 7 ℃, the cohesion of the SS-C increases by 243.4%; when from − 7 ℃ to − 14 ℃, it continues to increase by 285.7% compared with that at − 2 ℃, and the internal friction angle of the SS-C also shows a similar variation law with the temperature. At − 7 ℃, when the initial moisture content increases from 13.0% to 15.2%, the increase of cohesion is about 8.6%; when from 15.2% to 18.0%, it is about 22.8%, while the change of internal friction angle is less than 1%. Finally, the impact of hydrothermal action on the failure ratio of the SS-C was analyzed, and the relation equation between shear strength and tangent elastic modulus of the SS-C was established.

KeyWords AITranslate

Improved sandy silt Hydrothermal action Shear strength Deformation properties
No data

Basic Information:

DOI:https://doi.org/10.1016/j.cscm.2022.e01207

Chinese Library Classification Number:

Citation Information:

At present, researches on the stability of sandy silt improved by cement (SS-C) are abundant, but there are few researches on the shear strength and deformation characteristics of it under the conditions of low temperature and different moisture content in cold regions. Firstly, sandy silt was selected as the research object, which the liquid limit (wL) is 28.6% and plasticity index (IP) is 8.9, the coefficient of nonuniformity (Cu) is 61.5, and the optimum cement incorporation ratio was determined as 6% according to the maximum direct shear strength at − 7 ℃. Secondly, the SS-C was tested by direct shear at different temperatures (−2 ℃, −5 ℃, −7 ℃, −14 ℃) and moisture contents (13.0%, 15.2%, 18.0%). Subsequently, the effects of temperature and moisture content on shear strength and shear modulus were calculated and analyzed. The results show that when the temperature drops from − 2 ℃ to − 7 ℃, the cohesion of the SS-C increases by 243.4%; when from − 7 ℃ to − 14 ℃, it continues to increase by 285.7% compared with that at − 2 ℃, and the internal friction angle of the SS-C also shows a similar variation law with the temperature. At − 7 ℃, when the initial moisture content increases from 13.0% to 15.2%, the increase of cohesion is about 8.6%; when from 15.2% to 18.0%, it is about 22.8%, while the change of internal friction angle is less than 1%. Finally, the impact of hydrothermal action on the failure ratio of the SS-C was analyzed, and the relation equation between shear strength and tangent elastic modulus of the SS-C was established.

quote

GB/T 7714-2015 [1] Yu Zhang, Jie Liu, Ying Ma, et al. Case Studies in Construction Materials, 2022(17). DOI:10.1016/j.cscm.2022.e01207.
MLA [1] Yu Zhang, et al., Case Studies in Construction Materials, no. 17, 2022, https://doi.org/10.1016/j.cscm.2022.e01207.
APA [1] Yu Zhang, Jie Liu, Ying Ma, & Jianning Li. (2022). Case Studies in Construction Materials(17). https://doi.org/10.1016/j.cscm.2022.e01207