Control of Guest Thermal Release by Crystalline Host Orientation AITranslate
Abstract AITranslate
Thermal release of guest molecules from poly(2,6-dimethyl-1,4-phenylene)oxide (PPO) films, exhibiting host–guest co-crystalline (CC) phases with orientation of their chain axes being preferentially parallel or perpendicular to the film plane (c// and c⊥ orientations), is studied. TGA analyses show that, for all the considered CC PPO films, temperatures of guest release for CC films with c// orientation are definitely higher than those for CC films with c⊥ orientation, with differences even higher than 100 °C. Correspondingly, DSC scans of CC films with c⊥ orientation show separated endothermic peaks of guest release and melting, while CC films with c// orientation only exhibit one broad endothermic peak with superimposed guest release, glass transition (Tg), and melting (Tm) phenomena. This control of temperatures of guest release could be helpful to maximize the thermal stability of host–guest PPO co-crystalline phases and to tailor temperatures of active guest release.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.0c01246
Chinese Library Classification Number:
Citation Information:
Thermal release of guest molecules from poly(2,6-dimethyl-1,4-phenylene)oxide (PPO) films, exhibiting host–guest co-crystalline (CC) phases with orientation of their chain axes being preferentially parallel or perpendicular to the film plane (c// and c⊥ orientations), is studied. TGA analyses show that, for all the considered CC PPO films, temperatures of guest release for CC films with c// orientation are definitely higher than those for CC films with c⊥ orientation, with differences even higher than 100 °C. Correspondingly, DSC scans of CC films with c⊥ orientation show separated endothermic peaks of guest release and melting, while CC films with c// orientation only exhibit one broad endothermic peak with superimposed guest release, glass transition (Tg), and melting (Tm) phenomena. This control of temperatures of guest release could be helpful to maximize the thermal stability of host–guest PPO co-crystalline phases and to tailor temperatures of active guest release.
quote
| GB/T 7714-2015 | [1] Baku Nagendra, Giovanni Mondrone, Christophe Daniel, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01246. |
| MLA | [1] Baku Nagendra, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01246. |
| APA | [1] Baku Nagendra, Giovanni Mondrone, Christophe Daniel, Paola Rizzo, & Gaetano Guerra. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01246 |
| IEEE | [1] Baku Nagendra, Giovanni Mondrone, Christophe Daniel, Paola Rizzo, and Gaetano Guerra, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01246. keywords: {planar orientation;crystalline host anisotropy;thermogravimetry;differential scanning calorimetry;WAXD} |