Effect of Restricted Multi-Directional Forging on the Microstructure and Properties of Ti2AlNb-Based Alloy AITranslate

School of Materials Science and Engineering,Hefei University of Technology;School of Materials Science and Engineering,Hefei University of Technology;School of Materials Science and Engineering,Hefei University of Technology;School of Materials Science and Engineering,Hefei University of Technology;School of Materials Science and Engineering,Hefei University of Technology;School of Materials Science and Engineering,Hefei University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ti2AlNb-based alloy was subjected to three passes of isothermally restricted multi-directional forging(R-MDF) in the B2+O phase region.The microstructure of the deformed alloy samples was analyzed using metallographic microscope,X-ray diffractometer,scanning electron microscope,and transmission electron microscope.Quantitative analysis of the total volume fraction of O phase,width and volume fraction of lamellar O phase,and size of equiaxed O phase in each pass of multi-directional forging was conducted using Image software,aiming to study the deformation behavior of O phase in different passes.Vickers hardness test was conducted on Ti2AlNb-based alloy samples in different passes to reveal the relationship between microstructure and microhardness after multi-directional forging.The research results show that after deformation,coarse lamellar O phase fragments and refines into equiaxed O phase.After different passes of multi-directional forging,the size of equiaxed O phase initially increases from 0.57 μm in the first pass to 1.24 μm in the second pass and then gradually decreases,reaching an average size of approximately 0.84 μm after the third pass.Compared with the initial sample,the microhardness of the samples in each pass increases by approximately 15.4%,22.2%,and 14.8%,respectively.

KeyWords AITranslate

Ti2AlNb isothermally restricted multi-directional forging microstructure microhardness

1金怡然,孙书杰.“劝”之“劝说”义的产生过程及动因[J].河北科技师范学院学报(社会科学版),2024,23(2):97-102.

2邓勇,胡德胜,游君君,满勇,满晓,陈林,付大巍.南海西部原油领域勘探进展与突破方向[J].中国海上油气,2024,36(3):11-24.

3黄颖,周犇犇,李宝磊,幸亮,王达.一种基于种群划分的分布式自适应差分进化算法[J].赣南师范大学学报,2024,45(3):23-29.

4苏丽婷.金属材料常用硬度检测方法[J].一重技术,2024(3):38-42.

5WANG Min,LI Han,HU Bintao,TANG Chunping,XU Hui,KE Changqiang,XIE Zuoquan,YE Yang,YAO Sheng.Anti-inflammatory germacrane-type sesquiterpene lactones from Vernonia sylvatica[J].Chinese Journal of Natural Medicines,2024,22(6):568-576.

6马军,陈嘉琪,王学朋,何涛,戴万祥.不同重熔工艺下Ni60A涂层试验研究[J].中国新技术新产品,2024(11):46-49.

7陈佳颖,吴迪,党彤,汤泊夫,刘琳,贾语婧,李志伟.探头式共聚焦激光显微内镜量化指标诊断幽门螺杆菌相关萎缩性胃炎的临床研究[J].中华消化内镜杂志,2024,41(6):465-471.

8MOHAMMAD-TAGHI MORADI,DHIYA ALTEMEMY,MAJID ASADI-SAMANI,PEGAH KHOSRAVIAN,MARZIYEH SOLTANI,LEILA HASHEMI,AZADEH SAMIEI-SEFAT.The effect of celastrol in combination with 5-fluorouracil on proliferation and apoptosis of gastric cancer cell lines[J].Oncology Research,2024,32(7):1231-1237.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.416[金属学及工艺—金属材料]

Citation Information:

Ti2AlNb-based alloy was subjected to three passes of isothermally restricted multi-directional forging(R-MDF) in the B2+O phase region.The microstructure of the deformed alloy samples was analyzed using metallographic microscope,X-ray diffractometer,scanning electron microscope,and transmission electron microscope.Quantitative analysis of the total volume fraction of O phase,width and volume fraction of lamellar O phase,and size of equiaxed O phase in each pass of multi-directional forging was conducted using Image software,aiming to study the deformation behavior of O phase in different passes.Vickers hardness test was conducted on Ti2AlNb-based alloy samples in different passes to reveal the relationship between microstructure and microhardness after multi-directional forging.The research results show that after deformation,coarse lamellar O phase fragments and refines into equiaxed O phase.After different passes of multi-directional forging,the size of equiaxed O phase initially increases from 0.57 μm in the first pass to 1.24 μm in the second pass and then gradually decreases,reaching an average size of approximately 0.84 μm after the third pass.Compared with the initial sample,the microhardness of the samples in each pass increases by approximately 15.4%,22.2%,and 14.8%,respectively.

quote

GB/T 7714-2015 [1] XUE Ke-min, ZHI Qiang, DING Rui-dong, et al. Effect of Restricted Multi-Directional Forging on the Microstructure and Properties of Ti2AlNb-Based Alloy[J]. Rare Metals and Cemented Carbides, 2024(3): 66-71.
MLA [1] XUE Ke-min, et al., "Effect of Restricted Multi-Directional Forging on the Microstructure and Properties of Ti2AlNb-Based Alloy." Rare Metals and Cemented Carbides, no. 3, 2024, pp. 66-71.
APA [1] XUE Ke-min, ZHI Qiang, DING Rui-dong, SHI Cheng-feng, YU Ren-hai, & LI Ping. (2024). Effect of Restricted Multi-Directional Forging on the Microstructure and Properties of Ti2AlNb-Based Alloy. Rare Metals and Cemented Carbides(3), 66-71.
IEEE [1] XUE Ke-min, ZHI Qiang, DING Rui-dong, SHI Cheng-feng, YU Ren-hai, and LI Ping, "Effect of Restricted Multi-Directional Forging on the Microstructure and Properties of Ti2AlNb-Based Alloy," Rare Metals and Cemented Carbides, no. 3, pp. 66-71, 2024. keywords: {TiAlNb;isothermally restricted multi-directional forging;microstructure;microhardness}