Electrochemical Research and Performance Characterization of Ni-Co/ZrO_2 Composite Coatings AITranslate

School of Materials and Metallurgy,University of Science and Technology Liaoning;School of Materials and Metallurgy,University of Science and Technology Liaoning;School of Materials and Metallurgy,University of Science and Technology Liaoning;School of Materials and Metallurgy,University of Science and Technology Liaoning;School of Materials and Metallurgy,University of Science and Technology Liaoning
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ni-Co/ZrO2 composite coatings were prepared by co-deposition technology in acid sulfamate solu-tion. The effects of nanopartieles in Ni-Co/ZrO2 composite system on its electrochemical reaction process were studied by cathode linear scan test. The surface morphology and mierostructure of the composite coat-ings were analyzed by SEM and XRD. The corrosion resistance of the composite coatings was tested by Tafel curves and their thermal stability was characterized by microhardness test after annealing. The exper-imental results show that Ni-Co/ZrO2 co-deposition potential is about --0.90 V. Compared with Ni-Co al-loy,Ni-Co/ZrO2 composite coating surface is more uniform and compact,the grains are smaller,and its cor- rosion resistance and thermal stability are better.

KeyWords AITranslate

Ni-Co/ZrO2 composite coating co-deposition LSV curve Tafel test grain orientation

1郑文裕,陈潮钿,陈仲丛.二氧化锆的性质、用途及其发展方向[J].无机盐工业,2000,32(1):18-20. 被引量:54

2王国庆,尉海军,朱磊,简旭宇.Ni-Mo-Co合金电极制备工艺的研究[J].稀有金属与硬质合金,2011,39(1):21-24. 被引量:1

3张刚,赵中伟,霍广生,孙召明.阴极电沉积法制备钛基生物陶瓷复合材料的研究进展[J].稀有金属与硬质合金,2003,31(3):21-26. 被引量:6

4冯秋元,李廷举,金俊泽.复合电镀机理研究及最新进展[J].稀有金属材料与工程,2007,36(3):559-564. 被引量:38

5周海飞,钱洲亥,祝郦伟,杜楠.搅拌在Ni-diamond复合电沉积中的电化学行为[J].稀有金属材料与工程,2014,43(2):470-474. 被引量:6

6赵旭山,谭澄宇,陈文敬,刘宇,李劲风,郑子樵.Ni-SiC复合镀层电结晶初期动力学分析[J].中国有色金属学报,2008,18(5):823-828. 被引量:18

1敬双怡,侯娜,范保建,于玲红,李卫平,殷震育.稀土镨电极处理焦化尾水过程特性研究[J].现代化工,2021,41(8):139-144.

1郑翠翠,辛晨光,黄伟,杜亚雯,石标,朱世杰,姚鑫,范琳,魏长春,丁毅,李跃龙,王广才,许盛之,赵颖,张晓丹.一步沉积法中溴基钙钛矿薄膜的优化及应用[J].人工晶体学报,2018,47(7):1305-1311.

2汪笑鹤,胡振峰,吕镖,李锋,丁光雨.电刷镀n-Al_2O_3/Ni-Co纳米复合镀层的制备及摩擦学性能[J].材料保护,2018,51(8):69-72.

3杨文通,郭文亮,宫晓琴,李月敏,宋磊.面积和方向对铝电极性能的影响[J].电源技术,2018,42(10):1524-1525.

4汪太淼,朱云峰,刘雅娜,林怀俊,李李泉.PMMA/MWCNTs复合膜包覆Mg_3MnNi_2合金电极的电化学性能研究[J].电源技术,2018,42(10):1500-1503.

5王鑫,纪利俊,陈葵,武斌,吴艳阳,朱家文.pH与Ca^(2+)浓度对磷石膏常压制备α-半水硫酸钙的影响[J].无机盐工业,2017,49(11):56-60. 被引量:9

6于文肖,罗鸣,马争.镍在不同电解质溶液中的钝化行为的研究[J].全面腐蚀控制,2018,32(10):69-72.

7谢治辉.SDBS对镁合金LDHs涂层的缓释作用[J].兵器材料科学与工程,2018,41(4):23-26. 被引量:1

8郭方,孙万昌,张磊,贾宗伟,刘晓佳,董亚茹.LaCl3含量对Ni-P涂层耐腐蚀性能的影响[J].热加工工艺,2018,47(18):147-149. 被引量:6

9刘笑达,王一都,闫敏,卫英慧,侯利锋,郭春丽.金属阳离子对镁在含Cl^-溶液中腐蚀行为的影响[J].太原理工大学学报,2018,49(5):676-680.

10李景轩.一种新型锌镍合金电镀工艺及镀层的耐蚀性[J].材料保护,2018,51(9):74-79. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TG174.41[金属学及工艺—金属表面处理]

Citation Information:

Ni-Co/ZrO2 composite coatings were prepared by co-deposition technology in acid sulfamate solu-tion. The effects of nanopartieles in Ni-Co/ZrO2 composite system on its electrochemical reaction process were studied by cathode linear scan test. The surface morphology and mierostructure of the composite coat-ings were analyzed by SEM and XRD. The corrosion resistance of the composite coatings was tested by Tafel curves and their thermal stability was characterized by microhardness test after annealing. The exper-imental results show that Ni-Co/ZrO2 co-deposition potential is about --0.90 V. Compared with Ni-Co al-loy,Ni-Co/ZrO2 composite coating surface is more uniform and compact,the grains are smaller,and its cor- rosion resistance and thermal stability are better.

quote

GB/T 7714-2015 [1] ZHOU Xin-yu, WANG Yi-yong, JIN Hui, et al. Electrochemical Research and Performance Characterization of Ni-Co/ZrO_2 Composite Coatings[J]. Rare Metals and Cemented Carbides, 2018(5): 54-58.
MLA [1] ZHOU Xin-yu, et al., "Electrochemical Research and Performance Characterization of Ni-Co/ZrO_2 Composite Coatings." Rare Metals and Cemented Carbides, no. 5, 2018, pp. 54-58.
APA [1] ZHOU Xin-yu, WANG Yi-yong, JIN Hui, LIANG Zhi-peng, & LIU Xiang-lin. (2018). Electrochemical Research and Performance Characterization of Ni-Co/ZrO_2 Composite Coatings. Rare Metals and Cemented Carbides(5), 54-58.
IEEE [1] ZHOU Xin-yu, WANG Yi-yong, JIN Hui, LIANG Zhi-peng, and LIU Xiang-lin, "Electrochemical Research and Performance Characterization of Ni-Co/ZrO_2 Composite Coatings," Rare Metals and Cemented Carbides, no. 5, pp. 54-58, 2018. keywords: {Ni-Co/ZrO2 composite coating;co-deposition;LSV curve;Tafel test;grain orientation}