Analysis of Deterioration Cause and Investigation on the Stability Control Measures of Molten Salt System in TiCl_4 Molten Salt Chlorinator AITranslate

Guiyang Aluminum Magnesium Design Research Institute Co., Ltd.;Guiyang Aluminum Magnesium Design Research Institute Co., Ltd.;Guiyang Aluminum Magnesium Design Research Institute Co., Ltd.;Guiyang Aluminum Magnesium Design Research Institute Co., Ltd.;Guiyang Aluminum Magnesium Design Research Institute Co., Ltd.;Guiyang Aluminum Magnesium Design Research Institute Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The characterization parameters are summarized for performance evaluation of molten salt system in TICl4 molten salt chlorinator, and a preliminary analysis of its influencing factors is carried out. The causes of molten salt system deterioration during TICl4 molten salt chlorination are analyzed based on pro duction practice. According to the causes of molten salt system deterioration and the related factors,control measures for molten salt system stability are presented.

KeyWords AITranslate

TICl4 molten salt chlorination molten salt system deterioration cause analysis stability control measure

1王晓平.海绵钛生产工业现状及发展趋势[J].钛工业进展,2011,28(2):8-13. 被引量:10

2肖永华.熔盐氯化炉热平衡分析[J].钛工业进展,2005,22(1):36-38. 被引量:4

3常跃仁.四氯化钛生产工艺研究[J].有色矿冶,2009,25(4):37-39. 被引量:16

4程国荣.攀枝花钛渣熔盐氯化盐系组成的研究[J].钢铁钒钛,1998,19(2):9-12. 被引量:12

5居殿春,卿阳,严定鎏,陈志勇,李向阳.氯化物熔盐中钙镁离子固化工艺的热力学分析[J].钢铁钒钛,2011,32(3):25-29. 被引量:9

1杨大锦.2014年云南冶金年评[J].云南冶金,2015,44(2):44-66.

2李亮,李开华,苗庆东,徐宗宝,陈爱祥,夏建辉.钛渣熔盐氯化过程熔盐成分合格率影响因素分析[J].轻金属,2016,0(2):47-50. 被引量:2

3李亮,陈爱祥,李开华,苗庆东,徐宗宝,夏建辉.钛渣熔盐氯化炉稳定运行影响因素[J].轻金属,2016,0(5):38-42. 被引量:1

4陈祖春,何运秋,杨晓军.浅谈熔盐氯化工艺的“三废”治理[J].世界有色金属,2016,0(9):60-61. 被引量:1

5张苏新.熔盐氯化生产TiCl_4过程中固含量控制技术研究[J].钛工业进展,2018,35(5):42-46.

6陈凤,问悦凯,郭宇峰,郑富强,王帅,杨凌志,郑宇,李冬月,任雨荞.氯化熔盐体系黏度特性研究现状[J].无机盐工业,2022,54(6):1-5.

1李亮,陈爱祥,李开华,苗庆东,徐宗宝,夏建辉.钛渣熔盐氯化炉稳定运行影响因素[J].轻金属,2016,0(5):38-42. 被引量:1

2杨大锦.2016年云南冶金年评[J].云南冶金,2017,46(2):58-78.

3刘佳媛.熔盐氯化生产四氯化钛工艺研究[J].现代矿业,2019,35(5):221-225. 被引量:4

4贾要强,李亮,蒋文龙,邓攀,刘大春.四氯化钛制备用熔盐体系及其物性研究进展[J].昆明理工大学学报:自然科学版,2021,46(2):1-12. 被引量:1

1韩明堂.对大型熔盐氯化炉设计中的一些问题的看法和探讨[J].钒钛,1994(2):57-60. 被引量:2

2王德英.熔盐氯化炉氯化反应最高理论温度及其引热措施的探讨[J].钢铁钒钛,1990,11(3):74-79. 被引量:2

3陈怀忠,岳丽华.熔盐氯化炉锥体内衬砖尺寸计算[J].辽宁工业大学学报:自然科学版,1999,0(S1):21-22.

4居殿春,陈志勇,卿阳,严定鎏,李向阳.熔盐氯化炉稳态温度场有限元分析[J].钢铁钒钛,2011,32(2):25-28. 被引量:2

5胡元金.熔盐氯化炉保温期间的热平衡[J].轻工科技,2012,28(6):26-27. 被引量:2

6李亮,陈爱祥,李开华,苗庆东,徐宗宝,夏建辉.钛渣熔盐氯化炉稳定运行影响因素[J].轻金属,2016,0(5):38-42. 被引量:1

7杨健,李宗雄.钛渣熔盐氯化炉内氯气分布的冷态模拟研究[J].钒钛,1994(5):46-52.

8居殿春,严定鎏,李向阳,马恩权,臧颖波,李俊强.高钛渣加碳氯化反应热力学在熔盐氯化中的应用[J].钢铁钒钛,2010,31(2):32-36. 被引量:13

9杨健,薛生晖.樊矿钛渣熔盐氯化炉内固体物料分布[J].钒钛,1995(1):48-53.

10毕学工,杨绪平,李宏玉,李鹏.高炉异常炉况预报专家系统研究[J].河南冶金,2011,19(4):5-8. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TF823[冶金工程—有色金属冶金]

Citation Information:

The characterization parameters are summarized for performance evaluation of molten salt system in TICl4 molten salt chlorinator, and a preliminary analysis of its influencing factors is carried out. The causes of molten salt system deterioration during TICl4 molten salt chlorination are analyzed based on pro duction practice. According to the causes of molten salt system deterioration and the related factors,control measures for molten salt system stability are presented.

quote

GB/T 7714-2015 [1] LU Hui, WANG Hao, YANG Ren-mu, et al. Analysis of Deterioration Cause and Investigation on the Stability Control Measures of Molten Salt System in TiCl_4 Molten Salt Chlorinator[J]. Rare Metals and Cemented Carbides, 2014(2): 16-22.
MLA [1] LU Hui, et al., "Analysis of Deterioration Cause and Investigation on the Stability Control Measures of Molten Salt System in TiCl_4 Molten Salt Chlorinator." Rare Metals and Cemented Carbides, no. 2, 2014, pp. 16-22.
APA [1] LU Hui, WANG Hao, YANG Ren-mu, MENG Jun, XIE Gang, & XIE Hong-yan. (2014). Analysis of Deterioration Cause and Investigation on the Stability Control Measures of Molten Salt System in TiCl_4 Molten Salt Chlorinator. Rare Metals and Cemented Carbides(2), 16-22.
IEEE [1] LU Hui, WANG Hao, YANG Ren-mu, MENG Jun, XIE Gang, and XIE Hong-yan, "Analysis of Deterioration Cause and Investigation on the Stability Control Measures of Molten Salt System in TiCl_4 Molten Salt Chlorinator," Rare Metals and Cemented Carbides, no. 2, pp. 16-22, 2014. keywords: {TICl4 molten salt chlorination;molten salt system deterioration;cause analysis;stability control measure}