daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Detection of Long Wavelength Photons via Quasi-Two-Dimensional Ternary Ta2NiSe5 Detection of Long Wavelength Photons via Quasi-Two-Dimensional Ternary Ta2NiSe5 AITranslate

P. R. China|University of Chinese Academy of Sciences; University of Chinese Academy of Sciences; P. R. China|University of Chinese Academy of Sciences; P. R. China|University of Chinese Academy of Sciences; P. R. China|University of Chinese Academy of Sciences; Shanghai Institute of Technical Physics; Shanghai Institute of Technical Physics; Fudan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Terahertz technologies are of great significance in a wide range of applications, such as astronomy, medicine, communications and nondestructive material characterization. However, the energy of terahertz photons is so small that it is difficult to detect directly at room temperature. Two-dimensional (2D) materials with excellent optoelectronic properties provide opportunities for the development of terahertz photodetectors. Herein, we develop a high-performance terahertz photodetector with a metal–semiconductor–metal structure via a Ta2NiSe5 nanosheet. The photodetector shows an excellent responsivity of 1350 A W–1 and an extremely low noise equivalent power of 0.01 pW Hz–0.5 with a fast response of ∼550 ns at room temperature. Electromagnetic induced well theory is utilized to explain the highly sensitive terahertz photoelectric response. In addition, long-term stability over 6 months is realized for the detector. The terahertz imaging experiments demonstrate the excellent performance of the detector and potential applications. The results suggest that our strategy can be a strong candidate for high-performance terahertz photodetection systems.

KeyWords AITranslate

quasitwodimensional terahertz detection electromagnetic induced well Ta2NiSe5 terahertz imaging
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00421

Chinese Library Classification Number:

Citation Information:

Terahertz technologies are of great significance in a wide range of applications, such as astronomy, medicine, communications and nondestructive material characterization. However, the energy of terahertz photons is so small that it is difficult to detect directly at room temperature. Two-dimensional (2D) materials with excellent optoelectronic properties provide opportunities for the development of terahertz photodetectors. Herein, we develop a high-performance terahertz photodetector with a metal–semiconductor–metal structure via a Ta2NiSe5 nanosheet. The photodetector shows an excellent responsivity of 1350 A W–1 and an extremely low noise equivalent power of 0.01 pW Hz–0.5 with a fast response of ∼550 ns at room temperature. Electromagnetic induced well theory is utilized to explain the highly sensitive terahertz photoelectric response. In addition, long-term stability over 6 months is realized for the detector. The terahertz imaging experiments demonstrate the excellent performance of the detector and potential applications. The results suggest that our strategy can be a strong candidate for high-performance terahertz photodetection systems.

quote

GB/T 7714-2015 [1] Wanli Ma, Tuntan Wu, Wangchen Mao, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00421.
MLA [1] Wanli Ma, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00421.
APA [1] Wanli Ma, Tuntan Wu, Wangchen Mao, Qinxi Qiu, Jingbo Li, Lin Jiang, Niangjuan Yao, & Zhiming Huang. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00421
IEEE [1] Wanli Ma, Tuntan Wu, Wangchen Mao, Qinxi Qiu, Jingbo Li, Lin Jiang, Niangjuan Yao, and Zhiming Huang, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00421. keywords: {quasitwodimensional terahertz detection electromagnetic induced well Ta2NiSe5 terahertz imaging}